Study on Thermal Stability of γ-Al2O3 Powders Modified by Samarium Doping AITranslate
Abstract AITranslate
Using aluminum nitrate(Al(NO3)3·9H2O)as the oxidizing agent,glycine(C2H5NO2)as the reducing agent,and samarium nitrate(Sm(NO3)3·6H2O)as the modifier,γ-Al2O3 powders were synthesized by solution combustion method.The products were characterized by XRD,SEM,BET and TG-DTG.The effects of roasting temperature and modifier addition on the phase of the products were analyzed and discussed.The experimental results show that theγ-Al2O3 powders with high thermal stability could be prepared under the molar ratio of aluminum nitrate(Al(NO3)3·9H2O)to glycine(C2H5NO2)of 3∶5,addition of modifier Sm(NO3)3·6H2O of 1%,roasting temperature of 1025℃,and roasting time of 4 h.And theγ-Al2O(3)powders have the characteristics of large specific surface area and stable structure,which can be used as the carrier of catalyst.
KeyWords AITranslate
1Xiaoyu Zhang,Qing Ma,Bibo Cheng,Jun Wang,Jinshan Li,Fude Nie.Research on KOH/La-Ba-Al_2O_3 catalysts for biodiesel production via transesterification from microalgae oil[J].天然气化学杂志:英文版,2012,21(6):774-779. 被引量:6
1胡文丽,陈卫,王洪涛.高致密性Yb^(3+)和Gd^(3+)双掺杂CeO_(2)中温电解质的合成及其电性能研究[J].安阳师范学院学报,2023(2):13-17.
2贾洋刚,陈诗洁,邵霞,程婕,林娜,方道来,冒爱琴,李灿华.高性能无钴化钙钛矿型高熵氧化物负极材料的制备及储锂性能研究[J].化学学报,2023,81(5):486-495. 被引量:1
3郑旭惠,何艺施,赵文荻,李佳蔓,黄慧茹,江烨琳,朱健,任学梁.甘氨酸-硝酸盐燃烧合成制备铜/铁基纳米催化剂及表征[J].云南化工,2023,50(6):30-32.
4杨泽波,刘勇,陈清蓉,唐金爽,朱本谦,朱修昆.混凝土用矿物掺合料超细化作用机理[J].材料导报,2023,37(S01):143-147.
5李兵,魏瑞军,吕仁仨,郑玉倩,樊绪永,张小衡.高温高盐低渗透油藏表面活性剂驱提高采收率技术研究[J].当代化工,2023,52(5):1236-1241.
6陈梦梦,何永佳,吕林女,ZHANG Xulong.Effect of High Content Limestone Powder on Microstructure and Mechanical Properties of Cement-based Materials[J].武汉理工大学学报:材料科学英文版,2023,38(3):557-566.
7孔祥鹏,武瑞晗,元培红,王瑞虹,吴跃焕.Raney Cu催化剂催化草酸二甲酯加氢反应失活与活性再生[J].工业催化,2023,31(6):22-27.
Basic Information:
DOI:
Chinese Library Classification Number:TQ132.2[化学工程—无机化工]
Citation Information:
Using aluminum nitrate(Al(NO3)3·9H2O)as the oxidizing agent,glycine(C2H5NO2)as the reducing agent,and samarium nitrate(Sm(NO3)3·6H2O)as the modifier,γ-Al2O3 powders were synthesized by solution combustion method.The products were characterized by XRD,SEM,BET and TG-DTG.The effects of roasting temperature and modifier addition on the phase of the products were analyzed and discussed.The experimental results show that theγ-Al2O3 powders with high thermal stability could be prepared under the molar ratio of aluminum nitrate(Al(NO3)3·9H2O)to glycine(C2H5NO2)of 3∶5,addition of modifier Sm(NO3)3·6H2O of 1%,roasting temperature of 1025℃,and roasting time of 4 h.And theγ-Al2O(3)powders have the characteristics of large specific surface area and stable structure,which can be used as the carrier of catalyst.
quote
| GB/T 7714-2015 | [1] WANG Li-ming, JIA Ya-wei, MENG Zhu, et al. Study on Thermal Stability of γ-Al2O3 Powders Modified by Samarium Doping[J]. Rare Metals and Cemented Carbides, 2023(3): 47-51. |
| MLA | [1] WANG Li-ming, et al., "Study on Thermal Stability of γ-Al2O3 Powders Modified by Samarium Doping." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 47-51. |
| APA | [1] WANG Li-ming, JIA Ya-wei, MENG Zhu, FU Li-ting, WU Jing, SONG Li-juan, & CHU Gang. (2023). Study on Thermal Stability of γ-Al2O3 Powders Modified by Samarium Doping. Rare Metals and Cemented Carbides(3), 47-51. |
| IEEE | [1] WANG Li-ming, JIA Ya-wei, MENG Zhu, FU Li-ting, WU Jing, SONG Li-juan, and CHU Gang, "Study on Thermal Stability of γ-Al2O3 Powders Modified by Samarium Doping," Rare Metals and Cemented Carbides, no. 3, pp. 47-51, 2023. keywords: {solution combustion method;samarium doping;samarium nitrate;γ-AlO;modification;thermal stability} |