ZnGa2S4:an infrared nonlinear optical material with large second-harmonic generation response and wide band gap AITranslate
Abstract AITranslate
High-performance nonlinear optical(NLO)crystals are crucial devices to convert wavelength of solid-state lasers.Chalcogenides play an indispensable role in the research of infrared NLO materials.In this work,ternary chalcogenide ZnGa2S4 with defect diamond-like structure was screened out and synthesized by chemical vapor transport method.
KeyWords AITranslate
1Qiao-Lu Lin,Zheng-Fang Qian,Xiang-Yu Dai,Yi-Ling Sun,Ren-Heng Wang.Regulation of electronic structure of monolayer MoS_(2) by pressure[J].Rare Metals,2022,41(5):1761-1770. 被引量:3
2Tatsuya Nakazawa,Donghyun Kim,Jaehyeok Kim,Yohei Kotsugi,Taehoon Cheon,Seung-Min Chung,Soo-Hyun Kim,Hyungjun Kim.Development of RuS_(2) for near-infrared photodetector by atomic layer deposition and post-sulfurization[J].Rare Metals,2022,41(9):3086-3099. 被引量:3
3Youchao Liu,Youquan Liu,Zheshuai Lin,Yanqiang Li,Qingran Ding,Xin Chen,Lina Li,Sangen Zhao,Maochun Hong,Junhua Luo.Nonpolar Na_(10)Cd(NO_(3))_(4)(SO_(3)S)_(4) Exhibits a Large Second-Harmonic Generation[J].CCS Chemistry,2022,4(2):526-531. 被引量:2
4Yanqiang Li,Congling Yin,Xiaoyan Yang,Xiaojun Kuang,Jie Chen,Lunhua He,Qingran Ding,Sangen Zhao,Maochun Hong,Junhua Luo.A Nonlinear Optical Switchable Sulfate of Ultrawide Bandgap[J].CCS Chemistry,2021,3(7):2298-2306. 被引量:3
1Wenjing Tan,Chenyang Zhang,Tingting Huang,Bingbing Zhang.Recent progress of newly developed functional building units and corresponding nonlinear optical materials[J].Chinese Journal of Structural Chemistry,2023,42(9):71-82.
2Xuanyi Liu,Hongyan Fu.Highly-coherent second-harmonic generation in a chip-scale source[J].Light(Science & Applications),2024,13(1):6-7.
3Qian Lin,Jingui Ma,Zhe Yin,Peng Yuan,Jing Wang,Guoqiang Xie,Liejia Qian.Optical modification of nonlinear crystals for quasi-parametric chirped-pulse amplification[J].Fundamental Research,2024,4(1):43-50.
4Yang Yang,Qing-Rong Liang,Chun-Li Zhu,Guo-Zhong Zheng,Jian Zhang,Shou-Jun Zheng,Yung-Chang Lin,De-Zhi Zheng,Jia-Dong Zhou.Chemical vapor deposition synthesis of V-doped MoS_(2)[J].Rare Metals,2023,42(12):3985-3992.
5Sajid Khan,Dil Faraz Khan,R.Neffati,Tariq Usman,Muhammad Waqar Ahsraf,Shamim Khan,Saeed Ullah Jan,G.Murtaza.Electronic and thermoelectric properties of YbMg_(2)X_(2)(X=P,As,Sb,Bi)zintl compounds by first-principles method[J].Journal of Rare Earths,2024,42(1):147-154. 被引量:1
6施培松,窦红真,朱满意.基于非线性光学特性的还原氧化石墨烯复合材料的制备研究进展[J].许昌学院学报,2024,43(2):62-65.
7Ang Li,Yanhong Wang,Haotian Tian,Alimujiang Yalikun,Yves Journaux,Min Luo,Hongcheng Lu.Multifunctional properties of a polar spin chain compound[N(C_(3)H_(7))_(4)][Cu(C_(8)H_(4)NO_(4))]·H_(2)O exhibiting both one-dimensional magnetism and nonlinear optical activity[J].Chinese Chemical Letters,2024,35(2):622-625.
8Ming Li,Xiao-Xiao Xue,Yan-Lei Zhang,Xin-Biao Xu,Chun-Hua Dong,Guang-Can Guo,Chang-Ling Zou.Breaking the efficiency limitations of dissipative Kerr solitons using nonlinear couplers[J].Science China(Physics,Mechanics & Astronomy),2024,67(3):88-94.
9刘晓东,卢其亮,罗其全.Structure,electronic,and nonlinear optical properties of superalkaline M_(3)O(M=Li,Na)doped cyclo[18]carbon[J].Chinese Physics B,2024,33(2):311-317.
10XINYAO YU,FANGHAO LI,TINGTING LANG,JIANYUAN QIN,XIAO MA.Ultrasensitive tunable terahertz lithium niobate metasurface sensing based on bound states in the continuum[J].Photonics Research,2023,11(12):2168-2178.
Basic Information:
DOI:
Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]
Citation Information:
High-performance nonlinear optical(NLO)crystals are crucial devices to convert wavelength of solid-state lasers.Chalcogenides play an indispensable role in the research of infrared NLO materials.In this work,ternary chalcogenide ZnGa2S4 with defect diamond-like structure was screened out and synthesized by chemical vapor transport method.
quote
| GB/T 7714-2015 | [1] Chen-Yang Zhang, Xiao-Nan Niu, Yan-Feng Wei, et al. Rare Metals, 2024(1): 395-401. |
| MLA | [1] Chen-Yang Zhang, et al., Rare Metals, no. 1, 2024, pp. 395-401. |
| APA | [1] Chen-Yang Zhang, Xiao-Nan Niu, Yan-Feng Wei, Shu-Xing Zhou, Da-Qing Yang, Ying Wang, Jian Wang, & Bing-Bing Zhang. (2024). Rare Metals(1), 395-401. |
| IEEE | [1] Chen-Yang Zhang, Xiao-Nan Niu, Yan-Feng Wei, Shu-Xing Zhou, Da-Qing Yang, Ying Wang, Jian Wang, and Bing-Bing Zhang, Rare Metals, no. 1, pp. 395-401, 2024. |