Technological Research and Industrial Application of Centralized Saponification with Calcium Hydroxide Powder of Rare Earth Extraction Organic Phase AITranslate
Abstract AITranslate
The direct saponification of rare earth extraction organic phase with calcium hydroxide powder was studied.The experimental results show that the saponification values of P507 organic phase and naphthenic acid organic phase are 0.55 mol/L and 0.72 mol/L,respectively, with clear appearance and good fluidity through the process of direct saponification by using calcium hydroxide powder.When the calcium saponified organic phase is subject to extraction reaction with rare earth chloride feed liquid, the separation time of P507 organic phase is 40 s with the rare earth load of 0.19 mol/L,and the separation time of naphthenic acid organic phase is 180 s with the rare earth load of 0.19 mol/L.Based on the test data, a centra-lized calcium hydroxide powder direct saponification technology was developed.After years of industrial operation, the results show that calcium hydroxide powder directly saponifies the P507 organic phase and the naphthenic acid organic phase with good fluidity, fast phase separation, little impact on product quality, and no long-term adverse effects on the organic phase.And the saponification cost is only 16.5% of that of liquid alkali.Since the saponifier is a powder, there is no need for emulsion and the saponification reaction with the organic phase directly occurs.Compared with the saponification of liquid alkali, the wastewater greatly reduces and the environmental benefits are quite good.
KeyWords AITranslate
1王斌,李虎平,胡广寿,李甜甜,胡志龙.不同镁盐在硫酸萃取体系下皂化P507的对比[J].世界有色金属,2019,0(7):252-253. 被引量:2
2王道广,王均凤,张香平,王毅霖,张晓飞.离子液体在稀土萃取分离中的应用[J].化工学报,2020,71(10):4379-4394. 被引量:10
3张晓兵,张小林.现代分离技术在稀土分离中的应用[J].有色冶金节能,2019,35(6):8-10. 被引量:3
4雷金勇.稀土矿萃取分离过程皂化工艺改造工程[J].资源节约与环保,2015,30(2):62-62. 被引量:4
5张馨予,孙志敏.P204-P350萃取体系萃取稀土铈的研究[J].湖南有色金属,2022,38(1):33-36. 被引量:2
6詹光,黄草明,朱景和,刘风琴.南方离子型稀土冶炼废水治理现状与展望[J].矿产综合利用,2018(3):18-25. 被引量:19
7莫国荣,张亮玖.离子型稀土冶炼萃取废水处理工艺研究[J].冶金与材料,2019,39(1):59-60. 被引量:6
8刘瑞金,赵治华,桑晓云,许慧,高媛.稀土萃取分离皂化工艺及其废水资源化探讨[J].稀土,2015,36(4):132-137. 被引量:20
9蔡维中,左陆珅.一体式厌氧氨氧化工艺处理稀土废水脱氮性能的研究[J].化工安全与环境,2022,35(31):15-18. 被引量:1
10崔佳娜,王明.稀土萃取分离皂化工艺研究进展[J].稀有金属与硬质合金,2017,45(2):1-5. 被引量:13
1胡水龙,田钰.钱氏兄弟的稀土情怀——记中稀(江苏)稀土有限公司劳模标兵钱建龙、钱建平[J].中国有色金属,2022(22):44-45.
2中科稀土:实现从基础研究到产业化跨越[J].东西南北,2022(11):38-38.
3粟春兰,杨宪,郑红,曾婷,张雪.木香籽油理化性质及脂肪酸组成分析[J].粮食与油脂,2023,36(1):75-77.
4尹伟强,赵锦辉,赵龙胜,刘德鹏,齐少雷,冯宗玉.稀土萃余水相中乳化油滴稳定性及Al^(3+)水解破乳机制[J].稀有金属,2022,46(10):1322-1330.
5路嘉琦.高寒地区机场道面的病害及防治研究[J].中国新技术新产品,2022(22):116-118.
6王思捷,柳召刚,侯兆星.高品质碳酸镧的制备研究[J].当代化工研究,2023(2):179-181.
7吴蓓蕾.山楂茶复合果酒酿造工艺研究[J].食品工程,2022(4):41-43.
8冯荦荦,郭晓成,闫欣鹏,张润光,张有林.三叶木通籽油精炼前后理化指标及脂肪酸组成分析[J].粮食与油脂,2023,36(1):71-74. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
The direct saponification of rare earth extraction organic phase with calcium hydroxide powder was studied.The experimental results show that the saponification values of P507 organic phase and naphthenic acid organic phase are 0.55 mol/L and 0.72 mol/L,respectively, with clear appearance and good fluidity through the process of direct saponification by using calcium hydroxide powder.When the calcium saponified organic phase is subject to extraction reaction with rare earth chloride feed liquid, the separation time of P507 organic phase is 40 s with the rare earth load of 0.19 mol/L,and the separation time of naphthenic acid organic phase is 180 s with the rare earth load of 0.19 mol/L.Based on the test data, a centra-lized calcium hydroxide powder direct saponification technology was developed.After years of industrial operation, the results show that calcium hydroxide powder directly saponifies the P507 organic phase and the naphthenic acid organic phase with good fluidity, fast phase separation, little impact on product quality, and no long-term adverse effects on the organic phase.And the saponification cost is only 16.5% of that of liquid alkali.Since the saponifier is a powder, there is no need for emulsion and the saponification reaction with the organic phase directly occurs.Compared with the saponification of liquid alkali, the wastewater greatly reduces and the environmental benefits are quite good.
quote
| GB/T 7714-2015 | [1] ZHANG Jiang-hua, LUO Qi. Technological Research and Industrial Application of Centralized Saponification with Calcium Hydroxide Powder of Rare Earth Extraction Organic Phase[J]. Rare Metals and Cemented Carbides, 2022(6): 18-21. |
| MLA | [1] ZHANG Jiang-hua, and LUO Qi. "Technological Research and Industrial Application of Centralized Saponification with Calcium Hydroxide Powder of Rare Earth Extraction Organic Phase." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 18-21. |
| APA | [1] ZHANG Jiang-hua, & LUO Qi. (2022). Technological Research and Industrial Application of Centralized Saponification with Calcium Hydroxide Powder of Rare Earth Extraction Organic Phase. Rare Metals and Cemented Carbides(6), 18-21. |
| IEEE | [1] ZHANG Jiang-hua and LUO Qi, "Technological Research and Industrial Application of Centralized Saponification with Calcium Hydroxide Powder of Rare Earth Extraction Organic Phase," Rare Metals and Cemented Carbides, no. 6, pp. 18-21, 2022. keywords: {calcium hydroxide powder;centralized quantitative saponification;extraction organic phase;P507;naphthenic acid;rare earth separation} |