Research Progress of Enrichment and Recovery Technology of Scattered Metal Germanium in Coal Fly Ash AITranslate
Abstract AITranslate
Accelerating the extraction of germanium resource from coal fly ash can not only alleviate the contradiction between the shortage of germanium resource and its increasing demand but also broaden the ways of high-value utilization of coal fly ash and improve the added value of products.By reviewing the development status of germanium enrichment and recovery technology from coal fly ash in recent years,the merits and demerits of various methods are analyzed and relevant suggestions are given on the efficient utilization of germanium in coal fly ash.
KeyWords AITranslate
1李样生,李璠,刘光华.国内外从粉煤灰提锗现状[J].江苏化工,2000,28(12):23-24. 被引量:14
2冯林永,雷霆,张家敏,张玉林,刘志斌,杨显万.含锗褐煤综合利用新工艺研究[J].有色金属:冶炼部分,2008(5):35-37. 被引量:13
3普世坤,兰尧中.从粉煤灰中回收锗的湿法工艺研究[J].稀有金属与硬质合金,2012,40(5):15-17. 被引量:10
4普世坤,严云南,兰尧中.氢氧化钠预处理-盐酸蒸馏法回收锗的工艺研究[J].昆明理工大学学报:自然科学版,2012,37(2):19-22. 被引量:4
5王安亭,潘吉平.用仲辛醇萃取锗的研究[J].中国测试技术,2007,33(1):82-83. 被引量:8
6时文中,朱国才.氯化铵氯化—二酰异羟肟酸萃取法从粉煤灰中提取锗的研究[J].河南大学学报:自然科学版,2007,37(2):147-151. 被引量:13
7李样生,刘蓓,李璠,周耐根,刘光华.二酰异羟肟酸萃取法从粉煤灰中提取锗[J].现代化工,2000,20(8):34-36. 被引量:16
8刘丽霞,李文挺,彭军,张磊,安胜利,薛应东,刘伟,李晓明.粉煤灰中锗的赋存状态研究[J].稀有金属与硬质合金,2017,45(5):27-30. 被引量:6
9金明亚,陈少纯,曹洪杨.还原挥发法从低品位含锗煤灰中提取锗[J].有色金属:冶炼部分,2015(3):50-53. 被引量:8
10曹洪杨,陈冬冬,饶帅,高远,陈少纯,张魁芳,朱薇,刘志强.低品位含锗褐煤烟尘二次富集提锗工艺研究[J].有色金属:冶炼部分,2019,0(12):29-32. 被引量:6
1杨莹莹,洪常亮,米亚峰.退役晶硅光伏组件回收技术研究进展[J].中文科技期刊数据库(文摘版)工程技术,2023(2):0042-0044.
2一种“吃塑料”酶的发现,废PET回收或比从石油中提炼更便宜?[J].福建轻纺,2023(2):4-6.
3刘振宇.浅谈溶媒回收技术的应用[J].中文科技期刊数据库(全文版)自然科学,2022(12):0001-0004.
4翁定崧,王正豪,陈良,殷仁涛,肖海兵,刘维燥,梁斌,罗冬梅.蛇纹石与绿矾耦合提取富镁溶液矿化二氧化碳并回收镍[J].无机盐工业,2023,55(1):93-99.
5陈伟.当前基层动物疫病防控工作现状与应对措施[J].今日畜牧兽医:今日宠物,2022(12):52-53.
6米其林、普利司通联合发起倡议 推动回收炭黑发展[J].橡塑智造与节能环保,2022,6(12):40-40.
7张海静,王超,郭颖,刘烨,李杰.山东荣成市无花果产业现状、问题与发展建议[J].农业工程技术,2022,42(32):21-21.
8周彩珍.基于出版产业链视角探索学术期刊融合发展之路[J].编辑学刊,2023(1):73-78. 被引量:2
9林勇,谢思玲,柯菀萍,刘仲华.安化黑茶的降血糖作用及其机理[J].中国茶叶,2023,45(2):1-7.
10雷珺宇,义建军,张蔚,许蔷,王科峰,王莉,张明革,李荣波,高玉李.茂金属聚丙烯催化剂技术开发与应用[J].中国科技成果,2022,23(24):71-71.
Basic Information:
DOI:
Chinese Library Classification Number:TF843[冶金工程—有色金属冶金]
Citation Information:
Accelerating the extraction of germanium resource from coal fly ash can not only alleviate the contradiction between the shortage of germanium resource and its increasing demand but also broaden the ways of high-value utilization of coal fly ash and improve the added value of products.By reviewing the development status of germanium enrichment and recovery technology from coal fly ash in recent years,the merits and demerits of various methods are analyzed and relevant suggestions are given on the efficient utilization of germanium in coal fly ash.
quote
| GB/T 7714-2015 | [1] WANG Li-ping, LI Chao, LI Shi-chun. Research Progress of Enrichment and Recovery Technology of Scattered Metal Germanium in Coal Fly Ash[J]. Rare Metals and Cemented Carbides, 2022(6): 27-32. |
| MLA | [1] WANG Li-ping, et al., "Research Progress of Enrichment and Recovery Technology of Scattered Metal Germanium in Coal Fly Ash." Rare Metals and Cemented Carbides, no. 6, 2022, pp. 27-32. |
| APA | [1] WANG Li-ping, LI Chao, & LI Shi-chun. (2022). Research Progress of Enrichment and Recovery Technology of Scattered Metal Germanium in Coal Fly Ash. Rare Metals and Cemented Carbides(6), 27-32. |
| IEEE | [1] WANG Li-ping, LI Chao, and LI Shi-chun, "Research Progress of Enrichment and Recovery Technology of Scattered Metal Germanium in Coal Fly Ash," Rare Metals and Cemented Carbides, no. 6, pp. 27-32, 2022. keywords: {coal fly ash;germanium;enrichment;recovery} |