Study on Morphology and Properties of Ni-Co/ZrO_2 Composite Coatings AITranslate
Abstract AITranslate
Ni-Co/ZrO2 composite coatings were prepared by ultrasound-assisted electroplating in the system of sulfamate bath. The effects of current density, concentration of ZrO2 particles and ultrasonic power on hardness of Ni-Co/ZrO2 composite coatings were investigated with single variable method. The process pa- rameters of Ni-Co/ZrO2 composite electrodeposition were optimized. The coatings were tested by nanoin- dentation,and the morphology and composition of the optimized composite coatings were characterized by field emission scanning electron microscopy. The research results show that the optimized technological conditions are as follows:cathode current density of 5 A/dm2 , ZrO2 particle concentration of 10 g/L, ultrasonic power of 240 W. Under these conditions, the nanohardness, elastic modulus and the ratio of nanohardness to elastic modulus are up to 6.13 Gpa,291 Gpa and 0. 021 ,respectively. Furthermore,the coating is flat and compact,and ZrO2 nanoparticles are well eomposited in metal matrix.
KeyWords AITranslate
1武占文,陈吉,朴楠,杨明川.Ni-WC纳米复合镀层的制备及钝化性能研究[J].金属学报,2013,49(10):1185-1190. 被引量:12
2彭成章,朱玲玲.电沉积Ni-P/纳米Al_2O_3复合镀层的摩擦磨损与耐铝液侵蚀性能[J].中国有色金属学报,2010,20(6):1177-1182. 被引量:13
3佘晓林,孙万昌,张磊,侯嵬玮,苗春雨.脉冲沉积占空比对Ni-Co-ZrO_2复合镀层摩擦磨损性能的影响[J].稀有金属材料与工程,2013,42(S1):297-300. 被引量:3
4何新快,江雨妹,侯柏龙,吴璐烨,陈白珍.三价铬超声-脉冲电沉积Fe-Ni-Cr/SiC纳米复合镀层[J].北京科技大学学报,2014,36(4):473-481. 被引量:6
5舒绪刚,何湘柱,黄慧民,李大光,谢绍俊,雷华山,赵国鹏.电沉积Cr/ZrO_2复合镀层的结构和摩擦性能[J].中南大学学报:自然科学版,2010,41(3):871-875. 被引量:7
6毕晓勤.工艺参数对Ni-SiC复合镀层组织和性能的影响[J].材料工程,2007,35(5):39-42. 被引量:9
7王美娟,王日初,彭超群,冯艳,张纯,邓黎洁.Ni-金刚石复合镀层的制备[J].中南大学学报:自然科学版,2013,44(7):2688-2695. 被引量:8
8袁庆龙,凌文丹,李平,王海瑞.纳米ZrO_2含量对Ni/ZrO_2刷镀层组织和硬度的影响[J].材料热处理学报,2013,34(6):142-146. 被引量:4
9吴蒙华,刘娜娜,李智.电沉积工艺参数对Ni-TiN-CeO_2二元纳米复合镀层中粒子复合量的影响[J].功能材料,2012,43(19):2657-2660. 被引量:11
10吕镖,汪笑鹤,胡振峰,徐滨士.电沉积超细晶与纳米晶镍镀层的摩擦学行为比较[J].稀有金属材料与工程,2017,46(2):555-560. 被引量:3
1张肇伟.缸套表面沉积镍基碳化硅纳米镀层研究[J].兵器装备工程学报,2019,40(4):215-218. 被引量:2
2周宗熠,温林洁,张丽楠,齐海东,李运刚,杨海丽.TiO2对Sn-Ni合金电极析氢性能的影响[J].钢铁钒钛,2019,40(6):43-47.
3段双陆,傅秀清,沈莫奇,王清清,马文科.回转体表面喷射电沉积Ni-P-ZrO2复合镀层耐腐蚀性能研究[J].材料科学与工艺,2020,28(4):73-81. 被引量:2
1黄嘉乐,王启伟,阳颍飞,王晓明,赵阳,朱胜,李卫.替代电镀铬的碳化硅类复合电镀技术研究进展[J].表面技术,2021,50(1):130-137. 被引量:5
2黄嘉乐,陈德馨,王启伟,王文宇,张保国,朱胜,李卫.活塞表面Ni-P-SiC复合镀层的电沉积及性能表征[J].电镀与涂饰,2021,40(9):669-673. 被引量:4
3孙伟,杨辉,赵国光.超声波辅助磷化对建筑结构钢耐蚀性的影响[J].兵器材料科学与工程,2021,44(3):103-107.
4张宏斌,王金东,赵旭东,陈淑鑫.电流密度对Ni-AlN仿生镀层耐磨性的影响[J].兵器材料科学与工程,2022,45(1):1-6.
1李久顺.金属基质复合材料在汽车上的应用[J].内燃机技术,1991(1):44-47.
2李晓闲,刘美霞,张雪辉,陈颢.热处理对Ni-W-GO复合镀层组织及性能的影响[J].有色金属科学与工程,2017,8(5):115-120. 被引量:2
3陈新祥,刘彦.爆炸冲击载荷作用下靶板动态响应研究[J].兵工学报,2016,37(S2):149-153. 被引量:4
4施海明,陆军.化学镀镍及其应用[J].盐城工学院学报:自然科学版,2000,13(2):47-49. 被引量:1
5向雪琴,高莉洁,祝薇,石龙宇.城市分类研究进展综述[J].标准科学,2018(4):54-62. 被引量:3
6陈华,郭娟利,贾怡红,杜涛.建筑节能参数对全年耗热量的影响研究[J].建筑节能,2018,46(1):90-94. 被引量:8
7罗梦玉,黄宇,姜杰文,黄远星,穆岩.羟基氧化镍催化臭氧氧化水中草酸[J].净水技术,2018,37(3):71-76. 被引量:2
8徐淑庆,郑云云,黄学仁,李家明,蔡成翔.电沉积方法对Ni-ZrO_2复合镀层结构与性能的影响[J].兵器材料科学与工程,2017,40(6):79-82.
9周盛,王小敏.兼性固CO_2、N_2菌BHJ的分子生物学鉴定及生长条件的确定[J].玉林师范学院学报,2017,38(5):83-89.
10杨峰,夏晓雷,徐创.纳米铜润滑油添加剂的摩擦学特性及其自修复机理[J].材料保护,2018,51(2):22-25. 被引量:7
Basic Information:
DOI:
Chinese Library Classification Number:TG148[金属学及工艺—金属材料]
Citation Information:
Ni-Co/ZrO2 composite coatings were prepared by ultrasound-assisted electroplating in the system of sulfamate bath. The effects of current density, concentration of ZrO2 particles and ultrasonic power on hardness of Ni-Co/ZrO2 composite coatings were investigated with single variable method. The process pa- rameters of Ni-Co/ZrO2 composite electrodeposition were optimized. The coatings were tested by nanoin- dentation,and the morphology and composition of the optimized composite coatings were characterized by field emission scanning electron microscopy. The research results show that the optimized technological conditions are as follows:cathode current density of 5 A/dm2 , ZrO2 particle concentration of 10 g/L, ultrasonic power of 240 W. Under these conditions, the nanohardness, elastic modulus and the ratio of nanohardness to elastic modulus are up to 6.13 Gpa,291 Gpa and 0. 021 ,respectively. Furthermore,the coating is flat and compact,and ZrO2 nanoparticles are well eomposited in metal matrix.
quote
| GB/T 7714-2015 | [1] LIANG Zhi-peng, WANG Yi-yong, JIN Hui, et al. Study on Morphology and Properties of Ni-Co/ZrO_2 Composite Coatings[J]. Rare Metals and Cemented Carbides, 2018(2): 59-63. |
| MLA | [1] LIANG Zhi-peng, et al., "Study on Morphology and Properties of Ni-Co/ZrO_2 Composite Coatings." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 59-63. |
| APA | [1] LIANG Zhi-peng, WANG Yi-yong, JIN Hui, ZHOU Xin-yu, & LIU Xiang-lin. (2018). Study on Morphology and Properties of Ni-Co/ZrO_2 Composite Coatings. Rare Metals and Cemented Carbides(2), 59-63. |
| IEEE | [1] LIANG Zhi-peng, WANG Yi-yong, JIN Hui, ZHOU Xin-yu, and LIU Xiang-lin, "Study on Morphology and Properties of Ni-Co/ZrO_2 Composite Coatings," Rare Metals and Cemented Carbides, no. 2, pp. 59-63, 2018. keywords: {Ni - Co/ZrO2 composite coating;electrodeposition;single variable;hardness;nanoindentation;morphology} |