Platelet-Inspired Nanotherapeutics for Biomedical Applications AITranslate

Shenyang Pharmaceutical University; Shenyang Pharmaceutical University; Shenyang Pharmaceutical University; Shenyang Pharmaceutical University; Shenyang Pharmaceutical University; Shenyang Pharmaceutical University; Shenyang Pharmaceutical University; Shenyang Pharmaceutical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Platelets, as abundant corpuscles in the blood, are extensively involved in normal physiological processes and disease occurrence. Recently, remarkable progress in platelet-based nanotherapeutics has been made, especially with the burgeoning fields of biotechnology and nanomedicine. Herein, we aim to provide an overview on platelet-inspired nanotherapeutics for biomedical applications. First, the recent trends of biomimetic platelet-inspired nanotherapeutics are outlined, mainly including platelet membrane-camouflaged nanosystems, platelets loading with nanoparticles and platelet-mimicking nanocarriers. Then, the emerging nanotherapeutics for functional modulation of platelet aggregation, activation, and inhibition are discussed. Subsequently, platelet derivative-based nanotherapeutics are presented, including platelet extracellular vesicles and platelet polyphosphates. Finally, the clinical application prospects of these emerging nanotherapeutics are highlighted, with particular emphasis on their rationale, advantages, and challenges.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1021/acsmaterialslett.2c00832

Chinese Library Classification Number:

Citation Information:

Platelets, as abundant corpuscles in the blood, are extensively involved in normal physiological processes and disease occurrence. Recently, remarkable progress in platelet-based nanotherapeutics has been made, especially with the burgeoning fields of biotechnology and nanomedicine. Herein, we aim to provide an overview on platelet-inspired nanotherapeutics for biomedical applications. First, the recent trends of biomimetic platelet-inspired nanotherapeutics are outlined, mainly including platelet membrane-camouflaged nanosystems, platelets loading with nanoparticles and platelet-mimicking nanocarriers. Then, the emerging nanotherapeutics for functional modulation of platelet aggregation, activation, and inhibition are discussed. Subsequently, platelet derivative-based nanotherapeutics are presented, including platelet extracellular vesicles and platelet polyphosphates. Finally, the clinical application prospects of these emerging nanotherapeutics are highlighted, with particular emphasis on their rationale, advantages, and challenges.

quote

GB/T 7714-2015 [1] Fujun Yang, Zhiqiang Kong, Qingyu Ji, et al. ACS Materials Letters, 2023(5). DOI:10.1021/acsmaterialslett.2c00832.
MLA [1] Fujun Yang, et al., ACS Materials Letters, no. 5, 2023, https://doi.org/10.1021/acsmaterialslett.2c00832.
APA [1] Fujun Yang, Zhiqiang Kong, Qingyu Ji, Shumeng Li, Jin Sun, Zhonggui He, Shenwu Zhang, & Cong Luo. (2023). ACS Materials Letters(5). https://doi.org/10.1021/acsmaterialslett.2c00832
IEEE [1] Fujun Yang, Zhiqiang Kong, Qingyu Ji, Shumeng Li, Jin Sun, Zhonggui He, Shenwu Zhang, and Cong Luo, ACS Materials Letters, no. 5, 2023, doi: 10.1021/acsmaterialslett.2c00832.