Study on High and Low Temperature Mechanical Properties of Powder Metallurgy Be-Al Alloy AITranslate
Abstract AITranslate
Tensile tests were conducted on powder metallurgy Be-Al alloy at -100~500 ℃ ,and the effect of temperature on its mechanical properties was analyzed. Its fracture morphologies at different tempera- ture were obtained using scanning electron microscope. The results show that both tensile strength and yield strength decrease with improved temperature, but elongation firstly rises and then falls with improved temperature. The fracture mechanism of Be-Al alloy varies with improved temperature. At low tempera- ture, it is characterized by the mixed fracture of cleavage fracture of beryllium phase and ductile fracture of aluminum phase. With the temperature increasing, cracking of Be/Al interface and ductile fracture of alu- minum phase become main fracture morphologies. The inner stress field distribution of Be-Al alloy in high and low temperature tensile process is simulated with ABAQUS finite element software to reveal the me- chanical mechanism of transition of tensile fracture mode of Be-Al alloy at high temperature.
KeyWords AITranslate
1张健康,栾新刚,王战宏,王东新,李军义,代彦明,吕一格,李美岁.高铍铸造铍铝合金延伸率的评价指标[J].理化检验:物理分册,2016,0(6):375-378. 被引量:6
2张秋平,张永寿.Be-Al合金的机械性能[J].飞航导弹,2002(12):57-61. 被引量:8
3马玲,赵双群.铍铝合金的研究进展[J].材料导报,2005,19(F11):431-433. 被引量:10
4刘孝宁,马世光.铍铝合金的研究与应用[J].稀有金属,2003,27(1):62-65. 被引量:28
5王战宏,王莉,吴艳青,曲选辉.铍铝合金室温拉伸及原位疲劳失效分析[J].粉末冶金技术,2007,25(3):163-166. 被引量:6
6张健康,浮国运,栾新刚,王战宏,王东新,赵志灵,李美岁,吕一格,李志年.铍铝合金显微组织的评定方法[J].理化检验:物理分册,2015,51(5):320-322. 被引量:5
7马玲,赵双群.粉末冶金铍铝合金拉伸性能的有限元模拟[J].宁夏工程技术,2009,8(1):49-51. 被引量:4
8邱志聪,肖大武,陈向林,郎定木.温度对铍力学性能的影响[J].稀有金属,2015,39(1):16-22. 被引量:11
9许德美,李峰,王战宏,何力军,任玉平,裴文利,秦高梧.粉末热等静压和铸造Be-Al合金的室温拉伸断裂机理[J].中国有色金属学报,2009,19(12):2128-2135. 被引量:10
10马玲,冯婷,焦旗,赵双群.粉末冶金铍铝合金的微屈服行为及其机理[J].稀有金属材料与工程,2012,41(10):1795-1798. 被引量:3
1吕一格,张健康,代彦明,李美岁,赵志灵,李志年,李军义,魏冬冬.62Be-38Al合金高、低温力学性能及断裂机制[J].稀有金属与硬质合金,2020,48(3):73-76. 被引量:2
1夏一骁,匡泽洋,鞠渤宇,杨文澍,武高辉.铍/铝复合材料制备技术与性能设计研究进展[J].铸造技术,2023,44(6):514-524.
2王晶,彭仕先,王旻,张晨,张新建.基于球形铍粉制备的Be-50Al合金热变形行为研究[J].稀有金属材料与工程,2023,52(8):2901-2908.
1高福彬,张守伟,李建文,靖振权,丁剑,周丹.460C钢高温塑性变形行为研究[J].河南冶金,2017,25(4):5-7. 被引量:1
2侍光磊,张璟瑜,胡丰,潘晓扬,张英波,李康宁,吉华.6005A-T6铝合金型材双轴肩搅拌摩擦焊接头组织及力学性能[J].焊接,2017(8):21-25. 被引量:5
3陈涛,刘政,刘小梅.熔体搅拌方式对半固态A356-0.5Ce合金凝固组织和力学性能的影响[J].稀有金属与硬质合金,2017,45(4):47-51. 被引量:3
4张涛,樊文欣,席奇豪,孔维静,吉梦雯.错距旋压对连杆衬套硬度和微观组织的影响[J].热加工工艺,2017,46(15):151-153. 被引量:1
5李贺军,罗守靖,霍文灿.液态模锻对ZnAl4Cu3合金冲击韧性和断口形貌的影响[J].兵器材料科学与工程,1990(8):18-21.
6唐甜,张丁非,胡光山,胥钧耀,潘复生.挤压态ZM61-Sn合金的显微组织及高温力学性能(英文)[J].稀有金属材料与工程,2017,46(8):2102-2107. 被引量:2
7赵勇,田伟,祝成炎,张春娥,权利军,周慧慧.PLA/苎麻与PVA/苎麻复合材料的制备及其力学性能研究[J].现代纺织技术,2017,25(5):1-6. 被引量:4
8陈健,邱全荟,李晋升,赵蕾,季星星.采用V和Cu复合过渡段的TA2和304SS的激光焊接[J].热加工工艺,2017,0(19):48-50.
9孙云辉,周建忠,盛杰,黄舒,徐苏强,李京,徐高峰.深冷激光喷丸强化2024-T351铝合金拉伸性能及断口分析[J].中国激光,2017,44(8):107-114. 被引量:5
10闫雪艳,于江江,张克利.汽车底盘用DP780双相钢拉弯成形与断裂微观特征研究[J].铸造技术,2017,38(8):2001-2004.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.2[金属学及工艺—金属材料]
Citation Information:
Tensile tests were conducted on powder metallurgy Be-Al alloy at -100~500 ℃ ,and the effect of temperature on its mechanical properties was analyzed. Its fracture morphologies at different tempera- ture were obtained using scanning electron microscope. The results show that both tensile strength and yield strength decrease with improved temperature, but elongation firstly rises and then falls with improved temperature. The fracture mechanism of Be-Al alloy varies with improved temperature. At low tempera- ture, it is characterized by the mixed fracture of cleavage fracture of beryllium phase and ductile fracture of aluminum phase. With the temperature increasing, cracking of Be/Al interface and ductile fracture of alu- minum phase become main fracture morphologies. The inner stress field distribution of Be-Al alloy in high and low temperature tensile process is simulated with ABAQUS finite element software to reveal the me- chanical mechanism of transition of tensile fracture mode of Be-Al alloy at high temperature.
quote
| GB/T 7714-2015 | [1] ZHANG Jian-kang, LI Yan, WANG Zhan-hong, et al. Study on High and Low Temperature Mechanical Properties of Powder Metallurgy Be-Al Alloy[J]. Rare Metals and Cemented Carbides, 2017(4): 71-75. |
| MLA | [1] ZHANG Jian-kang, et al., "Study on High and Low Temperature Mechanical Properties of Powder Metallurgy Be-Al Alloy." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 71-75. |
| APA | [1] ZHANG Jian-kang, LI Yan, WANG Zhan-hong, XIA Biao, DAI Yan-ming, LV Yi-ge, LI Mei-sui, ZHONG Jing-ming, & LI Jun-yi. (2017). Study on High and Low Temperature Mechanical Properties of Powder Metallurgy Be-Al Alloy. Rare Metals and Cemented Carbides(4), 71-75. |
| IEEE | [1] ZHANG Jian-kang, LI Yan, WANG Zhan-hong, XIA Biao, DAI Yan-ming, LV Yi-ge, LI Mei-sui, ZHONG Jing-ming, and LI Jun-yi, "Study on High and Low Temperature Mechanical Properties of Powder Metallurgy Be-Al Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 71-75, 2017. keywords: {Be-Al alloy;mechanical property;tensile fracture;fracture mechanism;simulation} |