daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

The Latest Development and Prospect of Cemented Carbide Industry in China AITranslate

Manufacturing Teaching and Research Office, Department of Mechanical Engineering, North China Electric Power University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The manufacturing technologies,product characteristics,application and types of cemented carbides are briefly introduced.The development history of cemented carbide industry in China is reviewed,and its existing problems and shortages are analyzed.The development trend of new cemented carbide material is pointed out,and some advices about the future development of cemented carbide industry in China are presented.

KeyWords AITranslate

cemented carbide cutting tool material the latest development prospect

1周永贵,邹仿棱.中国硬质合金工业的历史、现状与发展[J].中国钨业,2004,19(5):62-68. 被引量:10

2Henk van den Berg. Hardmetals: trends in development and application[J].Powder Metallurgy, 2007,50 ( 1 ) : 7-10.

3北京双赢纵横信息咨询中心.2010-2015年中国硬质合金行业市场运行态势与投资前景预测分析报告[EB/OL].http://detail.china.alibaba.corn/buyer/offerde—tail/812371871.html.2010-12-10.

4沈壮行.中国工具工业的历史和现状[J].世界制造技术与装备市场,2006(4):27-28. 被引量:2

5Alistair Greason, Martin James, Mathias Tillman,et al. The future of finer grain hard metals[A]. Proc 16th Int Plansee Seminar[C]. Reutte.. Plansee AG, 2005. 314-338.

6谢宏,肖逸锋,贺跃辉,丰平.硬质合金涂层刀具研究的新进展[J].中国钨业,2006,21(2):33-36. 被引量:16

7张文毓.硬质合金涂层刀具研究进展[J].稀有金属与硬质合金,2008,36(1):59-63. 被引量:41

8张荆门.硬质合金工业的进展(1)[J].粉末冶金技术,2002,20(3):140-146. 被引量:24

9周建华,卢伟民.国内外硬质合金生产现状及近期发展动向分析[J].稀有金属与硬质合金,2006,34(1):36-41. 被引量:25

10叶永权,成晓玲,匡同春,白晓军,雷淑梅,向雄志,袁高群.梯度结构硬质合金的最新研究进展[J].稀有金属,2005,29(3):357-362. 被引量:5

1李亚军,栾道成,王正云,左洪松,秦琴,赵太源.烧结工艺对超细WC-6%Co-0.6%(VC/Cr_3C_2/TaC)硬质合金性能的影响[J].硬质合金,2012,29(1):24-28. 被引量:5

2章士麒,袁红梅,伍文辉,唐玲,赵玉玲.中国硬质合金发展与专业技术人才需求[J].硬质合金,2012,29(5):329-335. 被引量:5

3李友生.钨资源在硬质合金刀具行业中的可持续发展[J].制造技术与机床,2012(12):107-110. 被引量:1

4王洪涛,陈枭,白小波,纪岗昌,董增祥,仪登亮,杨凤根.冷喷多尺度WC-Co金属陶瓷涂层结构与性能研究[J].兵工学报,2013,34(7):876-882. 被引量:5

5钟志强,郑海华,欧阳水林,陈瀚.论七面体球磨介质的球磨效率及对合金组织性能的影响[J].有色金属科学与工程,2014,5(3):60-64. 被引量:1

6王瑶,宋晓艳,刘雪梅,魏崇斌,王海滨,王西龙,付军.氧化‐还原碳化法回收再生高性能硬质合金的研究[J].稀有金属材料与工程,2014,43(12):3172-3176. 被引量:8

7张卫兵,刘向中,陈振华,陈鼎,彭程.WC-Co硬质合金最新进展[J].稀有金属,2015,39(2):178-186. 被引量:63

8肖玄.TiMoC添加剂制备TiC金属陶瓷复合材料的研究[J].佛山陶瓷,2015,25(8):9-12. 被引量:1

9张昌娟,焦锋,赵波,牛赢.硬质合金激光加热辅助切削刀具磨损预测[J].机械科学与技术,2016,35(12):1877-1881. 被引量:1

10李志华,肖平安,李晨坤,刘洋,宋建勇,陈超.粗晶TM52钢结硬质合金的冲击磨料磨损性能研究[J].材料导报,2017,31(12):39-44. 被引量:3

1王悦,赵治,陈健,王海滨,韩铁龙,单宇鹏,刘雪梅,宋晓艳.有机粘结剂状态对硬质合金增材制造的影响[J].中国体视学与图像分析,2022,27(2):146-155.

2高德强,刘雪梅,冯浩,孙婷,刘超,宋晓艳.超粗晶WC-8Co硬质合金循环压缩过程中组织演变的研究[J].中国体视学与图像分析,2020(2):135-143. 被引量:2

3叶志坚,李晗,郑洲顺,杜勇.基于牛顿迭代法的WC晶体界面能函数规则化算法[J].中国体视学与图像分析,2020(2):128-134.

4赵太源,栾道成,王正云,熊万全.含(W,Ti,Ta)C的超细硬质合金的性能及组织研究[J].硬质合金,2012,29(5):289-296. 被引量:9

5吕小军,陈明,杨青青,熊惟皓.真空/压力烧结淬火一体化装置的研究[J].硬质合金,2013,30(3):167-172. 被引量:2

6李力,张崇才,陈慧,王权.烧结温度对WC-16TiC-4TaC-9Co硬质合金微观组织与性能的影响[J].重庆文理学院学报:社会科学版,2013,32(5):4-7.

7曹万里,于惠琴.中国硬质合金企业专利发展的现状与思考[J].稀有金属与硬质合金,2013,41(5):62-65. 被引量:1

8苏革新,周亮,王利捷,郑富康.冷喷涂沉积纳米结构涂层研究进展[J].热加工工艺,2018,47(22):7-11. 被引量:2

9刘雪梅,范金莲,冯浩,宋晓艳.WC-Co硬质合金的高温氧化过程研究[J].中国体视学与图像分析,2018,23(4):343-350. 被引量:1

10谢晨辉,谭立群,彭宇,周华堂.硬质合金的非常规检测技术[J].硬质合金,2018,35(6):390-402. 被引量:2

1周永贵,邹仿棱.中国硬质合金工业的历史、现状与发展[J].中国钨业,2004,19(5):62-68. 被引量:10

2林伯颖.硬质合金市场情况分析与对策思考[J].中国钨业,2004,19(5):36-39. 被引量:4

3梁辉.钢水罐倾翻装置电机及轴的选取[J].重工与起重技术,2015,0(2):6-7.

4赵晶.国内钢铁粉末的生产与发展[J].科技信息,2011(20). 被引量:1

5我国硬质合金工业喜忧参半[J].模具工程,2005(3):36-36.

6崔泽甫,萧玉麟.硬质合金工业中的防护与保健[J].硬质合金,1990(3):53-57.

7孙慎宏,陈立胜.50万吨连轧棒材生产线工艺流程及主要特点简介[J].特钢技术,2006,11(3):66-67. 被引量:1

8管建红.宝钢钢渣处理技术的发展及其产品特点[J].冶金丛刊,2005(1):31-33. 被引量:15

9刘世民.钢铁粉末的生产与发展[J].莱钢科技,2005(6):52-55. 被引量:3

10张荆门.硬质合金工业的进展(1)[J].粉末冶金技术,2002,20(3):140-146. 被引量:24

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

The manufacturing technologies,product characteristics,application and types of cemented carbides are briefly introduced.The development history of cemented carbide industry in China is reviewed,and its existing problems and shortages are analyzed.The development trend of new cemented carbide material is pointed out,and some advices about the future development of cemented carbide industry in China are presented.

quote

GB/T 7714-2015 [1] CHU Kai-yu. The Latest Development and Prospect of Cemented Carbide Industry in China[J]. Rare Metals and Cemented Carbides, 2011(1): 52-56.
MLA [1] CHU Kai-yu. "The Latest Development and Prospect of Cemented Carbide Industry in China." Rare Metals and Cemented Carbides, no. 1, 2011, pp. 52-56.
APA [1] CHU Kai-yu. (2011). The Latest Development and Prospect of Cemented Carbide Industry in China. Rare Metals and Cemented Carbides(1), 52-56.
IEEE [1] CHU Kai-yu, "The Latest Development and Prospect of Cemented Carbide Industry in China," Rare Metals and Cemented Carbides, no. 1, pp. 52-56, 2011. keywords: {cemented carbide;cutting tool material;the latest development;prospect}