daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Bioresorbable Pressure Sensor and Its Applications in Abnormal Respiratory Event Identification Bioresorbable Pressure Sensor and Its Applications in Abnormal Respiratory Event Identification AITranslate

Beijing Institute of Technology;Beijing Institute of Nanoenergy and Nanosystems; Beijing Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bioresorbable electronics that can be absorbed and become a part of the organism after their service life are becoming a trend to avoid secondary invasive surgery. However, the sustainable and secure supply of energy for biosensors is a significant challenge. Here, a bioresorbable pressure sensor (BPS) based on a triboelectric nanogenerator is reported. The BPS based on the triboelectric nanogenerator can directly convert ambient pressure changes into electrical signals. It offers excellent sensitivity (22.61 mV/mmHg), linearity (R2 = 0.99), and good durability (850,000 cycles). The bioresorbable materials of poly(lactic acid)/chitosan/sodium alginate in the BPS show great biocompatibility and can achieve 99.99% sterilization for both Gram-positive bacteria and Gram-negative bacteria. In addition, the device can successfully identify an abnormal respiratory event in small animals and will be completely degraded after 21 days. The BPS only employs medical materials used commonly in FDA-approved implants, which is crucial for the biosafety of bioresorbable devices. Triboelectric devices are expected to be applied in the clinic as bioresorbable electronics.

KeyWords AITranslate

biodegradable electronics pressure sensor triboelectric nanogenerator respiratory identification
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01782

Chinese Library Classification Number:

Citation Information:

Bioresorbable electronics that can be absorbed and become a part of the organism after their service life are becoming a trend to avoid secondary invasive surgery. However, the sustainable and secure supply of energy for biosensors is a significant challenge. Here, a bioresorbable pressure sensor (BPS) based on a triboelectric nanogenerator is reported. The BPS based on the triboelectric nanogenerator can directly convert ambient pressure changes into electrical signals. It offers excellent sensitivity (22.61 mV/mmHg), linearity (R2 = 0.99), and good durability (850,000 cycles). The bioresorbable materials of poly(lactic acid)/chitosan/sodium alginate in the BPS show great biocompatibility and can achieve 99.99% sterilization for both Gram-positive bacteria and Gram-negative bacteria. In addition, the device can successfully identify an abnormal respiratory event in small animals and will be completely degraded after 21 days. The BPS only employs medical materials used commonly in FDA-approved implants, which is crucial for the biosafety of bioresorbable devices. Triboelectric devices are expected to be applied in the clinic as bioresorbable electronics.

quote

GB/T 7714-2015 [1] Zhe Li, Cong Li, Yulin Deng. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01782.
MLA [1] Zhe Li, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01782.
APA [1] Zhe Li, Cong Li, & Yulin Deng. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01782
IEEE [1] Zhe Li, Cong Li, and Yulin Deng, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01782. keywords: {biodegradable electronics pressure sensor triboelectric nanogenerator respiratory identification}