daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Preparation of In-situ Reinforced Porous Nickel-based Composites by Laser Sintering AITranslate

School of Materials Science and Engineering, Nanjing University of Aeronautics and Astronautics;School of Materials Science and Engineering, Nanjing University of Aeronautics and Astronautics;School of Materials Science and Engineering, Nanjing University of Aeronautics and Astronautics
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The laser sint alloy and TiH2. The mi formation mechanisms cussed. In the sintered ering experiment was carried out on the powder mixture of self-melting nickel-based crostructure of sintered samples was characterized by XRD,SEM and EDX. And the of porous structure and precipitated phase in sintered samples were simply dis samples, the reinforcing phases TiC and TiBz are in-situ synthesized and structure is also formed. A large number of micron-sized pores are uniformly dispersed in the matrix as the high-temperature strengthening phase CrB with a radial or acicular-lobate shape. porous as well

KeyWords AITranslate

laser sintering in-situ reinforcement porous structure nickel-based alloy TiH2 composite

1潘琰峰,沈以赴,顾冬冬,胥橙庭.选择性激光烧结技术的发展现状[J].工具技术,2004,38(6):3-7. 被引量:66

2沈以赴,吴鹏,顾冬冬,李玉芳.激光烧结制备藕状316不锈钢多孔材料的微孔结构特征[J].航空学报,2007,28(5):1236-1241. 被引量:12

3蔡利芳,张永忠,席明哲,石力开.原位合成法在材料制备中的应用及进展[J].金属热处理,2005,30(10):1-6. 被引量:32

1吴昆,崔春娟,邹德宁,谢宸洋.Ni基复合材料的研究进展[J].热加工工艺,2013,42(18):7-9. 被引量:1

2张敏,刘畅,任博,严凯,陈长军,王晓南.3D打印激光制备多孔镍合金组织和力学性能研究[J].中国光学,2016,9(3):335-341. 被引量:11

3罗洪峰,张先满.多孔金属激光增材制造研究进展[J].铸造技术,2018,39(1):236-239. 被引量:2

4杨建明,汤阳,顾海,刘永加,黄大志,陈劲松.3D打印制备多孔结构的研究与应用现状[J].材料导报,2018,32(15):2672-2683. 被引量:19

5郑敏,杨瑾,张华.多孔金属材料的制备及应用研究进展[J].材料导报,2022,36(18):74-89. 被引量:8

6彭明媚,汪涛,何庆贤,武鑫,郑长天,王倩.纳米级Al_2O_3/Ni基高温合金复合粉末的制备及激光3D打印研究[J].稀有金属与硬质合金,2019,47(2):57-62. 被引量:2

7周瑜,楼淼森,张逸卿,朱和国.镍基复合材料制备研究进展[J].冶金工程,2016,3(2):57-63.

1王智勇,张国光,谢小林,邵志松,周韦,李琴,曹径倩,史少欣.不同电流密度对304不锈钢表面多孔铜层影响[J].南昌航空大学学报:自然科学版,2020(1):64-69.

2韩斌慧,原彩霞,唐必亮.采掘机械密封纸垫冲孔工具的3D打印技术研究[J].矿山机械,2019,47(1):55-59. 被引量:1

3杨晶,龚诚,赵佳宇,田浩琳,孙陆,陈平,林列,刘伟伟.利用3D打印技术制备太赫兹器件[J].中国光学,2017,10(1):77-85. 被引量:10

4梁建平.三维激光3D打印技术在数字化重现中的应用[J].激光杂志,2018,39(6):125-129. 被引量:3

5邱星武,吴明军,戚燕,刘春阁,张云鹏,黄崇湘.激光熔覆Al_2CrFeCoCuNi_xTi高熵合金涂层的组织及耐蚀性能(英文)[J].红外与激光工程,2018,47(7):90-97. 被引量:14

6彭进,张文洁,王星星,郭国全,张芙蓉.焊丝熔化填充方式对激光焊接熔池影响的数值模拟[J].红外与激光工程,2018,47(3):99-105. 被引量:4

7胡晓冬,黄利安,朱秀晖,姚建华,林英华.大功率激光立体成形熔道几何参数量化模型[J].浙江工业大学学报,2019,47(1):47-52. 被引量:2

8李帅,赵国忠,郭姣艳.4种三维打印材料的太赫兹光谱特性检测与分析[J].中国激光,2019,46(6):244-250. 被引量:3

9陈继文,陈清朋,王琛,杨红娟,李鑫.面向熔融沉积成型技术的曳引机壳拓扑结构优化设计[J].中国工程机械学报,2019,17(4):304-310. 被引量:2

10邱星武.激光熔覆Fe0.5NiCoCrCuTi高熵合金涂层的微观结构及性能(英文)[J].红外与激光工程,2019,48(7):141-148. 被引量:4

1王林,张覃轶,祝柏林,王爱华,谢长生.激光烧结纳米ZnO气敏传感器制备及其气敏特性研究[J].传感技术学报,2003,16(4):491-494. 被引量:12

2李亚宁,汤慧萍,王建永,李广忠,康新婷,张文彦,葛渊,杨保军.脱合金法制备纳米多孔镍材料研究进展[J].中国材料进展,2011,30(10):49-53. 被引量:2

3徐志锋,余欢,郑玉惠,蔡长春,严青松.碳化硅陶瓷预制体的选区激光烧结及真空压力渗铝[J].中国有色金属学报,2008,18(10):1864-1871. 被引量:4

4杨英惠(摘译).直接激光烧结法制造Co-Cr合金零件[J].现代材料动态,2007(4):11-11.

5郭世杰,乐启炽,崔建忠.加钙耐热镁合金的最新研究进展[J].材料导报,2004,18(10):44-46. 被引量:16

6黄文梅(摘译).用激光烧结法制备钛螺纹型牙种植体[J].现代材料动态,2010(6):12-12.

7守吉佑介,清水祯树,渡边隆行,张毅.B-C-N系纳米管的合成[J].上海钢研,2001(3):67-74.

8闫春泽,史玉升,杨劲松,黄树槐.高分子材料SLS中次级烧结实验[J].华中科技大学学报:自然科学版,2008,36(5):86-89. 被引量:12

9李宇,刘征,黄亦工.多次金属化烧结的初步探讨[J].真空电子技术,2006,19(2):49-51.

10朱旭.TriMode探测实现更高的调试效率及易用性[J].工业设计,2009(3):16-16.

Basic Information:

DOI:

Chinese Library Classification Number:TB333[一般工业技术—材料科学与工程]

Citation Information:

The laser sint alloy and TiH2. The mi formation mechanisms cussed. In the sintered ering experiment was carried out on the powder mixture of self-melting nickel-based crostructure of sintered samples was characterized by XRD,SEM and EDX. And the of porous structure and precipitated phase in sintered samples were simply dis samples, the reinforcing phases TiC and TiBz are in-situ synthesized and structure is also formed. A large number of micron-sized pores are uniformly dispersed in the matrix as the high-temperature strengthening phase CrB with a radial or acicular-lobate shape. porous as well

quote

GB/T 7714-2015 [1] YU Xiu-ping, SHEN Yi-fu, GU Dong-dong. Preparation of In-situ Reinforced Porous Nickel-based Composites by Laser Sintering[J]. Rare Metals and Cemented Carbides, 2009(4): 11-14.
MLA [1] YU Xiu-ping, et al., "Preparation of In-situ Reinforced Porous Nickel-based Composites by Laser Sintering." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 11-14.
APA [1] YU Xiu-ping, SHEN Yi-fu, & GU Dong-dong. (2009). Preparation of In-situ Reinforced Porous Nickel-based Composites by Laser Sintering. Rare Metals and Cemented Carbides(4), 11-14.
IEEE [1] YU Xiu-ping, SHEN Yi-fu, and GU Dong-dong, "Preparation of In-situ Reinforced Porous Nickel-based Composites by Laser Sintering," Rare Metals and Cemented Carbides, no. 4, pp. 11-14, 2009. keywords: {laser sintering;in-situ reinforcement;porous structure;nickel-based alloy;TiH2;composite}