daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on High Efficient Flotation Recovery of Some Refractory Molybdenum Ore with High Mud Content and Low Grade AITranslate

FanKou Lead-Zinc Mine of Zhongjin Lingnan Nonfemet Co.,Ltd.;Changsha Sanbo Mining Technology Co.,Ltd.;School of Minerals Processing and Bioengineering,Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The molybdenum content in some molybdenum ore in Fujian is only 0.09%,and most molybdenum exists in molybdenites while a small amount of molybdenum exists in the form of molybdenum oxide ore.The gangue minerals mainly consist of easy-sliming silicate minerals and the flotation activity of the molybdenum ore is low,showing that it is the typical refractory molybdenum ore with high mud content and low grade.A novel surface promoter MCS was introduced to effectively enhance the surface activity of the molybdenum ore,thereby improving the molybdenum flotation recovery.The appropriate grinding fineness,MCS dosage,water glass dosage and collector CM dosage for the flotation were determined through condition experiments.The results show that by using the flotation machine,molybdenum concentrates with a Mo grade of 45.75%and Mo recovery of 82.18%can be obtained after one roughing,three scavenging and seven cleaning,but this process is lengthy and the production and operation costs are high.Through the combined flotation column-flotation machine process,the qualified molybdenum concentrates are gained with a Mo grade of 46.01%and Mo recovery of 87.81%after four cleaning.Therefore,it is re-commended as the principle process for the recovery of molybdenum from the molybdenum ore.

KeyWords AITranslate

high mud content low grade molybdenum ore flotation surface promoter

1肖丽聪.辽宁某钼矿选矿试验研究[J].有色矿冶,2021,37(4):25-29. 被引量:1

2陈志友,苏小琼,肖洪旭,张海平.云南某微细粒辉钼矿工艺矿物学与浮选回收技术研究[J].矿物学报,2021,41(3):287-293. 被引量:5

3缑明亮,武俊杰,崔长征,孙阳.辉钼矿选矿药剂及选矿工艺研究[J].有色金属:选矿部分,2013(3):74-77. 被引量:5

4代淑娟,刘烱天,杨树勇,张其东,李晓安.捕收剂DT-1在钼矿浮选中的应用研究[J].中国矿业,2012,21(5):81-83. 被引量:5

5林清泉,吴启明,戴智飞,曾令明,林智炜.微细粒辉钼矿浮选机理研究[J].矿冶工程,2021,41(3):37-41. 被引量:9

6曹占芳,钟宏,刘广义,王帅,夏柳荫.秘鲁含砷铜钼矿高效浮选试验研究[J].稀有金属与硬质合金,2012,40(3):1-4. 被引量:3

7李琳,吕宪俊.辉钼矿捕收剂的研究与应用[J].中国矿业,2011,20(3):61-64. 被引量:9

8陈丽娟,李治杭,姚辉,刘雁鹰,苏圣博.辉钼矿浮选药剂研究进展[J].现代矿业,2022,38(2):19-23. 被引量:5

9曹占芳,钟宏,姜涛,王帅,刘广义,夏柳荫.栾川钼矿高效选矿试验研究[J].稀有金属与硬质合金,2012,40(1):1-4. 被引量:9

10张宝元,钟宏.辉钼矿的浮选及其捕收剂的研究进展[J].矿产保护与利用,2010,30(3):51-54. 被引量:15

1王立军.柱机联合工艺处理某硅钙质磷矿的试验研究[J].化工矿物与加工,2018,0(5):4-7. 被引量:2

2吴迪,王洪岭,孟庆波,卜浩,高玉德,张晓刚.内蒙古某多金属矿铜锌分离试验研究[J].有色金属:选矿部分,2021(4):72-76. 被引量:5

3邓杰,毛益林,张俊辉,邓善芝,孙缘,段永华,杨安仓.煅烧-铵盐两步浸出法对磷矿浮选尾矿钙镁回收研究[J].化工矿物与加工,2023,52(1):39-47.

4王天义,田勇,徐凤乾.基于复合电液式的大惯量回转机构制动能量回收研究[J].机床与液压,2022,50(23):99-104.

5钟春晖,冯博,严华山,周鹰,刘刚,陈渊淦,宁湘菡,汪惠惠.三种有机抑制剂在辉钼矿与滑石浮选分离中的作用[J].中国有色金属学报,2022,32(12):3843-3852. 被引量:2

6朱云峰,刘方忠,韩伟斌.热电企业烟气深度余热回收研究[J].石油石化物资采购,2023(1):178-180.

7王家圆,郭军康,张蕾,郭瑾,刘甜.离子-有机溶剂复合体系对电子废弃物中贵金属回收研究[J].应用化工,2023,52(1):96-101.

8陈海彬,周振华,张作金,张占峰,杨帅峰.钒钛磁铁矿综合回收研究进展[J].现代矿业,2023,39(1):7-9.

9王云伟,王忠应,陈艳平.贵州某中低品位萤石矿浮选试验研究[J].矿业工程,2023,21(1):17-20.

10刘波,杨启帆,卢舒舒,张茂富,黄美容,潘卫,曾宇,倪志明,府丽琴.辽宁地区某钠长石矿提纯试验研究[J].非金属矿,2022,45(6):54-57. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TD923[矿业工程—选矿]

Citation Information:

The molybdenum content in some molybdenum ore in Fujian is only 0.09%,and most molybdenum exists in molybdenites while a small amount of molybdenum exists in the form of molybdenum oxide ore.The gangue minerals mainly consist of easy-sliming silicate minerals and the flotation activity of the molybdenum ore is low,showing that it is the typical refractory molybdenum ore with high mud content and low grade.A novel surface promoter MCS was introduced to effectively enhance the surface activity of the molybdenum ore,thereby improving the molybdenum flotation recovery.The appropriate grinding fineness,MCS dosage,water glass dosage and collector CM dosage for the flotation were determined through condition experiments.The results show that by using the flotation machine,molybdenum concentrates with a Mo grade of 45.75%and Mo recovery of 82.18%can be obtained after one roughing,three scavenging and seven cleaning,but this process is lengthy and the production and operation costs are high.Through the combined flotation column-flotation machine process,the qualified molybdenum concentrates are gained with a Mo grade of 46.01%and Mo recovery of 87.81%after four cleaning.Therefore,it is re-commended as the principle process for the recovery of molybdenum from the molybdenum ore.

quote

GB/T 7714-2015 [1] SHI Hai-lan, ZHU Wen-long, ZOU Song. Study on High Efficient Flotation Recovery of Some Refractory Molybdenum Ore with High Mud Content and Low Grade[J]. Rare Metals and Cemented Carbides, 2022(6): 11-17.
MLA [1] SHI Hai-lan, et al., "Study on High Efficient Flotation Recovery of Some Refractory Molybdenum Ore with High Mud Content and Low Grade." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 11-17.
APA [1] SHI Hai-lan, ZHU Wen-long, & ZOU Song. (2022). Study on High Efficient Flotation Recovery of Some Refractory Molybdenum Ore with High Mud Content and Low Grade. Rare Metals and Cemented Carbides(6), 11-17.
IEEE [1] SHI Hai-lan, ZHU Wen-long, and ZOU Song, "Study on High Efficient Flotation Recovery of Some Refractory Molybdenum Ore with High Mud Content and Low Grade," Rare Metals and Cemented Carbides, no. 6, pp. 11-17, 2022. keywords: {high mud content;low grade;molybdenum ore;flotation;surface promoter}