daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Phase and Composition Tunable Out-of-Plane Seebeck Coefficients for MoS2-Based Films Phase and Composition Tunable Out-of-Plane Seebeck Coefficients for MoS2-Based Films AITranslate

Chung-Ang University; Chung-Ang University; Chung-Ang University; Chung-Ang University; Seoul National University; The University of Tokyo; Chung-Ang University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional layered transition-metal dichalcogenides (TMDCs) are promising materials for thermoelectric applications due to their superior electronic and phonon transport properties due to a favorable large energy bandgap with an atomically thin layer, which also provides unique density of states for confined electrons and holes. Seebeck coefficient controllability in TMDC materials is essential. This paper demonstrates controllable out-of-plane Seebeck coefficients for large-area MoS2 thin films by changing their phase and composition. We address large Seebeck coefficient differences at room temperature using large-area single- and mixed-phase MoS2 thin films by adjusting the reaction temperature during sampling and also discuss interface thermal resistance in sandwiched Cu/MoS2/Cu structures. Our findings confirm an ideal platform to control thermoelectric properties for low-dimensional materials for small-scale energy harvesting and microcooling technologies.

KeyWords AITranslate

outofplane Seebeck coefficient twodimensional layered materials molybdenum disulfide molybdenum trioxide interfacialShow More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01260

Chinese Library Classification Number:

Citation Information:

Two-dimensional layered transition-metal dichalcogenides (TMDCs) are promising materials for thermoelectric applications due to their superior electronic and phonon transport properties due to a favorable large energy bandgap with an atomically thin layer, which also provides unique density of states for confined electrons and holes. Seebeck coefficient controllability in TMDC materials is essential. This paper demonstrates controllable out-of-plane Seebeck coefficients for large-area MoS2 thin films by changing their phase and composition. We address large Seebeck coefficient differences at room temperature using large-area single- and mixed-phase MoS2 thin films by adjusting the reaction temperature during sampling and also discuss interface thermal resistance in sandwiched Cu/MoS2/Cu structures. Our findings confirm an ideal platform to control thermoelectric properties for low-dimensional materials for small-scale energy harvesting and microcooling technologies.

quote

GB/T 7714-2015 [1] WonYong Lee, MinSung Kang, NoWon Park, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01260.
MLA [1] WonYong Lee, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01260.
APA [1] WonYong Lee, MinSung Kang, NoWon Park, GilSung Kim, HoWon Jang, Eiji Saitoh, & SangKwon Lee. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01260
IEEE [1] WonYong Lee, MinSung Kang, NoWon Park, GilSung Kim, HoWon Jang, Eiji Saitoh, and SangKwon Lee, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01260. keywords: {outofplane Seebeck coefficient twodimensional layered materials molybdenum disulfide molybdenum trioxide interfacialShow More}