Research Progress of Reforming Hydrogen Production Catalysts Modified by La,Ce and Other Rare Earths AITranslate
Abstract AITranslate
The chemical reforming hydrogen production method has the advantages of easy availability of raw materials,low energy consumption,and high cost-effectiveness.However,its stable and efficient catalytic system is not yet perfect,and using rare earths to modify reforming hydrogen production catalysts has a good effect.From the perspectives of chemistry and energy,the research progress of reforming hydrogen production catalytic systems modified by rare earths at home and abroad is reviewed and commented.The effects of modification of reforming hydrogen production catalysts and their carriers respectively by La,Ce and Pr three commonly used rare earths on improvement of hydrogen production performance are emphatically expounded,and the mechanism of rare earth modification is analyzed.Combined with the current research trend that catalyst modification focuses on composite carrier modification,promoter modification and synthesis process optimization,the in-depth research direction of rare earth modified reforming hydrogen production catalysts in the future is proposed.
KeyWords AITranslate
1王嘉琦,王秋颖,朱桐慧,朱小梅,孙冰.甲烷重整制氢的研究现状分析[J].现代化工,2020,40(7):15-20. 被引量:14
2陈英杰.天然气制氢技术进展及发展趋势[J].煤炭与化工,2020,43(11):130-133. 被引量:22
3詹望成,郭耘,龚学庆,郭杨龙,王艳芹,卢冠忠.稀土催化材料的应用及研究进展[J].催化学报(英文),2014,35(8):1238-1250. 被引量:21
4焦桐,许雪莲,张磊,翁幼云,翁玉冰,高志贤.C_(u)O/C_(e)O2-Z_(r)O2/S_(i)C整体催化剂催化甲醇水蒸气重整制氢的研究[J].化学学报,2021,79(4):513-519. 被引量:8
5王菊枝,罗来涛,汤敏擘.稀土改性CuO-ZnO-ZrO_2催化剂甲醇水蒸汽重整制氢反应[J].南昌大学学报:理科版,2006,30(2):146-149. 被引量:2
6李亮荣,孙戊辰,陈祖杰,齐海霞.载体改性对Ni/La_(2)O_(2)CO_(3)催化乙醇水蒸气重整制氢的影响[J].稀有金属与硬质合金,2021,49(4):50-54. 被引量:4
7梁红,李树华,洪燕霞,王婷婷,陈姚.稀土改性氧化铝为载体的催化剂研究[J].广州大学学报:自然科学版,2012,11(3):45-49. 被引量:2
8江西将组建中重稀土重点实验室[J].浙江化工,2020,51(9):50-50. 被引量:1
9彭稳,雷艳秋,罗永明,梅毅,何德东.钐改性Ni/Al2O3催化剂及其用于甲醇水蒸气重整制氢反应研究[J].中国稀土学报,2019,37(3):303-310. 被引量:5
10李亮荣,陈祖杰,付兵,孙戊辰,齐海霞.MgO复合载体负载Ni催化乙醇水蒸气重整制氢[J].化学工程,2021,49(7):12-15. 被引量:1
1吴珺,郭文涛,刘欣坤,赵增武,刘宝玉.温度对La_(2)O_(3)-SiO_(2)-CaO-Al_(2)O_(3)-MgO系高温熔体结构的影响[J].稀有金属与硬质合金,2022,50(6):52-58.
2李亮荣,梁娇,彭建,艾盛,齐海霞.基于MOFs材料光催化分解水制氢的研究进展[J].精细化工,2023,40(3):553-564.
1李亮荣,李秋平,艾盛,邓志伟,倪智超,邱浩,熊磊.传统化石与新型生物质能源重整制氢研究现状[J].化学与生物工程,2021,38(11):1-6. 被引量:6
2李国靖,马潇,贾萌,李建其,刘育.氘代丁苯那嗪合成工艺优化[J].中国医药工业杂志,2021,52(12):1595-1598.
3吴利鑫,吴旭锋,王智慧,刘鹏程,洪黎鹏,王登.溴夫定有关物质的制备与结构鉴定[J].中国药物化学杂志,2022,32(2):106-110.
4李习红,刘皇见,吴李瑞,谷顺明,刘敏.3-氰基吡啶的合成工艺优化[J].安徽化工,2021,47(6):107-109.
5王新利,兰燕芹,王尧.抗癌新药依维莫司的合成工艺优化和抗癌活性研究[J].当代化工研究,2021(24):143-145.
6吴缰.安全与环保管理信息化系统在某集团的建设与应用[J].混凝土世界,2021(9):48-52. 被引量:1
7柯浩,杨汉跃,闫显光,李树亮,张珍明,李润莱.依折麦布关键中间体的合成工艺优化[J].精细化工,2022,39(2):426-432.
8姚忠全,杜伟宏,宋明伟,王宇驰,丁小东,曹胜华,董宏波.氯雷他定合成工艺优化[J].化学研究与应用,2021,33(12):2441-2448.
9曾丽,张欢,朱丽华.稀土掺杂调变催化剂多相催化加氢性能研究进展[J].工业催化,2022,30(2):1-5.
10邓玉晓,孙晋瑞,张宁,张宗磊,冯仰辉.盐酸尼莫司汀的合成工艺优化[J].食品与药品,2022,24(2):161-163.
Basic Information:
DOI:
Chinese Library Classification Number:TQ426[化学工程]
Citation Information:
The chemical reforming hydrogen production method has the advantages of easy availability of raw materials,low energy consumption,and high cost-effectiveness.However,its stable and efficient catalytic system is not yet perfect,and using rare earths to modify reforming hydrogen production catalysts has a good effect.From the perspectives of chemistry and energy,the research progress of reforming hydrogen production catalytic systems modified by rare earths at home and abroad is reviewed and commented.The effects of modification of reforming hydrogen production catalysts and their carriers respectively by La,Ce and Pr three commonly used rare earths on improvement of hydrogen production performance are emphatically expounded,and the mechanism of rare earth modification is analyzed.Combined with the current research trend that catalyst modification focuses on composite carrier modification,promoter modification and synthesis process optimization,the in-depth research direction of rare earth modified reforming hydrogen production catalysts in the future is proposed.
quote
| GB/T 7714-2015 | [1] LI Liang-rong, DING Yong-hong, DENG Zhi-wei, et al. Research Progress of Reforming Hydrogen Production Catalysts Modified by La,Ce and Other Rare Earths[J]. Rare Metals and Cemented Carbides, 2022(2): 45-49. |
| MLA | [1] LI Liang-rong, et al., "Research Progress of Reforming Hydrogen Production Catalysts Modified by La,Ce and Other Rare Earths." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 45-49. |
| APA | [1] LI Liang-rong, DING Yong-hong, DENG Zhi-wei, LIU Yan, PENG Jian, NI Zhi-chao, & XIONG Lei. (2022). Research Progress of Reforming Hydrogen Production Catalysts Modified by La,Ce and Other Rare Earths. Rare Metals and Cemented Carbides(2), 45-49. |
| IEEE | [1] LI Liang-rong, DING Yong-hong, DENG Zhi-wei, LIU Yan, PENG Jian, NI Zhi-chao, and XIONG Lei, "Research Progress of Reforming Hydrogen Production Catalysts Modified by La,Ce and Other Rare Earths," Rare Metals and Cemented Carbides, no. 2, pp. 45-49, 2022. keywords: {catalyst;reforming hydrogen production;rare earth modification;hydrogen energy;research progress} |