Study on the Mechanism of Preparation of De-β-layered Gradient Cemented Carbide with Nitrogen-free Raw Material AITranslate
Abstract AITranslate
De-β-1ayered gradient cemented carbide was prepared by micro-pressure nitrification and vacuum denitrification sintering with nitrogen-free raw material. The microstructure and element distribution of al- loy samples at different sintering steps were analyzed by SEM, EDS and EPMA techniques, their micro- structure evolution rules during sintering were investigated,and the formation mechanisms of cubic carbide free layer and Co-rich layer were summarized. The results indicate that TiC phase in the cemented carbide is nitrided to Ti(C,N) phase during micro-pressure nitrification. And then the dissolution of Ti(C,N) into the liquid phase and the N-Ti coupling diffusion result in the formation of cubic carbide free layer during denitrification sintering. The combined action of Co vacancy diffusion and liquid migration is responsible for the formation of Co-rich layer. Liquid migration during cooling results in the difference of Co content in dif- ferent regions of Co-rich layer.
KeyWords AITranslate
1史留勇,刘义敏,张守全,黄继华,张华,赵兴科.脱β层梯度硬质合金的制备及组织结构[J].粉末冶金材料科学与工程,2011,16(1):67-72. 被引量:10
2陈健,刘伟,伍尚华.表层富钴无立方相梯度硬质合金的制备及性能研究[J].人工晶体学报,2015,44(9):2555-2559. 被引量:2
3史留勇,刘义敏,张守全,黄继华,赵兴科.初始成分对梯度硬质合金微观组织及脱β层厚度的影响[J].中国有色金属学报,2012,22(7):1984-1990. 被引量:6
4张守全.碳含量对脱β层硬质合金组织和性能的影响[J].粉末冶金技术,2015,33(1):17-21. 被引量:4
1魏恒生,沈金城,姚蕾,杨海涛.高速重载火车轮毂加工刀片的材质分析[J].硬质合金,2021,38(3):165-170.
2欧阳水林,蒋俊鹏,钟志强,邱联昌,羊求民,谭卓鹏,雷志军,陈颢.TiN添加量对WC-TiC-TaNbC-10Co硬质合金组织结构及性能的影响[J].有色金属科学与工程,2022,13(4):54-60. 被引量:2
1曾湘华,汤昌仁,梁瑜,刘恒嵩,鄢志刚,林森.烧结碳气氛对CVD涂层刀片基体脱β层厚度的影响[J].中国钨业,2023,38(1):37-43.
2胡煜,赖朝彬,郑晓楠,罗迪强,邓庚凤.钛微合金钢研究现状及进展[J].江西冶金,2023,43(4):298-305.
1郑宁来.我国首创玉米芯制石墨烯[J].石油炼制与化工,2017,48(9):68-68.
2宁波氧誉科技:为国民提供充足氧气[J].浙江经济,2017,0(17).
3余立刚.液压缸双向制动阀的研究[J].南方农机,2017,48(18):55-55.
4李娟,周春英.中国水泥工业汞排放迁移机制及减排技术研究项目在北京正式启动[J].中国建材,2017,0(9):127-127.
5常进,张新建,刘清才,任山,王小青,周健.添加城市污泥对烧结过程及烧结矿质量的影响[J].钢铁研究学报,2017,29(9):711-716. 被引量:3
6龚虎.化学元素对12%Cr钢中铁素体含量的影响[J].大型铸锻件,2017(5):24-26.
7骆远征,邓永荣,岑伟富.六方相和立方相CdS声子色散和热力学特性研究[J].都市家教:下半月,2017,0(9):272-273.
8孙永哲,田笑,魏亚风,庄艳歆.热处理对冷轧变形Al_(0.3)CoCrFeNi高熵合金组织与力学性能的影响[J].材料热处理学报,2017,38(9):18-23. 被引量:9
9李孟孟,姜涛,KHUMBANYIWA Davison Daniel,刘洪波,杨健.基于耳石微化学的长江安徽和县江段刀鲚生境履历重建[J].水生生物学报,2017,41(5):1054-1061. 被引量:16
10夏碧华,高建,丁力,薛逊,吴道洪.电石冶炼原料制备工艺研究进展[J].煤炭加工与综合利用,2017(8):68-70. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
De-β-1ayered gradient cemented carbide was prepared by micro-pressure nitrification and vacuum denitrification sintering with nitrogen-free raw material. The microstructure and element distribution of al- loy samples at different sintering steps were analyzed by SEM, EDS and EPMA techniques, their micro- structure evolution rules during sintering were investigated,and the formation mechanisms of cubic carbide free layer and Co-rich layer were summarized. The results indicate that TiC phase in the cemented carbide is nitrided to Ti(C,N) phase during micro-pressure nitrification. And then the dissolution of Ti(C,N) into the liquid phase and the N-Ti coupling diffusion result in the formation of cubic carbide free layer during denitrification sintering. The combined action of Co vacancy diffusion and liquid migration is responsible for the formation of Co-rich layer. Liquid migration during cooling results in the difference of Co content in dif- ferent regions of Co-rich layer.
quote
| GB/T 7714-2015 | [1] YANG Jin-wei, SHI Liu-yong, ZHOU Teng, et al. Study on the Mechanism of Preparation of De-β-layered Gradient Cemented Carbide with Nitrogen-free Raw Material[J]. Rare Metals and Cemented Carbides, 2017(4): 76-81. |
| MLA | [1] YANG Jin-wei, et al., "Study on the Mechanism of Preparation of De-β-layered Gradient Cemented Carbide with Nitrogen-free Raw Material." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 76-81. |
| APA | [1] YANG Jin-wei, SHI Liu-yong, ZHOU Teng, ZHANG Xian-man, & LUO Hong-feng. (2017). Study on the Mechanism of Preparation of De-β-layered Gradient Cemented Carbide with Nitrogen-free Raw Material. Rare Metals and Cemented Carbides(4), 76-81. |
| IEEE | [1] YANG Jin-wei, SHI Liu-yong, ZHOU Teng, ZHANG Xian-man, and LUO Hong-feng, "Study on the Mechanism of Preparation of De-β-layered Gradient Cemented Carbide with Nitrogen-free Raw Material," Rare Metals and Cemented Carbides, no. 4, pp. 76-81, 2017. keywords: {gradient cemented carbide;nitrogen-free raw material;cubic carbide free layer;Co-rich layer;for- mation mechanism} |