Influence of Diluent Types on Self-propagating High Temperature Synthesis of Tungsten Powder AITranslate
Abstract AITranslate
Using tungsten trioxide, magnesium powder and diluents as raw materials, tungsten powder was prepared by self-propagating high temperature synthesis method.The influence of diluent types on the properties of tungsten powder in different raw material states was studied, and the determination of the best reaction diluent and process improvement for the preparation of tungsten powder by self-propagating high temperature synthesis were further explored.The experimental results show that elemental tungsten powder can be obtained regardless of whether the reactants are in powder state or pressed state, and the particle size of tungsten powder prepared in powder state is smaller.Different types of diluents have a significant effect on the morphology of the product tungsten powder.Using MgO as the diluent, the particles of the product tungsten powder is relatively larger and the distribution is relatively uneven.Using K2CO3,Na2CO3and Li2CO3as the diluent, the particle size of the obtained tungsten powder is un-even and increases in turn.NaCl is the best diluent for the preparation of tungsten powder by self-propagating high temperature synthesis method, the morphology of the obtained tungsten powder is the best, and the overall particle size of tungsten powder is less than 200 nm.
KeyWords AITranslate
1刘夙伟,季峰,张艳,郭宇航.钨对高铬铸铁耐磨性能影响的研究[J].铸造技术,2020,41(12):1126-1130. 被引量:4
2姜文伟,普崇恩.等离子喷雾法制取球形钨粉工艺探讨[J].硬质合金,2000,17(2):85-88. 被引量:19
3王凯飞,张国华.高纯超细钨和碳化钨粉体的制备[J].中国有色金属学报:英文版,2020,30(6):1697-1706. 被引量:11
4陈丽杰,谢中华,王瑞祥,田磊,聂华平.氧化钨粉还原碳化机理分析及超细碳化钨粉的制备[J].稀有金属与硬质合金,2018,46(2):11-15. 被引量:7
5张勇,张国华.纳米钨辅助氢气还原氧化钨制备超细钨粉[J].粉末冶金材料科学与工程,2020,25(5):375-380. 被引量:2
6郑艾龙,吴传露,杨益航,黄志民,陈俊卿,叶铭海.高纯钨的制备及粒度影响研究[J].中国钨业,2019,34(6):61-68. 被引量:5
7罗来马,章宇翔,昝祥,刘家琴,朱晓勇,吴玉程.自蔓延高温合成高熔点粉体的研究现状与发展[J].稀有金属,2018,42(11):1210-1220. 被引量:7
8王延玲,张廷安,杨欢,魏世丞.自蔓延高温还原法制备钨粉的研究[J].稀有金属材料与工程,2001,30(4):310-313. 被引量:17
9豆志河,张廷安.自蔓延冶金法制备粉体与合金的研究进展[J].中国材料进展,2016,35(8):598-605. 被引量:3
10史冠勇,熊民,陈平,豆志河.自蔓延高温合成制备钨粉的热力学研究[J].江西冶金,2019,39(3):12-15. 被引量:3
1马凯丽,滕阳阳,张峥.在线测厚探头的研制[J].金属热处理,2019,0(S01):680-683.
2全温灿,艾志龙,吴彤,史冠勇,豆志河.自蔓延高温合成制备碳化钨粉的热力学研究[J].江西冶金,2022,42(2):13-17.
Basic Information:
DOI:
Chinese Library Classification Number:TF123[冶金工程—粉末冶金]
Citation Information:
Using tungsten trioxide, magnesium powder and diluents as raw materials, tungsten powder was prepared by self-propagating high temperature synthesis method.The influence of diluent types on the properties of tungsten powder in different raw material states was studied, and the determination of the best reaction diluent and process improvement for the preparation of tungsten powder by self-propagating high temperature synthesis were further explored.The experimental results show that elemental tungsten powder can be obtained regardless of whether the reactants are in powder state or pressed state, and the particle size of tungsten powder prepared in powder state is smaller.Different types of diluents have a significant effect on the morphology of the product tungsten powder.Using MgO as the diluent, the particles of the product tungsten powder is relatively larger and the distribution is relatively uneven.Using K2CO3,Na2CO3and Li2CO3as the diluent, the particle size of the obtained tungsten powder is un-even and increases in turn.NaCl is the best diluent for the preparation of tungsten powder by self-propagating high temperature synthesis method, the morphology of the obtained tungsten powder is the best, and the overall particle size of tungsten powder is less than 200 nm.
quote
| GB/T 7714-2015 | [1] QUAN Wen-can, ZHONG Yi-hui, YAN Run, et al. Influence of Diluent Types on Self-propagating High Temperature Synthesis of Tungsten Powder[J]. Rare Metals and Cemented Carbides, 2022(2): 26-30. |
| MLA | [1] QUAN Wen-can, et al., "Influence of Diluent Types on Self-propagating High Temperature Synthesis of Tungsten Powder." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 26-30. |
| APA | [1] QUAN Wen-can, ZHONG Yi-hui, YAN Run, SHI Guan-yong, & DOU Zhi-he. (2022). Influence of Diluent Types on Self-propagating High Temperature Synthesis of Tungsten Powder. Rare Metals and Cemented Carbides(2), 26-30. |
| IEEE | [1] QUAN Wen-can, ZHONG Yi-hui, YAN Run, SHI Guan-yong, and DOU Zhi-he, "Influence of Diluent Types on Self-propagating High Temperature Synthesis of Tungsten Powder," Rare Metals and Cemented Carbides, no. 2, pp. 26-30, 2022. keywords: {tungsten powder;diluent;self-propagating high temperature synthesis;phase composition;micromorphology;particle size} |