The Latest Development of Super Capacitor and its Electrode Material of Nanometer MoO_3 AITranslate
Abstract AITranslate
The working principle and application development of super capacitor are introduced, and the latest development of three series of electrode materials is summarized including carbon materials, metal oxides and conductive polymers. The future application of nanometer MoO3 as the electrode material of super capacitor is intensively analyzed.
KeyWords AITranslate
1Gamby J, Tabema P L, Simon D,et a l. Studies and char- acterizations of supercapacitors [J]. J Power Sources, 2001,101 (1) : 109-116.
2Saliger,R, Fischer U, Herta C, et al. High surface area carbon aerogels for supercapacitors[J]. Journal of Non- Crystalline Solids,1998,225(1) :81-85.
3江奇,瞿美臻,张伯兰,于作龙.电化学超级电容器电极材料的研究进展[J].无机材料学报,2002,17(4):649-656. 被引量:43
4Leeh Y, Goodenough J B. Ideal supercapacitor behavior of amorphous V2Os nil20 potassium chloride (KC1) aqueous solution[J]. Solid State Chem, 1999,148(1):81 -84.
5赵鹏,赵亚丽.多形态三氧化钼粉体的水热法制备[J].无机盐工业,2009,41(5):15-17. 被引量:10
6祁琰媛,陈文,麦立强,胡彬,金伟.过氧钼酸溶胶制备的MoO_3纳米带及其电化学性能研究[J].稀有金属,2007,31(1):67-71. 被引量:11
7Hassan M F, Guo Z P, Chen Z, et al. Carbon-coated MoO3 nanobelts as anode materials for lithium ion bat- teries[J]. Power Sources, 2010,195 : 2 372-2 376.
8Song J M,Wang X,Ni X M,et al. Preparation of hexa- gonal-MoO3 and electrochemical properties of lithium intercalation into the oxide[J]. Materials Research Bulle- tin,2005,40(10):1 751-1 756.
9Lee S H,Deshpande R,Benhammou D,etal. Metal oxide nanoparticles for advanced energy applications[J]. Thin Solid Films,2009,517:3 591-3 595.
10高海燕,彭文修,魏欣,亓瞻,赵倩倩,杨加芹,焦丽芳,司玉昌,袁华堂.纳米三氧化钼的制备与电化学性能研究[J].南开大学学报:自然科学版,2010,43(5):72-77. 被引量:11
1周晓平,冯宗财,马琳,许丽梅,徐旭耀.片状三氧化钼的合成及超电容性能研究[J].电源技术,2015,39(8):1708-1710.
2陈明华,刘威铎,范鹤,李宏武,陈庆国.钼基化合物超级电容器电极材料研究进展[J].哈尔滨理工大学学报,2020,25(6):1-9. 被引量:6
1韩曼舒,周志浩,李誉,陈明华,陈庆国.钛基材料在超级电容器中的研究进展[J].哈尔滨理工大学学报,2021,26(4):1-8. 被引量:3
2董国涛,王静,葛烨,胡天豪.单金属氧化物电极研究现状[J].广州化工,2021,49(17):14-17. 被引量:1
3孙翔,罗志斌.MnO_(2)在超级电容器电极材料中的研究进展[J].材料开发与应用,2022,37(4):93-100.
4曾鑫渔,方志刚,井润田,王倩,毛智龙,朱依文.团簇NiCo_(2)S_(4)极性及成键性质[J].哈尔滨理工大学学报,2023,28(1):129-136.
5蔡丹,张忠洋,武智惠,张学磊,赵荣达,相珺.NiMoS_(4)@MoS_(3)复合电极的制备及电化学性能研究[J].稀有金属与硬质合金,2023,51(4):47-51.
6席艳杰,马琳,孙劲毅.硫化钼分层纳米材料的制备及赝电容性能综合实验设计[J].创新教育研究,2022,10(8):2018-2026.
Basic Information:
DOI:
Chinese Library Classification Number:TM535[电气工程—电器]
Citation Information:
The working principle and application development of super capacitor are introduced, and the latest development of three series of electrode materials is summarized including carbon materials, metal oxides and conductive polymers. The future application of nanometer MoO3 as the electrode material of super capacitor is intensively analyzed.
quote
| GB/T 7714-2015 | [1] GONG Fang-fang, LI Ji-wen, WEI Shi-zhong. The Latest Development of Super Capacitor and its Electrode Material of Nanometer MoO_3[J]. Rare Metals and Cemented Carbides, 2012(6): 53-55. |
| MLA | [1] GONG Fang-fang, et al., "The Latest Development of Super Capacitor and its Electrode Material of Nanometer MoO_3." Rare Metals and Cemented Carbides, no. 6, 2012, pp. 53-55. |
| APA | [1] GONG Fang-fang, LI Ji-wen, & WEI Shi-zhong. (2012). The Latest Development of Super Capacitor and its Electrode Material of Nanometer MoO_3. Rare Metals and Cemented Carbides(6), 53-55. |
| IEEE | [1] GONG Fang-fang, LI Ji-wen, and WEI Shi-zhong, "The Latest Development of Super Capacitor and its Electrode Material of Nanometer MoO_3," Rare Metals and Cemented Carbides, no. 6, pp. 53-55, 2012. keywords: {super capacitor;electrode materials;nanometer MoO3;working principle;application develop-ment} |