Ion-Selective Separation Using MXene-Based Membranes: A Review AITranslate
Abstract AITranslate
Global lack of clean water makes it essential that new technologies are developed for separation of pollutants from raw water. Membrane separation has arisen as a promising solution among other conventional liquid-separation processes, such as evaporation, distillation, and crystallization. Synthetic polymer membranes have been emphasized as an important component in liquid separation processes due to their outstanding water/salt selectivity and ionic conductivity. However, their inherent trade-off between selectivity and permeability has remained a challenge for polymeric membranes. Recently, two-dimensional nanomaterials have been actively sought after as an alternative to polymeric membranes. MXene, a new type of nanomaterial, has been attracting considerable attention as a building block for nanostructured separation membranes. Due to several appealing features, such as their surface functional groups with negative charge, they have been used in size-, charge-, and adsorption-selective separation for different ions or molecules. This article reviews recent progress in MXene-based membranes, with a particular emphasis on ion-selective separation and their applications for water purification including salt rejection, reverse electrodialysis, or heavy metal adsorption. Lastly, the challenges and future directions of MXene-based ion-selective membranes are discussed.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsmaterialslett.2c00914
Chinese Library Classification Number:
Citation Information:
Global lack of clean water makes it essential that new technologies are developed for separation of pollutants from raw water. Membrane separation has arisen as a promising solution among other conventional liquid-separation processes, such as evaporation, distillation, and crystallization. Synthetic polymer membranes have been emphasized as an important component in liquid separation processes due to their outstanding water/salt selectivity and ionic conductivity. However, their inherent trade-off between selectivity and permeability has remained a challenge for polymeric membranes. Recently, two-dimensional nanomaterials have been actively sought after as an alternative to polymeric membranes. MXene, a new type of nanomaterial, has been attracting considerable attention as a building block for nanostructured separation membranes. Due to several appealing features, such as their surface functional groups with negative charge, they have been used in size-, charge-, and adsorption-selective separation for different ions or molecules. This article reviews recent progress in MXene-based membranes, with a particular emphasis on ion-selective separation and their applications for water purification including salt rejection, reverse electrodialysis, or heavy metal adsorption. Lastly, the challenges and future directions of MXene-based ion-selective membranes are discussed.
quote
| GB/T 7714-2015 | [1] Seunghyun Hong, Faisal Al Marzooqi, Jehad K. ElDemellawi, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00914. |
| MLA | [1] Seunghyun Hong, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00914. |
| APA | [1] Seunghyun Hong, Faisal Al Marzooqi, Jehad K. ElDemellawi, Noora Al Marzooqi, Hassan A. Arafat, & Husam N. Alshareef. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00914 |
| IEEE | [1] Seunghyun Hong, Faisal Al Marzooqi, Jehad K. ElDemellawi, Noora Al Marzooqi, Hassan A. Arafat, and Husam N. Alshareef, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00914. |