Study on Preparation of Tungsten Powders by Reduction with Different Tungsten Oxides and their Characteristics AITranslate

Chongyi Zhangyuan Tungsten Co.,Ltd.;Chongyi Zhangyuan Tungsten Co.,Ltd.;Chongyi Zhangyuan Tungsten Co.,Ltd.;Chongyi Zhangyuan Tungsten Co.,Ltd.;Chongyi Zhangyuan Tungsten Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tungsten powders were prepared by hydrogen reduction with chromium-doped tungsten oxide, purple tungsten oxide and yellow tungsten oxide as raw materials at different reaction temperatures.The phase and microstructure of tungsten powders prepared by reduction of different tungsten oxides were analyzed by XRD and SEM,and the influence of chromium doping on the reduction process of tungsten oxide was explored.The results show that under the same reduction conditions, purple tungsten oxide is the easiest to reduce due to its loose and breathable fine needle-like structure, and the prepared W powder has good dispersibility, fine particle size and uniform distribution.Chromium-doped tungsten oxide is the most difficult to reduce due to the inhibitory effect of Cr2O3,and the prepared W powder has a large number of fine-grained aggregates, with poor powder particle size uniformity and small average particle size.The reduction difficulty of yellow tungsten oxide is between purple tungsten oxide and chromium-doped tungsten oxide due to its dense and airtight cubic structure, and the prepared W powder has coarse particle size and serious agglomeration.

KeyWords AITranslate

tungsten oxide chromium doping purple tungsten oxide yellow tungsten oxide tungsten powder hydrogen reduction

1羊求民,羊建高,苏伟,陈丽勇,陈颢,郭圣达.纳米/超细晶WC-Co类硬质合金的研究进展[J].稀有金属与硬质合金,2018,46(1):76-83. 被引量:18

2李重典,时凯华,王海霞,闵召宇,廖军,徐志超.烧结工艺对WC-1.0TiC-3.1TaC-4.5Co硬质合金性能及微观组织的影响[J].材料工程,2016,44(12):74-79. 被引量:6

3董凯林,时凯华,顾金宝,曾伟,吴翔.抑制剂在硬质合金中的应用及研究现状[J].稀有金属与硬质合金,2019,47(4):76-82. 被引量:4

4王学政,王海滨,刘雪梅,杨涛,谢丽杰,占王彬,宋晓艳.复合添加晶粒长大抑制剂对WC-12Co超细晶硬质合金涂层性能的影响[J].稀有金属材料与工程,2018,47(4):1216-1220. 被引量:1

5郑虎春,范景莲,杨文华,张忠健,刘涛.VC/Cr_3C_2及配碳量对WC-0.5Co超细硬质合金组织与性能的影响[J].稀有金属材料与工程,2015,44(4):912-917. 被引量:6

6刘雪梅,王海滨,宋晓艳,王西龙,李玉玺.VC添加量对纳米晶硬质合金的制备及性能影响[J].稀有金属材料与工程,2016,45(2):477-481. 被引量:10

7刘柏雄,杨高玲,邝梦杰,尚宜生,朱根松,杨斌.氧化钇掺杂对制备纳米WC-Co复合粉的影响规律及其调控机制[J].稀有金属,2020,0(1):26-33. 被引量:4

8张雪辉,黄柱,徐畅,李晓闲,蔡志勇,陈颢.Cr_3C_2对SPS烧结WC-6Co硬质合金组织与性能的影响[J].中国有色金属学报,2017,27(8):1580-1588. 被引量:10

9叶楠,唐建成,魏晓枭,张静.纳米W粉阶段碳化制备纳米WC粉的工艺及机制研究[J].稀有金属,2017,41(7):775-782. 被引量:2

1王红云,王韶毅,刘莉,唐彦渊,羊求民.配碳量对原位碳热反应制备Co_(x)W_(y)C复合粉末微观结构的影响[J].稀有金属与硬质合金,2022,50(5):47-51.

1专利信息[J].中国钨业,2021,36(6):76-76.

2鲍瑞,郭圣达,易健宏,陈颢,羊建高,余飞.微波反应烧结制备WC-Co硬质合金工艺性能[J].中国有色金属学报,2020,30(8):1828-1836. 被引量:6

3杨星波,朱纪磊,陈斌科,凤治华,李晓辉.等离子旋转电极雾化技术及粉末粒度控制研究现状[J].粉末冶金工业,2022,32(2):90-95. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF123[冶金工程—粉末冶金]

Citation Information:

Tungsten powders were prepared by hydrogen reduction with chromium-doped tungsten oxide, purple tungsten oxide and yellow tungsten oxide as raw materials at different reaction temperatures.The phase and microstructure of tungsten powders prepared by reduction of different tungsten oxides were analyzed by XRD and SEM,and the influence of chromium doping on the reduction process of tungsten oxide was explored.The results show that under the same reduction conditions, purple tungsten oxide is the easiest to reduce due to its loose and breathable fine needle-like structure, and the prepared W powder has good dispersibility, fine particle size and uniform distribution.Chromium-doped tungsten oxide is the most difficult to reduce due to the inhibitory effect of Cr2O3,and the prepared W powder has a large number of fine-grained aggregates, with poor powder particle size uniformity and small average particle size.The reduction difficulty of yellow tungsten oxide is between purple tungsten oxide and chromium-doped tungsten oxide due to its dense and airtight cubic structure, and the prepared W powder has coarse particle size and serious agglomeration.

quote

GB/T 7714-2015 [1] YANG Cheng-hui, XU Guo-zuan, LIU Ru-tiez, et al. Study on Preparation of Tungsten Powders by Reduction with Different Tungsten Oxides and their Characteristics[J]. Rare Metals and Cemented Carbides, 2022(2): 19-25.
MLA [1] YANG Cheng-hui, et al., "Study on Preparation of Tungsten Powders by Reduction with Different Tungsten Oxides and their Characteristics." Rare Metals and Cemented Carbides, no. 2, 2022, pp. 19-25.
APA [1] YANG Cheng-hui, XU Guo-zuan, LIU Ru-tiez, ZHANG Long-hui, & YANG Qiu-min. (2022). Study on Preparation of Tungsten Powders by Reduction with Different Tungsten Oxides and their Characteristics. Rare Metals and Cemented Carbides(2), 19-25.
IEEE [1] YANG Cheng-hui, XU Guo-zuan, LIU Ru-tiez, ZHANG Long-hui, and YANG Qiu-min, "Study on Preparation of Tungsten Powders by Reduction with Different Tungsten Oxides and their Characteristics," Rare Metals and Cemented Carbides, no. 2, pp. 19-25, 2022. keywords: {tungsten oxide;chromium doping;purple tungsten oxide;yellow tungsten oxide;tungsten powder;hydrogen reduction}