daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High-Temperature Stable Narrowband Near-Infrared Phosphor-Converted Light-Emitting Diode Based on Melt-Grown CsPbCl3: Yb3+ Crystal AITranslate

AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Narrowband near-infrared (NIR) phosphor-converted light-emitting diodes (pc-LEDs) featuring low full-width at half maximum (FWHM) and high conversion efficiency are crucial for chemical content evaluation, light therapy, and bioimaging. Recently, Yb3+ doped CsPbCl3 nanocrystals (NCs) have emerged as promising phosphors for NIR pc-LEDs, delivering narrowband 980 nm emission with an FWHM below 50 nm and a photoluminescence quantum yield (PLQY) exceeding 100%. However, the practical employment of CsPbCl3: Yb3+ NCs is limited by their poor thermal stability. In this work, we present a high-temperature stable, melt-grown CsPbCl3: Yb3+ single crystal (SC) and narrowband NIR pc-LEDs fabricated from CsPbCl3: Yb3+ powder and violet LED chips. Our pc-LEDs achieve a low FWHM of 46.81 nm and a high conversion efficiency of 2.44% at a drive current of 20 mA. More importantly, our pc-LEDs exhibit exceptional thermal stability, retaining 98.2% of their PL emission intensity at 360 K. Finally, these NIR pc-LEDs successfully demonstrate applications in night vision, vein imaging, non-destructive testing, and the detection of early fruit bruises. This work underscores the significant potential of narrowband 980 nm pc-LEDs based on CsPbCl3: Yb3+ crystal for diverse applications.

KeyWords AITranslate

NIR luminescence phosphor-converted LED rare-earth ion doping thermal stability Yb3+doped CsPbCl3 crystal
No data

Basic Information:

DOI:

Chinese Library Classification Number:

Citation Information:

Narrowband near-infrared (NIR) phosphor-converted light-emitting diodes (pc-LEDs) featuring low full-width at half maximum (FWHM) and high conversion efficiency are crucial for chemical content evaluation, light therapy, and bioimaging. Recently, Yb3+ doped CsPbCl3 nanocrystals (NCs) have emerged as promising phosphors for NIR pc-LEDs, delivering narrowband 980 nm emission with an FWHM below 50 nm and a photoluminescence quantum yield (PLQY) exceeding 100%. However, the practical employment of CsPbCl3: Yb3+ NCs is limited by their poor thermal stability. In this work, we present a high-temperature stable, melt-grown CsPbCl3: Yb3+ single crystal (SC) and narrowband NIR pc-LEDs fabricated from CsPbCl3: Yb3+ powder and violet LED chips. Our pc-LEDs achieve a low FWHM of 46.81 nm and a high conversion efficiency of 2.44% at a drive current of 20 mA. More importantly, our pc-LEDs exhibit exceptional thermal stability, retaining 98.2% of their PL emission intensity at 360 K. Finally, these NIR pc-LEDs successfully demonstrate applications in night vision, vein imaging, non-destructive testing, and the detection of early fruit bruises. This work underscores the significant potential of narrowband 980 nm pc-LEDs based on CsPbCl3: Yb3+ crystal for diverse applications.

quote

GB/T 7714-2015 [1] High-Temperature Stable Narrowband Near-Infrared Phosphor-Converted Light-Emitting Diode Based on Melt-Grown CsPbCl3: Yb3+ Crystal[J]. Rare Metals, 2026(3).
MLA [1] "High-Temperature Stable Narrowband Near-Infrared Phosphor-Converted Light-Emitting Diode Based on Melt-Grown CsPbCl3: Yb3+ Crystal." Rare Metals, no. 3, 2026.
APA [1] (2026). High-Temperature Stable Narrowband Near-Infrared Phosphor-Converted Light-Emitting Diode Based on Melt-Grown CsPbCl3: Yb3+ Crystal. Rare Metals(3).
IEEE [1] "High-Temperature Stable Narrowband Near-Infrared Phosphor-Converted Light-Emitting Diode Based on Melt-Grown CsPbCl3: Yb3+ Crystal," Rare Metals, no. 3, 2026. keywords: {NIR luminescence;phosphor-converted LED;rare-earth ion doping;thermal stability;Yb3+doped CsPbCl3 crystal}