Research on Reduction of F^- Content in Nb_2O_5 AITranslate

Conghua Small Small Reining Factory;Conghua Small Small Reining Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Research is made on the technological improvement of the original precipitation and pressure washing for preparation of NbO(H)_5.Comparison is made between the calcinators for NbO(H)_5.The results showed that the problem of F removal out of NbO(H)_5 washing solution from precipitation of high-concentration(Nb_2O_5>120 g/L)Nb solution can be solved through pretreatment with the addition of diluent.The new pressure washing process is characterized byhigher washing water temperature,more pulp-conditioning times,higher F-removal efficiency, water-saving and more up-to-standard Nb_2O_5 product

KeyWords AITranslate

niobium solution precipitation pressure washing calcinations Nb_2O_5 F-removal

1王肇信 幸良佐 曾芳屏.钽铌冶金学[M].北京:稀有金属冶金学会,1998.232-254.

2韩建设.氧化铌生产工艺及装备的进展[J].稀有金属与硬质合金,2003,31(1):35-38. 被引量:14

1唐德胜,晏慧娟.钽铌氢氧化物洗水回用工艺研究[J].稀有金属与硬质合金,2010,38(4):43-45.

2晏慧娟,唐德胜.传统工艺生产氧化钽(铌)除杂技术特点及研究进展[J].稀有金属与硬质合金,2016,44(4):14-19. 被引量:4

1王常清,易艳萍,曹小华,严平.以铌铁作为铌矿替代原料生产高纯氧化铌的研究[J].有色金属:冶炼部分,2018(9):40-43. 被引量:2

2鲁东,喻文斌,王诗海,张伟宁,郭洪范.结晶法和萃取法制备高纯氧化铌的研究[J].广州化工,2020,48(20):53-54. 被引量:1

3颉维平,喻文斌,鲁东,李辉,张伟宁,郭洪范.以汞为介质分离钽、铌金属废料的研究[J].中国金属通报,2020(16):228-229.

4潘岩,鄢锋,郭徽,唐昭辉,杨静雅,曾祥吉.有色金属冶炼自动控制研究现状与展望[J].中国有色金属学报,2021,31(1):96-105. 被引量:2

1方勤升,王庆生,钱晓杨,张信龙.反浮选—冷结晶生产氯化钾工艺过程的优化[J].无机盐工业,2001,33(5):32-33. 被引量:11

2何之华,汪继清,杨文赋.工业磷酸用氯化钠、硅酸钠脱氟的实验研究[J].磷肥与复肥,2009,24(2):21-23. 被引量:2

3陈勇,张品三,杨金顺,应慧敏.联二脲生产中缩合工艺的实验研究[J].氯碱工业,2006,42(6):30-32. 被引量:5

4陈红武.氧化铝生产中氢氧化铝洗涤探讨[J].铝镁通讯,2010(2):4-6.

5骆艳华,陈思学,王凡,王克玉.硫酸锰直接制备四氧化三锰的研究[J].矿业快报,2008,24(2):17-19. 被引量:8

6李恩超,尹婷婷.焦化反渗透浓水除氟试验研究[J].冶金动力,2015(4):50-53. 被引量:3

7程瑶,范宝安,段利中,余凡.两步法制湿法磷酸过程中除氟效果的研究[J].化工矿物与加工,2015,44(12):9-12.

8盛俊.去除锌冶炼尾气吸收液中氟离子的试验研究[J].有色金属设计,2016,43(4):14-17.

9马伟,罗洪杰,姚鸿海,董宝林.粗氧化锌制备活性氧化锌及其有关性能分析[J].有色矿冶,1996,12(6):32-34. 被引量:3

10李兵,甘顺鹏.粗粒氯化钾浮选工艺试验研究[J].有色金属文摘,2015,30(3):160-161. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ135.12[化学工程—无机化工]

Citation Information:

Research is made on the technological improvement of the original precipitation and pressure washing for preparation of NbO(H)_5.Comparison is made between the calcinators for NbO(H)_5.The results showed that the problem of F removal out of NbO(H)_5 washing solution from precipitation of high-concentration(Nb_2O_5>120 g/L)Nb solution can be solved through pretreatment with the addition of diluent.The new pressure washing process is characterized byhigher washing water temperature,more pulp-conditioning times,higher F-removal efficiency, water-saving and more up-to-standard Nb_2O_5 product

quote

GB/T 7714-2015 [1] DENG Xiao-fen, WANG Cai-ming. Research on Reduction of F^- Content in Nb_2O_5[J]. Rare Metals and Cemented Carbides, 2005(1): 11-13.
MLA [1] DENG Xiao-fen, and WANG Cai-ming. "Research on Reduction of F^- Content in Nb_2O_5." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 11-13.
APA [1] DENG Xiao-fen, & WANG Cai-ming. (2005). Research on Reduction of F^- Content in Nb_2O_5. Rare Metals and Cemented Carbides(1), 11-13.
IEEE [1] DENG Xiao-fen and WANG Cai-ming, "Research on Reduction of F^- Content in Nb_2O_5," Rare Metals and Cemented Carbides, no. 1, pp. 11-13, 2005. keywords: {niobium solution;precipitation;pressure washing;calcinations;Nb_2O_5;F-removal}