Experimental Study on Production of Deep-drawn Tantalum Sheet by Powder Metallurgy AITranslate

Jiujiang Non-ferrous Metal Smelting Co.,LTD;Jiujiang Non-ferrous Metal Smelting Co.,LTD;Jiujiang Non-ferrous Metal Smelting Co.,LTD;Jiujiang Non-ferrous Metal Smelting Co.,LTD
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Pure tantalum ingot blanks were prepared by powder metallurgy, and tantalum sheets with a thickness of 0. 28 mm were produced through forging and rolling of the ingot blanks. The effects were studied of different particle size proportion, intermediate annealing temperature and product annealing tem- perature on the physical properties of tantalum sheets. The results show that the properties of pure tanta- lum sheets obtained by powder metallurgy such as tensile strength, elongation and microhardness can be controlled to a certain extent through different particle size proportion,intermediate annealing temperature and product annealing temperature, and the properties of the produced tantalum sheets reach the require- ments of customers.

KeyWords AITranslate

tantalum sheet Ta powder metallurgy particle size proportion annealing temperature physical property

1张行健,王志法,姜国圣,陈德欣,张瑾瑾.锭坯生产工艺对纯钽板再结晶温度影响的研究[J].粉末冶金技术,2006,24(2):118-121. 被引量:5

2冯彦国.高比容钽粉的应用对成型、烧结工艺的研究[J].中国科技纵横,2010(21):7-8. 被引量:1

3姜国圣,王志法,崔大田,张行健.纯钽片晶粒大小控制与深冲性能[J].矿冶工程,2007,27(2):78-80. 被引量:6

1近期不锈钢锭坯价格[J].不锈:市场与信息,2004(9):36-36.

2Xiao-Jie Ma,Guo-Fu Ding,Sheng-Feng Qin,Rong Li,Kai-Yin Yan,Shou-Ne Xiao,Guang-Wu Yang.Transforming Multidisciplinary Customer Requirements to Product Design Specifications[J].中国机械工程学报:英文版,2017,30(5):1069-1080. 被引量:4

3张江江.胶印机操作经验谈[J].印刷技术,2017,0(4):65-67.

4周广亮.胶黏剂选择有诀窍[J].印刷工业,2017,0(9):60-61.

5意雯.女婴被打包成快递 寄往福利院[J].天风,2017,0(9):57-57.

6员强鹏,翟冬雨,张炜.正火态X42N管线的工业研发[J].南钢科技与管理,2017,0(3):34-37.

7陈疌瑗.浅析收入会计准则的修订对售后回购业务的影响[J].现代商业,2017(24):140-141. 被引量:2

8姜帆,郭飞,杜君,王于波,庞振江.手机音频读卡器在燃气缴费领域的应用[J].单片机与嵌入式系统应用,2017,17(10):74-77. 被引量:1

9李银娥,姜婷.高温钎料BCu69NiMnCoSiB的制备[J].广州化工,2017,45(18):42-43.

10瓦尔特,Dirk Masu.航空工业:安全快速的钛合金加工——瓦尔特正在使用专用工具改进钛合金加工[J].金属加工:冷加工,2017,0(18):15-16.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.6[冶金工程—有色金属冶金]

Citation Information:

Pure tantalum ingot blanks were prepared by powder metallurgy, and tantalum sheets with a thickness of 0. 28 mm were produced through forging and rolling of the ingot blanks. The effects were studied of different particle size proportion, intermediate annealing temperature and product annealing tem- perature on the physical properties of tantalum sheets. The results show that the properties of pure tanta- lum sheets obtained by powder metallurgy such as tensile strength, elongation and microhardness can be controlled to a certain extent through different particle size proportion,intermediate annealing temperature and product annealing temperature, and the properties of the produced tantalum sheets reach the require- ments of customers.

quote

GB/T 7714-2015 [1] LIU Jun-rong, HU Gen-huo, ZHU Feng, et al. Experimental Study on Production of Deep-drawn Tantalum Sheet by Powder Metallurgy[J]. Rare Metals and Cemented Carbides, 2017(4): 67-70.
MLA [1] LIU Jun-rong, et al., "Experimental Study on Production of Deep-drawn Tantalum Sheet by Powder Metallurgy." Rare Metals and Cemented Carbides, no. 4, 2017, pp. 67-70.
APA [1] LIU Jun-rong, HU Gen-huo, ZHU Feng, & LI Qi-chao. (2017). Experimental Study on Production of Deep-drawn Tantalum Sheet by Powder Metallurgy. Rare Metals and Cemented Carbides(4), 67-70.
IEEE [1] LIU Jun-rong, HU Gen-huo, ZHU Feng, and LI Qi-chao, "Experimental Study on Production of Deep-drawn Tantalum Sheet by Powder Metallurgy," Rare Metals and Cemented Carbides, no. 4, pp. 67-70, 2017. keywords: {tantalum sheet;Ta;powder metallurgy;particle size proportion;annealing temperature;physical property}