Nano WC Preparation Technologies and their Latest Development AITranslate
Abstract AITranslate
The latest development of WC preparation technologies both at home and abroad is reviewed including solid phase method,fluid phase method,gas phase method and so on.Their advantages,shortcomings and possible ways to overcome are analyzed.The development trend of preparation research of nano is advised in china.
KeyWords AITranslate
1Kear B H, Mc Candlish L E. Chemical processing and properties of nanostructured WC- Co Materials [J].Nanostruct Mater, 1993,3 (1-6):19-30.
2Kim B K,Ha G H,Lee C; G,etal. Structure and proper- ties of nanophase WC/Co/VC/TaC hard metal E J]. Nanostruct Mater, 1997,9 (1-8) :233-236.
3Goren Muginstein G R, Berger S, Rosen A. Sintering study of nanoerystal[ine tungsten carbide powders[J].Nanostruct. Maler, 1998,10(5) :795-804.
4I.eclercq L, Provost M, Pastor H, et al. Catalytic proper- ties of transition metal carbides[J].Jan Catal, 1989,117 (2) :371-383.
5C-arg D, Dyer P N. Tungsten carbide erosion resistant coating for aerospace components [ A]. Chemical vapor deposition of refractory metals and ceramics: Proceed- ings of the symposium [C]. Boston: Materials Research Society, 1989.213-220.
6柳林 李兵 丁星兆 等.硬质合金的制备.科学通报,1994,13(3):32-36.
7Qiang Wang,Fang yu Cao. Synthesis of hexagonal tungsten carbide in tungsten-sodium and supereritical carbon dioxide system[J]. Mater Chem Phys, 2006,95 ( 1 ):113- 116.
8Nersisyan H H,Won H I,Won C W,et al. Study of the combustion synthesis process of nanostructured WC and WC-Co[J]. Mater Chem Phys,2005,94(1) : 153-158.
9吴成义,张丽英.一种纳米级钨粉及碳化钨粉的制备方法[P].中国专利1608983 2005-04-27.
10qLee Jong Dae, Lee Dong Hwal, Park No Kuk,et al. The preparation of nanophase tungsten carbide with zeoliteX catalysts[J]. Appl Phys,2006,6(6):1 040-1 043.
1梅文强,刘志国,郭名亮,朱启伟,郭华彬.特粗WC颗粒的制备方法研究[J].金属功能材料,2012,19(4):25-29. 被引量:1
2邱建美,张玲洁,申乾宏,杨辉,陈乐生,樊先平.碳化钨粉体在水介质中的分散研究[J].稀有金属,2014,38(6):1086-1092. 被引量:2
3李广生.准纳米WC粉的试制[J].硬质合金,2015,32(3):175-181.
4向承翔.机床用WC/Al_2O_3复相陶瓷刀具材料的研究[J].铸造技术,2016,37(4):649-652. 被引量:1
1黄丽容,陈宇航,王晓雷.微孔结构对低钴粗晶WC硬质合金摩擦性能的影响[J].金属功能材料,2016,23(3):37-41. 被引量:6
2胡涛,胡忠举,郭世柏,郭涛.无粘结相WC基硬质合金刀具材料的研究现状与前景[J].工具技术,2019,53(2):7-11. 被引量:8
3陈文孝,于秀清,冯如信.化学置换沉积银制备AgWC(40)触头材料的方法[J].电工材料,2020(3):9-11.
4张曼,陶君,李颖,汪应龙,朱玉峰,张宇晗,伽亮亮,丁瑜.聚乙烯吡咯烷酮含量对纳米碳化钨粉末在无水乙醇中分散性的影响[J].黄冈师范学院学报,2020,40(3):46-49.
1段波,赵兴中,李星国,张同俊,肖建中,胡镇华,崔昆.超微粉制备技术的现状与展望[J].材料工程,1994,22(6):5-8. 被引量:26
2段波,赵兴中,李星国,张同俊.超微粉制备技术的现状与展望[J].材料导报,1995,9(3):31-34. 被引量:13
3李晓娥,祖庸.纳米TiO_2的制备[J].现代化工,1999,19(11):42-44. 被引量:24
4伍贺东,陈为亮,孟德龙,张凌义,戴永年.超细镍粉制备技术研究进展[J].湿法冶金,2007,26(2):57-61. 被引量:4
5祖庸,李晓娥.气相法制备纳米二氧化钛[J].钛工业进展,1996(4):2-5. 被引量:5
6唐阳清,周馨我.超细高纯氧化铝的制备[J].材料导报,1995,9(6):39-43. 被引量:7
7崔祝屏,钟法宝.铜屑气相法去除粗TiCl_4中钒杂质的研究[J].广东有色金属学报,1992,2(1):23-29.
8高海燕,曹顺华.机械合金化制备纳米晶硬质合金粉的进展[J].粉末冶金技术,2003,21(6):355-358. 被引量:6
9罗骥,方哲成,郭志猛,邵慧萍.含V和Cr纳米W粉碳化热力学分析及实验[J].材料热处理学报,2011,32(2):26-29.
10蒋志坚.八钢原料解决的途径[J].新疆钢铁,2005(1):4-5.
Basic Information:
DOI:
Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]
Citation Information:
The latest development of WC preparation technologies both at home and abroad is reviewed including solid phase method,fluid phase method,gas phase method and so on.Their advantages,shortcomings and possible ways to overcome are analyzed.The development trend of preparation research of nano is advised in china.
quote
| GB/T 7714-2015 | [1] FU Xiao-ming. Nano WC Preparation Technologies and their Latest Development[J]. Rare Metals and Cemented Carbides, 2011(1): 57-60. |
| MLA | [1] FU Xiao-ming. "Nano WC Preparation Technologies and their Latest Development." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 57-60. |
| APA | [1] FU Xiao-ming. (2011). Nano WC Preparation Technologies and their Latest Development. Rare Metals and Cemented Carbides(1), 57-60. |
| IEEE | [1] FU Xiao-ming, "Nano WC Preparation Technologies and their Latest Development," Rare Metals and Cemented Carbides, no. 1, pp. 57-60, 2011. keywords: {nano tungsten carbide;preparation technology;solid phase method;fluid phase method;gas phase method;the latest development} |