daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress in Preparation Methods of Vanadium Metal AITranslate

College of Metallurgy and Energy,North China University of Technology;College of Metallurgy and Energy,North China University of Technology;College of Metallurgy and Energy,North China University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

China is rich in vanadium resources.Vanadium metal is widely used in steel, national defense, aviation and other fields because of its excellent performance.At present, vanadium metal is mainly prepared by metallothermic reduction, followed by refining to obtain high-purity vanadium metal.In this paper, several typical methods of the preparation and refining of crude vanadium are analyzed and summarized, and it is pointed out that the development direction of vanadium preparation is high yield, low cost, low energy consumption, and short process in the future.

KeyWords AITranslate

vanadium metal preparation of crude vanadium refining of crude vanadium research progress development direction

1卢伟亮,张盈,孙沛,郑诗礼,乔珊,张洋,李平,张懿.金属钒的制备方法综述[J].过程工程学报,2021,21(10):1117-1131. 被引量:1

2王焱辉,刘奇,李方,薄新维,王小宇,何浩然.电子束熔炼法制备高纯金属钒的实验研究[J].稀有金属,2020,44(8):891-896. 被引量:8

3孔亚鹏,李斌川,陈建设,刘奎仁,韩庆.氟化物熔盐中快速电脱氧制备金属钒及其机理[J].稀有金属材料与工程,2018,47(6):1824-1829. 被引量:3

4Wei Weng,Mingyong Wang,Xuzhong Gong,Zhi Wang,Zhancheng Guo.Thermodynamic analysis on the direct preparation of metallic vanadium from NaVO_3 by molten salt electrolysis[J].中国化学工程学报:英文版,2016(5):671-676. 被引量:4

5吴春亮,王宝华,陈兴,王海龙,王娜.熔盐中钙热还原钒酸钙制备金属钒粉[J].有色金属:冶炼部分,2019,0(6):52-54. 被引量:3

1李杰,何春林,刘云,齐明伟,刘尊章.D201树脂对四价和五价钒离子的吸附-解吸性能研究[J].广东化工,2022,49(24):7-11.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

China is rich in vanadium resources.Vanadium metal is widely used in steel, national defense, aviation and other fields because of its excellent performance.At present, vanadium metal is mainly prepared by metallothermic reduction, followed by refining to obtain high-purity vanadium metal.In this paper, several typical methods of the preparation and refining of crude vanadium are analyzed and summarized, and it is pointed out that the development direction of vanadium preparation is high yield, low cost, low energy consumption, and short process in the future.

quote

GB/T 7714-2015 [1] HOU Shuai, TIAN Ying, LI Yun-gang. Research Progress in Preparation Methods of Vanadium Metal[J]. Rare Metals and Cemented Carbides, 2022(6): 22-26.
MLA [1] HOU Shuai, et al., "Research Progress in Preparation Methods of Vanadium Metal." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 22-26.
APA [1] HOU Shuai, TIAN Ying, & LI Yun-gang. (2022). Research Progress in Preparation Methods of Vanadium Metal. Rare Metals and Cemented Carbides(6), 22-26.
IEEE [1] HOU Shuai, TIAN Ying, and LI Yun-gang, "Research Progress in Preparation Methods of Vanadium Metal," Rare Metals and Cemented Carbides, no. 6, pp. 22-26, 2022. keywords: {vanadium metal;preparation of crude vanadium;refining of crude vanadium;research progress;development direction}