Study on Denitration Performance of Manganese-Modified Sulfuric Acid Activated Rare Earth Tailings Catalyst AITranslate
Abstract AITranslate
Mn-modified sulfuric acid activated rare earth tailings catalyst was prepared by impregnation method to investigate the effects of sulfuric acid concentration and Mn modification amount on the denitration activity of the catalyst,and its performance was analyzed by BET,XRD,H2-TPR and NH3-TPD.The results show that with the sulfuric acid concentration of 3 mol/L,the reaction temperature window of the catalyst is 350~450℃and its best denitration efficiency of 67%is reached at 400℃.After the addition of 5%Mn,the reaction temperature window of the catalyst moves down to 250~350℃and the N2 selectivity is maintained above 70%with the best denitrification efficiency reaching 86%at 300℃.With the increase of the sulfuric acid concentration,the specific surface area of the catalyst first increases and then decreases,while the pore volume and pore size decrease rapidly.The sulfuric acid activation increases the number of acidic sites on the catalyst surface and improves the adsorption and desorption ability of the catalyst to NH3.Mn element exists in the amorphous form on the catalyst surface.The stronger redox ability of the manganese-modified catalyst in the low temperature section is the main reason for its lower reaction temperature window compared with the sulfuric acid activated catalyst.
KeyWords AITranslate
1侯丽敏,闫笑,乔超越,崔梦壳,武文斐,王建,徐国栋.从工艺矿物学角度分析稀土尾矿作为NH_(3)-SCR催化剂的可行性[J].中国稀土学报,2022,40(2):216-224. 被引量:3
2陈旺生,张成刚,胡发立,秦林波,赵波.硫酸改性烧结矿催化剂脱硝性能研究[J].烧结球团,2019,44(5):65-69. 被引量:3
3查贤斌,梁辉,归柯庭,蔡森,王瑞.铁矿石低温催化脱硝性能研究[J].工程热物理学报,2015,36(4):811-815. 被引量:6
4于国峰,顾月平,金瑞奔.Mn/TiO_2和Mn-Ce/TiO_2低温脱硝催化剂的抗硫性研究[J].环境科学学报,2013,33(8):2149-2157. 被引量:17
5陆良樑,李伟,郭士义,郭瑞堂,潘卫国.碱土金属Mg和Ca中毒催化剂的再生研究[J].上海电力学院学报,2016,32(4):344-348. 被引量:1
6付金艳,王振峰,白心蕊,崔梦壳,武文斐.γ-Al2O3酸性修饰稀土尾矿NH3-SCR脱硝性能[J].中国环境科学,2020,40(9):3741-3747. 被引量:10
1侯丽敏,胡志斐,乔超越,武文斐.硫酸浓度对Mn改性稀土尾矿催化剂NH_(3)-SCR脱硝性能的影响[J].稀有金属与硬质合金,2022,50(6):46-51. 被引量:1
2侯丽敏,栗浩博,乔超越,武文斐.锰修饰稀土尾矿催化剂NH_(3)-SCR性能研究[J].中国稀土学报,2023,41(2):287-295.
3吴小芳,许志泉,王琪,闫东东,刘吉玲,周峰.基于响应面的低温移动储罐轻量化数值模拟[J].辽宁化工,2023,52(1):65-68.
4陈相言.酸改性海泡石催化分子氧化环己烷一步制备己二酸[J].山西化工,2023,43(6):15-17.
5陈文明.试析T75UN可移动罐柜欧标的设计、制造、检验[J].中文科技期刊数据库(引文版)工程技术,2022(3):0318-0320.
6王晓军,鲁妮,付源益,逯畅,管美丽,王坤华,于昊.铌掺杂提高钨酸盐氧化锆固体酸催化剂表面酸性制备5-羟甲基糠醛[J].化学物理学报(英文),2023,36(3):319-328.
7殷成阳,侯铭,杨爽,毛迪,刘俊言.过渡金属改性Cu-SSZ-13分子筛脱硝催化剂研究进展[J].化工进展,2023,42(6):2963-2974.
8马金明,张群飞,肖长江.(1-x)BaTiO_(3-x)Bi(Ni_(0.5)Zr_(0.5))O_(3)陶瓷的制备和介电性能研究[J].陶瓷学报,2023,44(1):72-77.
9姜明海.金泥湿法处理工艺研究[J].世界有色金属,2023(4):22-25.
10许婧晖,祁聪,段浩,张红娟,余剑英.多聚磷酸对沥青高低温性能和老化性能的影响[J].科学技术与工程,2023,23(18):7952-7959.
Basic Information:
DOI:
Chinese Library Classification Number:TD983[矿业工程—选矿]
Citation Information:
Mn-modified sulfuric acid activated rare earth tailings catalyst was prepared by impregnation method to investigate the effects of sulfuric acid concentration and Mn modification amount on the denitration activity of the catalyst,and its performance was analyzed by BET,XRD,H2-TPR and NH3-TPD.The results show that with the sulfuric acid concentration of 3 mol/L,the reaction temperature window of the catalyst is 350~450℃and its best denitration efficiency of 67%is reached at 400℃.After the addition of 5%Mn,the reaction temperature window of the catalyst moves down to 250~350℃and the N2 selectivity is maintained above 70%with the best denitrification efficiency reaching 86%at 300℃.With the increase of the sulfuric acid concentration,the specific surface area of the catalyst first increases and then decreases,while the pore volume and pore size decrease rapidly.The sulfuric acid activation increases the number of acidic sites on the catalyst surface and improves the adsorption and desorption ability of the catalyst to NH3.Mn element exists in the amorphous form on the catalyst surface.The stronger redox ability of the manganese-modified catalyst in the low temperature section is the main reason for its lower reaction temperature window compared with the sulfuric acid activated catalyst.
quote
| GB/T 7714-2015 | [1] HOU Li-min, LIU Jia-lin, GAO Hong-min, et al. Study on Denitration Performance of Manganese-Modified Sulfuric Acid Activated Rare Earth Tailings Catalyst[J]. Rare Metals and Cemented Carbides, 2023(3): 52-58. |
| MLA | [1] HOU Li-min, et al., "Study on Denitration Performance of Manganese-Modified Sulfuric Acid Activated Rare Earth Tailings Catalyst." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 52-58. |
| APA | [1] HOU Li-min, LIU Jia-lin, GAO Hong-min, QIAO Chao-yue, HU Zhi-fei, & WU Wen-fei. (2023). Study on Denitration Performance of Manganese-Modified Sulfuric Acid Activated Rare Earth Tailings Catalyst. Rare Metals and Cemented Carbides(3), 52-58. |
| IEEE | [1] HOU Li-min, LIU Jia-lin, GAO Hong-min, QIAO Chao-yue, HU Zhi-fei, and WU Wen-fei, "Study on Denitration Performance of Manganese-Modified Sulfuric Acid Activated Rare Earth Tailings Catalyst," Rare Metals and Cemented Carbides, no. 3, pp. 52-58, 2023. keywords: {rare earth tailings;NH-SCR catalyst;sulfuric acid activation;Mn modification;denitration performance} |