Effect of Combined Mn-Fe Loading and Sulphuric Acid Acidification on NH3-SCR Denitration Performance of Synthetic(Ce,La)CO3F AITranslate

School of Energy and Environment,Inner Mongolia University of Science&Technology;School of Energy and Environment,Inner Mongolia University of Science&Technology;School of Energy and Environment,Inner Mongolia University of Science&Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bayan Obo bastnaesite was selected as the research object,and according to its Ce/La mass ratio,(Ce,La)CO3F crystal grains were synthesized by hydrothermal method to study their NH3-SCR denitration performance.The results show that(Ce,La)CO3F synthesized by adding excess NaHCO3has better catalytic effect.After roasted at 500℃,the(Ce,La)CO3F grains have the best denitration effect,and the NOx conversion rate is 34%at the catalytic reaction temperature of 200℃.The combined action of Mn-Fe loading and sulfuric acid acidification can excite the active components of(Ce,La)CO3F catalyst.After the catalyst with the combined action is roasted at 400℃,the NOx conversion rate of 93%is obtained at the catalytic reaction temperature of 250℃.The reaction mechanism of(Ce,La)CO3F catalyst was explored by in-situ infrared technology.The results show that the surface reaction of Mn-Fe loaded and sulfuric acid acidified(Ce,La)CO3F catalyst mainly follows the E-R mechanism.The reactive species are NH+4/NH3(a)generated by NH3(g)adsorption on the catalyst surface and NO,which undergo a series of intermediate reactions to produce N2 and H2O.This study can provide theoretical guidance for the use of rare earth concentrates as denitration catalysts.

KeyWords AITranslate

synthetic(Ce La)CO3F Mn-Fe loading sulphuric acid acidification combined action denitration performance catalytic mechanism

1朱智慧,杨占峰,王其伟,王振江,李娜.白云鄂博稀土精矿工艺矿物学研究[J].有色金属:选矿部分,2019,0(6):1-4. 被引量:15

2宋忠贤,张秋林,宁平,刘昕,樊洁,黄真真.Introduction manner of sulfate acid for improving the performance of SO_4^(2–)/CeO_2 on selective catalytic reduction of NO by NH_3[J].稀土学报:英文版,2016,34(7):667-674. 被引量:8

3张强,刘璐,于梦云,周洲.氧化铝载体硫酸化对锰铈催化剂SCR脱硝性能的影响[J].燃料化学学报,2019,47(9):1137-1145. 被引量:5

4张秋林,张金辉,宁平,宋忠贤,王燕彩,徐利斯,唐小苏.SO_4^(2-)改性对Ce、Ti基催化剂NH_3-SCR脱硝性能的影响[J].昆明理工大学学报:自然科学版,2014,39(6):110-115. 被引量:4

5张治安,杨邦朝,邓梅根,胡永达,汪斌华.超级电容器纳米氧化锰电极材料的合成与表征[J].化学学报,2004,62(17):1617-1620. 被引量:39

6刘珊珊,王强,张润铎.MnO_x和Fe_2O_3的酸化及组合用于NH_3-SCR脱硝反应的研究[J].中国科学:化学,2018,48(6):620-629. 被引量:2

1黄振洋.几种常用氧化还原指标适用性讨论[J].河南科技,2021,40(33):104-106. 被引量:1

2樊晓泽,王瑞,马骏,齐二帅.混合稀土对AZ91D压铸镁合金流动性及力学性能的影响[J].铸造技术,2022,43(4):285-289.

3张红雨,苏犁,秦红.内蒙古大沟井寒武纪黑色页岩元素地球化学特征及钒赋存形式[J].现代地质,2022,36(1):321-332. 被引量:1

4何洪茜,肖加飞,杨海英,兰青,黄明亮.贵州北部五峰组烃源岩沉积环境及页岩气资源潜力[J].贵州科学,2022,40(2):59-64.

5王永斌,彭军,罗果萍,张芳,安胜利.MgO、F、碱金属对球团矿相组织的影响[J].钢铁,2022,57(4):34-42. 被引量:2

6李铁芳.内蒙古乌兰西萤石矿地质特征与找矿标志研究[J].市场调查信息:综合版,2022(6):00134-00136.

7Wenjie Zhang,Dongxia Feng,Xian Xie,Xiong Tong,Yunpeng Du,Yang Cao.Solvent extraction and separation of light rare earths from chloride media using HDEHP-P350 system[J].稀土学报:英文版,2022,40(2):328-337. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TQ426[化学工程]

Citation Information:

Bayan Obo bastnaesite was selected as the research object,and according to its Ce/La mass ratio,(Ce,La)CO3F crystal grains were synthesized by hydrothermal method to study their NH3-SCR denitration performance.The results show that(Ce,La)CO3F synthesized by adding excess NaHCO3has better catalytic effect.After roasted at 500℃,the(Ce,La)CO3F grains have the best denitration effect,and the NOx conversion rate is 34%at the catalytic reaction temperature of 200℃.The combined action of Mn-Fe loading and sulfuric acid acidification can excite the active components of(Ce,La)CO3F catalyst.After the catalyst with the combined action is roasted at 400℃,the NOx conversion rate of 93%is obtained at the catalytic reaction temperature of 250℃.The reaction mechanism of(Ce,La)CO3F catalyst was explored by in-situ infrared technology.The results show that the surface reaction of Mn-Fe loaded and sulfuric acid acidified(Ce,La)CO3F catalyst mainly follows the E-R mechanism.The reactive species are NH+4/NH3(a)generated by NH3(g)adsorption on the catalyst surface and NO,which undergo a series of intermediate reactions to produce N2 and H2O.This study can provide theoretical guidance for the use of rare earth concentrates as denitration catalysts.

quote

GB/T 7714-2015 [1] CHEN Ze-dong, LI Na, WU Wen-fei. Effect of Combined Mn-Fe Loading and Sulphuric Acid Acidification on NH3-SCR Denitration Performance of Synthetic(Ce,La)CO3F[J]. Rare Metals and Cemented Carbides, 2022(2): 37-44.
MLA [1] CHEN Ze-dong, et al., "Effect of Combined Mn-Fe Loading and Sulphuric Acid Acidification on NH3-SCR Denitration Performance of Synthetic(Ce,La)CO3F." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 37-44.
APA [1] CHEN Ze-dong, LI Na, & WU Wen-fei. (2022). Effect of Combined Mn-Fe Loading and Sulphuric Acid Acidification on NH3-SCR Denitration Performance of Synthetic(Ce,La)CO3F. Rare Metals and Cemented Carbides(2), 37-44.
IEEE [1] CHEN Ze-dong, LI Na, and WU Wen-fei, "Effect of Combined Mn-Fe Loading and Sulphuric Acid Acidification on NH3-SCR Denitration Performance of Synthetic(Ce,La)CO3F," Rare Metals and Cemented Carbides, no. 2, pp. 37-44, 2022. keywords: {synthetic(Ce,La)COF;Mn-Fe loading;sulphuric acid acidification;combined action;denitration performance;catalytic mechanism}