Feasibility Study of Direct Extraction of Rare Earth from Bauxite in a Mine AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the feasibility of RE extraction from RE-containing bauxite ore newly found in somewhere in China.In order to know whether is it existed in the adsorption phase,investigation is made on the feasibility of extracting rare earths by means of ion exchange method,i.e.percolation and agitation leaching with saltsolution.According to the IEX test results and based on the conclusion of XRD about alumina,the results of selective rare earths leaching,we concluded the rate of adsorption type in all of the rare earths mineral that existed in bauxite ore is very low,the majority is independent rare earths mineral.

KeyWords AITranslate

bauxite ore rare earth ion exchange acid leaching

1黄春辉.稀土元素[M].北京:科学出版社,1998.374.

1庹必阳,王建丽,张覃.稀土元素在铝土矿中的赋存状态及利用现状[J].稀土,2007,28(1):117-119. 被引量:29

2唐波,付勇,龙克树,龙珍,王天顺,刘阳,杨颖.中国铝土矿含铝岩系伴生稀土资源分布特征及富集机制[J].地质学报,2021,95(8):2284-2305. 被引量:8

1吴艳艳,秦勇,易同生.贵州凯里梁山组高硫煤中稀土元素的富集及其地质成因[J].地质学报,2010,84(2):280-285. 被引量:32

2谭洪旗,刘玉平.氧化铝赤泥的综合利用及回收工艺探讨[J].中国矿业,2011,20(4):78-81. 被引量:7

3黄宝贵,张志勇,杨林,高静,李玉茹,陈述.中国化学物相分析研究的新成就(下)[J].中国无机分析化学,2011,1(3):8-15. 被引量:9

4胡志中,杨波,杜谷,徐金沙,程江,王凤玉.铝土矿地质研究中分析技术应用进展[J].世界科技研究与发展,2011,33(6):963-965. 被引量:4

5张正伟,李玉娇,周灵洁,吴承泉.黔东南铝土矿含矿岩系“煤-铝-铁结构”及地球化学特征[J].地质学报,2012,86(7):1119-1131. 被引量:20

6王建丽,黄雄源,刘竹林.从粉煤灰中浮选富集碳的试验研究[J].湖南工业大学学报,2012,26(3):16-19.

7李军敏,丁俊,尹福光,廖朝贵,陈阳,吕涛,陈莉.渝南申基坪铝土矿矿区钪的分布规律及地球化学特征研究[J].沉积学报,2012,30(5):909-918. 被引量:15

8陈华,姚会禄,陈启飞.黔中地区含铝岩系中钪的分布及丰度研究[J].贵州地质,2012,29(4):270-274. 被引量:3

9李军敏,陈莉,徐金沙,闫武,吕涛,杨波,陈阳.渝南大佛岩矿区铝土矿碎屑锆石中钪的赋存形式研究[J].沉积学报,2013,31(4):630-638. 被引量:13

10李再会,朱同兴,尹福光,吕涛.渝南与黔北铝土矿含矿岩系沉积时代探讨[J].地层学杂志,2013,37(4):499-504. 被引量:2

1曹明明,张建良,邢相栋,姜吉吉,毛瑞.硫酸渣含碳球团高温焙烧试验研究[J].烧结球团,2013,38(1):42-45. 被引量:4

2李京社,高增福,杨宏博,刘成松,黄婷.RH喷粉脱硫工艺物理模拟研究[J].河南冶金,2013,21(3):1-5.

3刘春奇,杨惠林,李大树.从废钯催化剂中回收钯──渗滤浸出法处理低品位废钯催化剂[J].有色矿冶,1996,12(4):34-37. 被引量:11

4马文源.硫脲浸出提取金[J].有色与稀有金属国外动态,1994(13):9-10.

5徐亚飞,李永刚,廖元双,杨大锦.石煤矿硫酸浸出提取钒的研究[J].矿冶,2012,21(4):63-65. 被引量:8

6周坐东.高铁含锌烟尘浸出工艺研究[J].湖南有色金属,2012,28(3):35-37. 被引量:3

7李博,刘述平,刘东,邹建华,刘峰,徐凌飞,唐湘平.低品位稀有金属复合矿的浸出性能研究[J].稀有金属与硬质合金,2015,43(1):18-20. 被引量:2

8李林,刘金辉,刘亚洁,刘艳,田娟.铀矿石粒径对细菌渗滤浸出的研究[J].有色金属:冶炼部分,2006(3):39-41. 被引量:2

9陈庆根.石煤钒矿提钒工艺技术的研究进展[J].矿产综合利用,2009(2):30-34. 被引量:35

10郭相玲.影响铁精矿K_2O、Na_2O、SiO_2含量的因素分析[J].冶金标准化与质量,2003,41(1):9-12. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF111.31[冶金工程—冶金物理化学]

Citation Information:

Study is made of the feasibility of RE extraction from RE-containing bauxite ore newly found in somewhere in China.In order to know whether is it existed in the adsorption phase,investigation is made on the feasibility of extracting rare earths by means of ion exchange method,i.e.percolation and agitation leaching with saltsolution.According to the IEX test results and based on the conclusion of XRD about alumina,the results of selective rare earths leaching,we concluded the rate of adsorption type in all of the rare earths mineral that existed in bauxite ore is very low,the majority is independent rare earths mineral.

quote

GB/T 7714-2015 [1] ZHANG Chun, XIAO Lian-sheng. Feasibility Study of Direct Extraction of Rare Earth from Bauxite in a Mine[J]. Rare Metals and Cemented Carbides, 2005(1): 8-10.
MLA [1] ZHANG Chun, and XIAO Lian-sheng. "Feasibility Study of Direct Extraction of Rare Earth from Bauxite in a Mine." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 8-10.
APA [1] ZHANG Chun, & XIAO Lian-sheng. (2005). Feasibility Study of Direct Extraction of Rare Earth from Bauxite in a Mine. Rare Metals and Cemented Carbides(1), 8-10.
IEEE [1] ZHANG Chun and XIAO Lian-sheng, "Feasibility Study of Direct Extraction of Rare Earth from Bauxite in a Mine," Rare Metals and Cemented Carbides, no. 1, pp. 8-10, 2005. keywords: {bauxite ore;rare earth;ion exchange;acid leaching}