daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Tensile Properties and Deformation Behavior of Beryllium at Different Strain Rate AITranslate

State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin;State Key Laboratory of Special Rare Metal Material,Northwest Rare Metal Material Institute,Shizuishan 753000,Chin
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The strain rate tensile tests of isostatie beryllium were carried out with the universal testing ma- chine at room temperature. The fracture and plastic deformation behavior of beryllium were investigated by using SEM and EBSD techniques. The results show that with the increase of strain rate, the strength of beryllium is increased, but the ductility is decreased and the stress intensity factor of beryllium material is also decreased. In addition, during the stretching process, the slip is the main mechanism of plastic deform- ation. The twin crystals have no obvious effect on plastic deformation for the isotropic effect of mechanical properties of isostatic beryllium,and have little contribution to the plasticity of beryllium.

KeyWords AITranslate

beryllium strain rate stress intensity factor slip stretch twin crystal

1宋德军,张习敏,胡强,周成.铍焊接技术研究发展概况[J].材料导报,2006,20(2):66-69. 被引量:8

2许德美,李峰,王东新,任玉平,裴文利,秦高梧.组织缺陷对金属铍室温断裂行为的影响规律研究[J].稀有金属,2010,34(6):844-849. 被引量:12

3许德美,李峰,王文伟,贾莉.铍中Be_2C及硅基夹杂对铍材伸长率的影响[J].理化检验:物理分册,2005,41(10):491-493. 被引量:3

4王长义,刘正,毛萍莉.{102}拉伸孪晶对AZ31B镁合金动态力学行为及应变速率敏感性的影响[J].热加工工艺,2011,40(12):19-21. 被引量:7

1代彦明,吕一格,王东新,张健康,许德美,钟景明,王小宇.铍室温变形过程中的孪生及织构演变[J].稀有金属与硬质合金,2019,47(3):42-46. 被引量:1

2郑莉芳,刘新宇,鲍帅平,张健康,钟景明,丁玉龙.稀有金属铍的性能研究进展[J].稀有金属,2023,47(2):292-302.

1郑莉芳,刘新宇,鲍帅平,张健康,钟景明,丁玉龙.稀有金属铍的性能研究进展[J].稀有金属,2023,47(2):292-302.

1韩远飞,李九霄,项娟,黄光法,王立强,吕维洁.非连续TiB+TiC颗粒增强钛基复合材料的剧烈塑性变形行为[J].稀有金属材料与工程,2017,46(S1):56-60. 被引量:3

2李曼,薛庆国,佘雪峰,王广,刘迎立,王静松.碱金属(K)对焦炭不同光学组织气化规律的试验研究[J].有色金属科学与工程,2018,9(1):9-14. 被引量:2

3郑海亚,孟晨曦,胡冬力,顾辉,刘海涛,张国军.织构化ZrB_2-SiC超高温陶瓷中取向关系的EBSD研究[J].无机材料学报,2018,33(4):380-384. 被引量:3

4吴恒,张鸿,吕佳峰,林超,刘建纲,陈彦旭.连续柱状晶组织纯铜室温超延展变形机理[J].中国有色金属学报,2017,27(12):2426-2433. 被引量:3

5叶学民,张建坤,李春曦.叶顶改型对双级轴流风机性能影响的仿真研究[J].系统仿真学报,2018,30(4):1511-1519. 被引量:1

6杨凤,黄模佳,赵腾飞,晏洪,刘军.包含织构系数的任意应力状态下六角晶粒正交板材屈服函数理论研究[J].塑性工程学报,2017,24(6):157-164. 被引量:1

7王雪姣,李新娥.基于可靠性的智能电子标签壳体方案优化设计[J].包装工程,2018,39(7):11-15. 被引量:1

8张丽屏,田俊,李建,杨宇,阚前华.基于耦合损伤本构模型的508-3钢循环塑性变形模拟[J].核动力工程,2018,39(1):165-168. 被引量:1

9许晓静,杨帆,赵建吉,朱金鑫,丁清,汪成松.升温速率与固溶时间对超高强铝合金挤压材组织性能的影响[J].稀有金属,2018,42(3):238-245. 被引量:6

10王嘉勇,肖成志,何晨曦.静压桩对邻近埋地管道性能影响的数值分析[J].西南交通大学学报,2018,53(2):322-329. 被引量:12

Basic Information:

DOI:

Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料]

Citation Information:

The strain rate tensile tests of isostatie beryllium were carried out with the universal testing ma- chine at room temperature. The fracture and plastic deformation behavior of beryllium were investigated by using SEM and EBSD techniques. The results show that with the increase of strain rate, the strength of beryllium is increased, but the ductility is decreased and the stress intensity factor of beryllium material is also decreased. In addition, during the stretching process, the slip is the main mechanism of plastic deform- ation. The twin crystals have no obvious effect on plastic deformation for the isotropic effect of mechanical properties of isostatic beryllium,and have little contribution to the plasticity of beryllium.

quote

GB/T 7714-2015 [1] DAI Yan-ming, WANG Dong-xin, ZHANG Jian-kang, et al. Tensile Properties and Deformation Behavior of Beryllium at Different Strain Rate[J]. Rare Metals and Cemented Carbides, 2018(2): 54-58.
MLA [1] DAI Yan-ming, et al., "Tensile Properties and Deformation Behavior of Beryllium at Different Strain Rate." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 54-58.
APA [1] DAI Yan-ming, WANG Dong-xin, ZHANG Jian-kang, LV Yi-ge, LI Mei-sui, LI Jun-yi, LI Shao-yin, & ZHONG Jing-ming. (2018). Tensile Properties and Deformation Behavior of Beryllium at Different Strain Rate. Rare Metals and Cemented Carbides(2), 54-58.
IEEE [1] DAI Yan-ming, WANG Dong-xin, ZHANG Jian-kang, LV Yi-ge, LI Mei-sui, LI Jun-yi, LI Shao-yin, and ZHONG Jing-ming, "Tensile Properties and Deformation Behavior of Beryllium at Different Strain Rate," Rare Metals and Cemented Carbides, no. 2, pp. 54-58, 2018. keywords: {beryllium;strain rate;stress intensity factor;slip;stretch;twin crystal}