Solution-Processed Self-Powered Panchromatic Organic Photodiode and Its Application in Biomedical Devices Solution-Processed Self-Powered Panchromatic Organic Photodiode and Its Application in Biomedical Devices AITranslate
Abstract AITranslate
Non-fullerene acceptor (NFA)-based optoelectronic devices have received great research interest because of their unique optoelectronic characteristics like tunable bandgap, strong near-infrared (NIR) light absorption, and enhanced stability. However, the demonstration of a self-powered NIR broadband photodiode with excellent photoresponse and low dark current density comparable to that of commercial inorganic counterpart remains a challenge. Herein, the high-performance solution-processed self-powered organic broadband photodiode is demonstrated by using a narrow bandgap NFA with a low dark current density (Jd) of 1.05 nA/cm2 at 0 V. The dark leakage current of the device is greatly improved by adopting a “thick junction” strategy, and the optimized device exhibits a Jd of 6.5 nA/cm2 even at a moderate applied bias voltage of −1.5 V. The devices exhibit more than 70% external quantum efficiency in the 550–830 nm wavelength (λ) range and a specific detectivity of 2.65 × 1012 jones at λ ∼ 770 nm under the self-powered mode of operation. The fabricated photodetector is used in photoplethysmography (PPG) measurement, demonstrating its application in real-time heart-rate monitoring and pulse oximetry.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c01248
Chinese Library Classification Number:
Citation Information:
Non-fullerene acceptor (NFA)-based optoelectronic devices have received great research interest because of their unique optoelectronic characteristics like tunable bandgap, strong near-infrared (NIR) light absorption, and enhanced stability. However, the demonstration of a self-powered NIR broadband photodiode with excellent photoresponse and low dark current density comparable to that of commercial inorganic counterpart remains a challenge. Herein, the high-performance solution-processed self-powered organic broadband photodiode is demonstrated by using a narrow bandgap NFA with a low dark current density (Jd) of 1.05 nA/cm2 at 0 V. The dark leakage current of the device is greatly improved by adopting a “thick junction” strategy, and the optimized device exhibits a Jd of 6.5 nA/cm2 even at a moderate applied bias voltage of −1.5 V. The devices exhibit more than 70% external quantum efficiency in the 550–830 nm wavelength (λ) range and a specific detectivity of 2.65 × 1012 jones at λ ∼ 770 nm under the self-powered mode of operation. The fabricated photodetector is used in photoplethysmography (PPG) measurement, demonstrating its application in real-time heart-rate monitoring and pulse oximetry.
quote
| GB/T 7714-2015 | [1] Alvin Joseph, Anitha B. Pillai, Vijith K. Pulikodan, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01248. |
| MLA | [1] Alvin Joseph, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01248. |
| APA | [1] Alvin Joseph, Anitha B. Pillai, Vijith K. Pulikodan, Akhil Alexander, Raees Muhammed, & Manoj A. G. Namboothiry. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01248 |
| IEEE | [1] Alvin Joseph, Anitha B. Pillai, Vijith K. Pulikodan, Akhil Alexander, Raees Muhammed, and Manoj A. G. Namboothiry, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01248. keywords: {organic photodiode selfpowered photodiode nearinfrared photodetector nonfullerene acceptor photoplethysmographyShow More} |