Low-temperature Nonpressurized Sintering and Performance of High-purity Er_2O_3 Target Material AITranslate
Abstract AITranslate
High-purity Er2O3 ceramic target material of about 90% relative density was prepared by lowtemperature nonpressurized sintering at 1 450℃ and with Er2O3 nanopowders as its raw material. The target materials prepared with Er2O3 nanopowders of various shape were analyzed from their fracture appearance and density. The results show that the target material prepared by low-temperature nonpressurized sintering and with three-dimensionally subsphaeroidal Er2O3 nanopowders as its raw material has the optimal performance.
KeyWords AITranslate
1张丽艳,胡丽丽,姜中宏.高能、超短脉冲、可调谐激光器用掺镱氟磷酸盐玻璃研究进展(英文)[J].物理学进展,2003,23(4):473-483. 被引量:3
2金贵铸,郑云万,袁茂林,等.稀土火法冶炼工艺学[M].北京:中国有色金属工业总公司职工教育教材编审办公室,1986.
3施利毅,付红霞,张登松,方建慧.一维纳米稀土氧化物的研究进展[J].功能材料,2006,37(10):1535-1538. 被引量:6
4林海,康维刚,黄曼,丁浩,许霞.绢云母质二维纳米薄片材料机械力化学改性及应用研究[J].北京科技大学学报,2004,26(6):627-630. 被引量:5
1杜帅,李发,高陇桥,陈丽梅,张雪梅,刘征,李龙土,桂治轮.添加剂和烧结工艺对A1N瓷性能的影响[J].功能材料,1995,26(6):557-560. 被引量:2
2常青,茹红强,喻亮,岳新艳.羟基磷灰石粉体的低温无压烧结行为[J].人工晶体学报,2009,38(S1):366-370. 被引量:2
3吴音,周和平,缪卫国,韩巍,薛鸿陆.冲击波处理的AlN粉体的低温烧结特性[J].无机材料学报,1998,13(2):229-233. 被引量:4
4何捍卫,胡岳华,黄可龙,张莉.影响均相沉淀法制备高纯纳米氧化铒的因素及机理研究[J].稀土,2000,21(3):4-8. 被引量:4
5付静,吴文远,涂赣峰,王兆文,杨红晓.熔盐电解法制取铝铒合金的研究[J].稀有金属,2003,27(6):718-720. 被引量:5
6Yuki Tahara,Kazufumi Yasunaga,Toshiyuki Matsui,Fuminobu Hori,Akihiro Iwase.Study on analysis of crystal structure in CeO_2 doped with Er_2O_3 or Gd_2O_3[J].稀土学报:英文版,2010(S1):164-167. 被引量:1
7李晓杰,张越举.爆炸压实烧结ITO陶瓷靶材的实验研究[J].稀有金属材料与工程,2005,34(3):417-420. 被引量:7
8吴宇.加温加压离子交换法制取激光晶体级Ho_2O_3、Er_2O_3、Tm_2O_3、Yb_2O_3、Lu_2O_3工艺要点[J].江西有色金属,2008,22(2):26-28. 被引量:2
9刘建华,孙杰,李松梅.席夫碱盐燃烧法制备纳米Er2O3晶体[J].中国稀土学报,2003,21(6):667-667.
10田君,尹敬群.用草酸沉淀法从2-乙基己基膦酸单2-乙基己基酯负载有机相中反萃取铒[J].湿法冶金,1997,16(3):26-28. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF125.42[冶金工程—粉末冶金]
Citation Information:
High-purity Er2O3 ceramic target material of about 90% relative density was prepared by lowtemperature nonpressurized sintering at 1 450℃ and with Er2O3 nanopowders as its raw material. The target materials prepared with Er2O3 nanopowders of various shape were analyzed from their fracture appearance and density. The results show that the target material prepared by low-temperature nonpressurized sintering and with three-dimensionally subsphaeroidal Er2O3 nanopowders as its raw material has the optimal performance.
quote
| GB/T 7714-2015 | [1] DENG Yan-lai, DENG Zhi-jun. Low-temperature Nonpressurized Sintering and Performance of High-purity Er_2O_3 Target Material[J]. Rare Metals and Cemented Carbides, 2009(4): 15-17. |
| MLA | [1] DENG Yan-lai, and DENG Zhi-jun. "Low-temperature Nonpressurized Sintering and Performance of High-purity Er_2O_3 Target Material." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 15-17. |
| APA | [1] DENG Yan-lai, & DENG Zhi-jun. (2009). Low-temperature Nonpressurized Sintering and Performance of High-purity Er_2O_3 Target Material. Rare Metals and Cemented Carbides(4), 15-17. |
| IEEE | [1] DENG Yan-lai and DENG Zhi-jun, "Low-temperature Nonpressurized Sintering and Performance of High-purity Er_2O_3 Target Material," Rare Metals and Cemented Carbides, no. 4, pp. 15-17, 2009. keywords: {Er2O3 nanopowder;high-purity Er2O3 ceramic target material;low-temperature nonpressurizedsintering;density;fracture appearance} |