Effects of Two Different Dispersants on Agglomeration of ITO Powder AITranslate

School of Materials and Engineering, Central South University;School of Materials and Engineering, Central South University;School of Materials and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nano-ITO powder is prepared with sol-gel process.Study is made on the effects of different dispersants on powder agglomeration.The structure and morphology of powders are analyzed through differential thermal analysis(DTA),X-ray diffractometer(XRD),scan electron microscope(SEM).The result shows that the two dispersants have obvious effects on reduction of agglomeration of ITO powder,No.2 dispersant is better than No.1,but the grain size of powder with No.2 dispersant is smaller than that with No.1 dispersant, and both of them have little effect on the structures and morphology of the said product.

KeyWords AITranslate

sol-gel process nano ITO powder dispersant agglomeration

1王剑华,郭玉忠.超细粉制备方法及其团聚问题[J].昆明理工大学学报:理工版,1997,22(1):71-77. 被引量:30

2何小虎,韦莉.铟锡氧化物及其应用[J].稀有金属与硬质合金,2003,31(4):51-55. 被引量:22

3黄培云.粉末冶金原理[M].北京:冶金工业出版社,1981..

4征茂平,金燕苹,顾明元,金国良.Sol-Gel法制备有机改性硅酸盐及其掺杂复合光学材料研究进展[J].功能材料,2000,31(2):127-129. 被引量:11

5Marsumoto R, et al. Analysis of powder compaction using a conpaction rate diagram[J] .J Am Ceram Soc, 1990, 73(2):465.

6Granqvist C G. et al .Transparent and conducting ПО films:new develognents and applications[J] .Tlain Solid Films, 2002, 411 :1.

7Ota R. et al. Fabrication of indiura- tin- oxide films by dip coating process using ethanol solution of chlorides and surfacrants[J] .Thin Solid Films, 2002, 411:42.

1肖劲,万烨,李劼.AACH热分解制备超细α-Al_2O_3粉末[J].中国有色金属学报,2006,16(12):2120-2125. 被引量:3

2崔升,林本兰,黄杏芳,沈晓冬.锡掺杂的氧化铟纳米粉体的表面修饰与改性[J].材料科学与工艺,2008,16(3):338-341.

3黎铉海,魏坤,梁信源.化学液相共沉淀法制备ITO纳米粉体的工艺研究[J].金属矿山,2008(9):73-77. 被引量:3

4黎铉海,魏坤,梁信源.化学液相共沉淀法制备ITO纳米粉体的新工艺研究[J].化工技术与开发,2008,37(10):1-6. 被引量:1

5刘喜波,陈派明,杨硕,王政红,张秀勤.退火处理对铟锡氧化物粉末的影响[J].材料导报,2011,25(18):30-34.

1王伟礼,毕见强,邢政,管培强,张政,孙凌云.氯化铵对AACH热分解制备纳米α-Al_2O_3的影响[J].人工晶体学报,2009,38(2):309-312. 被引量:5

2饶焰高,饶平根,薛佳祥,李伟信,吕明,吴建青.AACH热分解法制备α-Al2O3超细粉末[J].人工晶体学报,2009,38(3):782-787.

3石志霞,余章龙,张碧田,王星明,储茂友,段华英.AACH在柠檬酸铝制备多孔氧化铝中的应用研究[J].稀有金属,2012,36(1):115-119. 被引量:1

4崔晓芳,郗雨林.共沉淀法制备纳米ITO粉末影响因素[J].热加工工艺,2013,42(8):66-68. 被引量:1

5王松,谢明,王塞北,杨云峰,付作鑫.高密度氧化铟锡(ITO)靶材制备工艺的研究进展[J].材料导报:纳米与新材料专辑,2013,27(1):207-210. 被引量:13

6蔡晓兰,彭刚,胡翠.铟锡氧化物纳米粉体的制备方法及分散的研究进展[J].粉末冶金技术,2014,32(4):290-295. 被引量:3

7李艳玲,邓卫华,冀克俭,朱杉,赵晓刚,周彤,高岩立.ITO成分分析标准物质的研制[J].化学分析计量,2016,25(2):8-11. 被引量:1

1崔晓芳,郗雨林.纳米ITO粉末制备技术[J].热加工工艺,2012,41(24):98-100.

2葛荣德,刘志宏,陈慧光,张多默,赵天从.球磨对ZrO_2(Y_2O_3)超细粉末性能的影响[J].稀有金属材料与工程,1995,24(2):45-49. 被引量:4

3崔晓芳,郗雨林.共沉淀法制备纳米ITO粉末影响因素[J].热加工工艺,2013,42(8):66-68. 被引量:1

4李晓杰,张越举,王金相,李瑞勇,赵铮.ITO纳米粉末爆炸压实烧结致密化陶瓷靶材研究[J].材料科学与工程学报,2004,22(1):12-14. 被引量:6

5董领锋,袁英.钼酸铵粉末费氏粒度的测试[J].中国钼业,1998,22(3):49-50.

6段雨露,叶锐,闫星辰,戴诚,谭江,徐国富.pH值和煅烧温度对共沉淀法制备ITO纳米粉末的影响[J].粉末冶金材料科学与工程,2014,19(3):413-420.

7朱协彬,段学臣.在纳米ITO粉末共沉淀法制备过程中pH值的影响[J].稀有金属与硬质合金,2006,34(2):8-11. 被引量:7

8刘喜波,陈派明,杨硕.铟锡氧化物陶瓷靶的制备[J].材料开发与应用,2011,26(3):26-29. 被引量:1

9张维佳,王天民,糜碧,洪轲.纳米ITO粉末及高密度ITO靶制备工艺的研究现状[J].稀有金属材料与工程,2004,33(5):449-453. 被引量:26

10张越举,李晓杰,孙贵磊,陈涛,王小红.制备ITO靶材的探索[J].真空,2005,42(6):27-32. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]

Citation Information:

Nano-ITO powder is prepared with sol-gel process.Study is made on the effects of different dispersants on powder agglomeration.The structure and morphology of powders are analyzed through differential thermal analysis(DTA),X-ray diffractometer(XRD),scan electron microscope(SEM).The result shows that the two dispersants have obvious effects on reduction of agglomeration of ITO powder,No.2 dispersant is better than No.1,but the grain size of powder with No.2 dispersant is smaller than that with No.1 dispersant, and both of them have little effect on the structures and morphology of the said product.

quote

GB/T 7714-2015 [1] MAO Li-ming, LI Li-li, DUAN Xue-chen. Effects of Two Different Dispersants on Agglomeration of ITO Powder[J]. Rare Metals and Cemented Carbides, 2005(1): 5-7.
MLA [1] MAO Li-ming, et al., "Effects of Two Different Dispersants on Agglomeration of ITO Powder." Rare Metals and Cemented Carbides, no. 1, 2005, pp. 5-7.
APA [1] MAO Li-ming, LI Li-li, & DUAN Xue-chen. (2005). Effects of Two Different Dispersants on Agglomeration of ITO Powder. Rare Metals and Cemented Carbides(1), 5-7.
IEEE [1] MAO Li-ming, LI Li-li, and DUAN Xue-chen, "Effects of Two Different Dispersants on Agglomeration of ITO Powder," Rare Metals and Cemented Carbides, no. 1, pp. 5-7, 2005. keywords: {sol-gel process;nano ITO powder;dispersant;agglomeration}