daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation and Electrochemical Energy Storage of NiMoO4@NiMn2O4 Nanocomposites AITranslate

School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology;School of Materials Science and Engineering,Liaoning University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The NiMoO4@NiMn2O4 composite electrode material based on nickel foam was successfully prepared by two-step hydrothermal method.The phase composition and microstructure of the electrode material were studied by X-ray diffractometer(XRD)and scanning electron microscope(SEM).The electrochemical performance of the electrode material was tested by cyclic voltammetry(CV),galvanostatic charge-discharge(GCD)and electrochemical impedance spectroscopy(EIS).The results show that the velvet-like NiMn2O4is attached to the nanowire-like NiMoO4,which increases the specific surface area and the specific capacitance of the electrode material.At the current density of 1 mA/cm2,the specific capacitances of NiMoO4 and NiMoO4@NiMn2O4 are 240 mF/cm2and 2120 mF/cm2,respectively.Compared with the single NiMoO;electrode material,the NiMoO4@NiMn2O4composite electrode material exhibits more excellent electrochemical performance due to the dual optimization of composition and structure.

KeyWords AITranslate

hydrothermal method nickel foam nanocomposite NiMoO4@NiMn2O4 electrochemical performance specific capacitance

1贾志军,王俊,王毅.超级电容器电极材料的研究进展[J].储能科学与技术,2014,3(4):322-338. 被引量:11

2李明伟,杨绍斌,贾婧,顾金峰,耿福洋.花状与颗粒状NiMn2O4纳米材料的制备及其超级电容性能[J].化工进展,2020,39(5):1844-1850. 被引量:1

3王广建,陈征,周桃.NiMoO_(4)-CoMoO_(4)纳米复合材料的制备及其电化学性能[J].微纳电子技术,2021,58(4):292-295. 被引量:4

4李明伟,杨绍斌.低结晶度NiMn_(2)O_(4)/还原氧化石墨烯复合材料的制备及其超级电容性能[J].硅酸盐学报,2021,49(3):503-510. 被引量:6

1赵苗苗,陈小强,王英,贺彦强.基于小波包熵及双重优化神经网络的牵引逆变器开路故障诊断[J].铁道科学与工程学报,2022,19(4):1101-1110. 被引量:1

2沈添天,袁思敏,吴芳,陈中祥,余果.基于线性矩阵不等式的智能飞行器航迹规划方法[J].全球定位系统,2022,47(2):73-81.

Basic Information:

DOI:

Chinese Library Classification Number:TB383[一般工业技术—材料科学与工程]

Citation Information:

The NiMoO4@NiMn2O4 composite electrode material based on nickel foam was successfully prepared by two-step hydrothermal method.The phase composition and microstructure of the electrode material were studied by X-ray diffractometer(XRD)and scanning electron microscope(SEM).The electrochemical performance of the electrode material was tested by cyclic voltammetry(CV),galvanostatic charge-discharge(GCD)and electrochemical impedance spectroscopy(EIS).The results show that the velvet-like NiMn2O4is attached to the nanowire-like NiMoO4,which increases the specific surface area and the specific capacitance of the electrode material.At the current density of 1 mA/cm2,the specific capacitances of NiMoO4 and NiMoO4@NiMn2O4 are 240 mF/cm2and 2120 mF/cm2,respectively.Compared with the single NiMoO;electrode material,the NiMoO4@NiMn2O4composite electrode material exhibits more excellent electrochemical performance due to the dual optimization of composition and structure.

quote

GB/T 7714-2015 [1] BU Nan, XIANG Jun, ZHAO Rong-da, et al. Preparation and Electrochemical Energy Storage of NiMoO4@NiMn2O4 Nanocomposites[J]. Rare Metals and Cemented Carbides, 2022(2): 31-36.
MLA [1] BU Nan, et al., "Preparation and Electrochemical Energy Storage of NiMoO4@NiMn2O4 Nanocomposites." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 31-36.
APA [1] BU Nan, XIANG Jun, ZHAO Rong-da, MA Dong-mei, LI Mei-ting, & LI Jia. (2022). Preparation and Electrochemical Energy Storage of NiMoO4@NiMn2O4 Nanocomposites. Rare Metals and Cemented Carbides(2), 31-36.
IEEE [1] BU Nan, XIANG Jun, ZHAO Rong-da, MA Dong-mei, LI Mei-ting, and LI Jia, "Preparation and Electrochemical Energy Storage of NiMoO4@NiMn2O4 Nanocomposites," Rare Metals and Cemented Carbides, no. 2, pp. 31-36, 2022. keywords: {hydrothermal method;nickel foam;nanocomposite;NiMoO@NiMnO;electrochemical performance;specific capacitance}