Experimental Research on the Composite Material of Nano-Al_2O_3/Cemented Carbide AITranslate

Key Laboratory of Natural Gas Equipment of the Ministry of Education, Southwest Petroleum University;Key Laboratory of Natural Gas Equipment of the Ministry of Education, Southwest Petroleum University;Key Laboratory of Natural Gas Equipment of the Ministry of Education, Southwest Petroleum University;Key Laboratory of Natural Gas Equipment of the Ministry of Education, Southwest Petroleum University;Key Laboratory of Natural Gas Equipment of the Ministry of Education, Southwest Petroleum University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Adding nano-Al2O3 into WC-Co substrate may be useful to enhance the performance of cemented carbides.Based on the above view,the mechanical properties,wear and shock resistance,and microstructure of the composite material of nano-Al2O3/cemented carbide with different formula were investigated.The results show that adding proper nano-Al2O3 not only refines alloy grains,and improves microstructure uniformity and wear resistance of the composite material,but also enhances the strength of WC grain boundary,which plays a role of strengthening and toughening and results in fracture form shift from intergranular fracture to transgranular fracture of the composite material.Meanwhile,adding rare earth also improves the comprehensive performance of the composite material.Drill teeth made with the nano-composite materials are assembled into a drill bit that is then tested in situ.Compared with the drill bit assembled with cemented carbide drill teeth,the above drill bit is of 20% higher rock breaking efficiency and 80% longer service life.

KeyWords AITranslate

WC nano-Al2O3 wear resistance strengthening and toughening microstructure

1王鹏飞,李红卫,于敦波,李世鹏,杨红川,徐静,应启明.铸锭方式和热处理对Nd_(12.6)Fe_(81)B_6Ga_(0.4)合金微观组织的影响[J].稀有金属,2007,31(5):610-614. 被引量:4

2王占勇,温艳玲,谷南驹,刘金芳,岑伟,刘文杰.烧结NdFeB的铸锭组织分析[J].磁性材料及器件,2002,33(1):7-9. 被引量:5

3闫俊萍,任惠平,王玉峰.NdFeB合金铸锭组织及均匀化退火[J].稀土,2004,25(1):70-72. 被引量:4

4周仲成,刘国征,刘树峰,吕卫东,武斌,赵瑞金,鲁富强.Nd-Fe-B系铸锭显微结构的研究[J].稀土,2005,26(2):26-28. 被引量:5

5杨刚,刘颖,高升吉,杨眉,涂铭旌.铸锭方式对NdFeB合金铸锭显微结构的影响[J].金属功能材料,2004,11(2):5-7. 被引量:3

6曾振鹏.烧结NdFeB永磁材料的断裂研究[J].稀有金属材料与工程,1996,25(3):18-21. 被引量:25

1黄奔,伏坤,周建华,李晓峰.添加Al_2O_3对粗晶WC-10%Co硬质合金力学性能和显微结构的影响[J].硬质合金,2015,32(5):311-316. 被引量:1

2黄志强,袁媛,谢豆,于德良.含纳米Co的新型PDC复合片性能试验研究[J].材料导报:纳米与新材料专辑,2016,30(1):76-81. 被引量:3

1衡军,骈小璇,史春燕,秦伟丽,栗正新,栗晓龙.不同黏结剂聚晶金刚石晶粒界面研究进展[J].金刚石与磨料磨具工程,2017,37(5):74-78. 被引量:5

2石亮,陈坤,常雪婷,王东胜,尹衍升.球形碳化钨增强钴基堆焊涂层的组织及低温耐磨性[J].表面技术,2022,51(2):165-175. 被引量:1

3聂孟杰,裴夤崟,黄成志,赵东鹏,李文彬.PDC性能优化及其钎焊技术研究现状[J].电焊机,2023,53(4):63-72.

4陈卫民,李磊,刘杰,邢波,杨馨蕊,罗丽萍,孙福华.钴的脱除工艺对聚晶金刚石复合片性能的影响[J].硬质合金,2023,40(4):271-278.

1袁慎铁,赖朝彬,陈英俊,熊文名.含铌、钒、钛EQ47海洋平台用钢的高温塑性研究[J].有色金属科学与工程,2014,5(2):52-56. 被引量:8

2徐湘涛.加工钢—硬质合金复合材料用金刚石磨具的试验研究[J].硬质合金,1997,14(3):164-166.

3张建德,曾舟山,谢飞.热变形致密细晶粒钼棒的组织和性能[J].粉末冶金材料科学与工程,2008,13(4):235-239. 被引量:12

4万林生,曾学品,赖星任,杨亮,刘鹏.仲钨酸铵结晶掺Cr制备的WC粉和超细硬质合金的性能研究[J].稀有金属与硬质合金,2016,44(6):54-59. 被引量:6

5李晓红,胡淑文,解子章,杨让.液相烧结Mo-Cu合金的研究[J].新技术新工艺,1996(1):35-36. 被引量:5

6王慧芳,方少垣.高温钼粉的性能对其成形及烧结的影响[J].粉末冶金技术,1994,12(2):103-108. 被引量:2

7张雪峰,李林风,麻永林,苍大强.电磁搅拌处理Al-Si合金晶粒组织细化的机理分析[J].材料导报:网络版,2007,2(5):26-27.

8张立.WC添加方式对Cr_3C_2基硬质合金性能的影响[J].硬质合金,1998,15(2):102-104. 被引量:2

9姚萍屏,张忠义,汪琳,熊翔,何俊,李红梅.烧结温度对铁基粉末冶金航空刹车材料摩擦磨损性能的影响[J].润滑与密封,2007,32(6):1-5. 被引量:7

10王正云,栾道成,雒晗,王志军.高能球磨时间对钨铜复合材料性能的影响[J].西华大学学报:自然科学版,2007,26(3):15-18. 被引量:7

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

Adding nano-Al2O3 into WC-Co substrate may be useful to enhance the performance of cemented carbides.Based on the above view,the mechanical properties,wear and shock resistance,and microstructure of the composite material of nano-Al2O3/cemented carbide with different formula were investigated.The results show that adding proper nano-Al2O3 not only refines alloy grains,and improves microstructure uniformity and wear resistance of the composite material,but also enhances the strength of WC grain boundary,which plays a role of strengthening and toughening and results in fracture form shift from intergranular fracture to transgranular fracture of the composite material.Meanwhile,adding rare earth also improves the comprehensive performance of the composite material.Drill teeth made with the nano-composite materials are assembled into a drill bit that is then tested in situ.Compared with the drill bit assembled with cemented carbide drill teeth,the above drill bit is of 20% higher rock breaking efficiency and 80% longer service life.

quote

GB/T 7714-2015 [1] HUANG Zhi-qiang, LI Wei, LI Qin, et al. Experimental Research on the Composite Material of Nano-Al_2O_3/Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2011(1): 61-65.
MLA [1] HUANG Zhi-qiang, et al., "Experimental Research on the Composite Material of Nano-Al_2O_3/Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 61-65.
APA [1] HUANG Zhi-qiang, LI Wei, LI Qin, GUO En-hong, & QIU Cheng-song. (2011). Experimental Research on the Composite Material of Nano-Al_2O_3/Cemented Carbide. Rare Metals and Cemented Carbides(1), 61-65.
IEEE [1] HUANG Zhi-qiang, LI Wei, LI Qin, GUO En-hong, and QIU Cheng-song, "Experimental Research on the Composite Material of Nano-Al_2O_3/Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 61-65, 2011. keywords: {WC;nano-Al2O3;wear resistance;strengthening and toughening;microstructure}