Preparation of ZnS Nanocrystals by Reduction Method AITranslate
Abstract AITranslate
ZnS nanocrystals were synthesized by direct reduction, with zinc sulfate as the sulfur & zinc source and hexamethylene tetramine as the reducer. The structure and morphology of the as-prepared samples were characterized by XRD and SEM,and the result shows that they are pure face-centered cubic ZnS nanocrystals. Meanwhile,the influences of reaction time and temperature on the products were studied,and the reduction mechanism was also investigated.
KeyWords AITranslate
1牛新书,刘艳丽,徐甲强.室温固相合成纳米ZnS及其气敏性能研究[J].无机材料学报,2002,17(4):817-821. 被引量:19
2杨信成,薛永强,石建青.均匀沉淀法制备不同粒径的纳米硫化锌[J].无机盐工业,2011,43(7):13-15. 被引量:9
3常鹏,刘肃,王秀华,唐莹.水热法制备硫化锌纳米线及性能研究[J].人工晶体学报,2007,36(4):817-820. 被引量:12
4柴多里,刘忠煌,杨保俊.气-固相还原硫酸盐制备系列硫化物纳米晶[J].无机化学学报,2010,26(1):153-156. 被引量:1
5王玲,戴金辉,刘西中.层状硫化锌的溶剂热法制备[J].材料导报,2011,25(2):57-59. 被引量:4
6刘金成,於黄忠,覃东欢,彭俊彪,曹镛.化学沉淀法用于多种形貌ZnS纳米晶的可控合成[J].化学学报,2008,66(8):1003-1007. 被引量:6
7郝伟,孙中溪.沉淀溶解法制备纳米硫化锌[J].无机化学学报,2007,23(3):461-465. 被引量:10
8刘淑玲,石强强,程芳玲.过渡金属硫化物纳米晶的溶剂热合成与表征[J].原子与分子物理学报,2010,27(2):372-376. 被引量:1
9李云峰,兰尧中.纳米硫化锌的制备与应用状况[J].湿法冶金,2007,26(3):123-127. 被引量:6
1张翔,黄金亮,李丽华,顾永军,李谦.ZnS:Cu纳米晶的制备及发光性质[J].现代化工,2014,34(2):82-84.
1李吉蓉,黄剑锋,曹丽云,吴建鹏,贺海燕.声化学法合成ZnS纳米晶及反应动力学研究[J].人工晶体学报,2008,37(5):1264-1267. 被引量:3
2刘俊业,刘春旭,许武,李丹.玻璃基质中ZnS纳米晶Mn^(2+)掺杂的两种组态下载流子限域[J].发光学报,1997,18(4):323-325.
3陈建设,王文祥,赵合全.合成氨铁钴催化剂还原行为的研究[J].化学研究与应用,1993,5(4):70-74.
4蔡金法.氨合成催化剂升温还原时间的确定[J].小氮肥设计技术,2001,22(1):25-25.
5秦艳利,孙正,石广立,柴萌,宫铖.表面官能团对硫化锌/碳纳米管复合材料的制备及光致发光光谱性能影响[J].沈阳理工大学学报,2016,35(6):48-52.
6柴多里,储志兵,杨保俊,张柠.纳米四氧化三铁吸附水溶液中砷的研究(英文)[J].硅酸盐学报,2011,39(3):419-423. 被引量:11
7冯守爱,宋昌,杜桂香,赵江红,朱珍平.爆炸辅助气相沉积法制备炭纳米线的研究[J].新型炭材料,2010,25(2):97-103.
8王建荣,杨中喜,王英姿.Ti^(3+)在Sol-gel多孔磷光SiO_2干凝胶中的发光[J].硅酸盐通报,2002,21(4):28-30. 被引量:1
9袁定胜,张静娴,刘应亮,胡春凤.化学镀CuNiP-碳纳米管复合材料的制备与表征[J].暨南大学学报:自然科学与医学版,2005,26(5):653-656. 被引量:1
10姚素薇,刘冰,张卫国,郭鹤桐,杉山孝雄.电沉积Ni-Co合金及其结构研究[J].电镀与精饰,1996,18(5):7-10. 被引量:15
Basic Information:
DOI:
Chinese Library Classification Number:TQ132.41[化学工程—无机化工]
Citation Information:
ZnS nanocrystals were synthesized by direct reduction, with zinc sulfate as the sulfur & zinc source and hexamethylene tetramine as the reducer. The structure and morphology of the as-prepared samples were characterized by XRD and SEM,and the result shows that they are pure face-centered cubic ZnS nanocrystals. Meanwhile,the influences of reaction time and temperature on the products were studied,and the reduction mechanism was also investigated.
quote
| GB/T 7714-2015 | [1] YANG Yu, YANG Shao-dong, CHENG Bo, et al. Preparation of ZnS Nanocrystals by Reduction Method[J]. Rare Metals and Cemented Carbides, 2012(6): 56-59. |
| MLA | [1] YANG Yu, et al., "Preparation of ZnS Nanocrystals by Reduction Method." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 56-59. |
| APA | [1] YANG Yu, YANG Shao-dong, CHENG Bo, XIA Lun-peng, YIN Xin-min, & CHAI Duo-li. (2012). Preparation of ZnS Nanocrystals by Reduction Method. Rare Metals and Cemented Carbides(6), 56-59. |
| IEEE | [1] YANG Yu, YANG Shao-dong, CHENG Bo, XIA Lun-peng, YIN Xin-min, and CHAI Duo-li, "Preparation of ZnS Nanocrystals by Reduction Method," Rare Metals and Cemented Carbides, no. 6, pp. 56-59, 2012. keywords: {ZnS nanocrystal reduction hexamethylene tetramine} |