The study was carried out on the effect of extrusion temperature on microstructure and properties of beryllium material and its texture evolution during extrusion. The results show that the crystal grains of beryllium ingot are refined after extrusion, and its tensile strength, yield strength and fracture elongation are improved in different degrees. With extrusion temperature increasing, beryllium grain size increases and (1010) fiber texture is enhanced, both affecting the mechanical properties of beryllium rods. In order to ana- lyze the relationship between mechanical properties, crystal structure and texture of extruded beryllium rods, mechanical testing was carried out with the samples obtained according to a certain slope angle along the extrusion direction. It is found that the tensile strength and yield strength significantly decrease, while the fracture elongation greatly increases. Therefore, the plasticity of beryllium material can be improved by controlling texture direction via equal channel extrusion.
KeyWords AITranslate
1钟景明,许德美,李春光,王战宏,李峰,王莉,李志年.金属铍的应用进展[J].中国材料进展,2014,33(9):568-575. 被引量:18
2许德美,秦高梧,李峰,王战宏,钟景明,何季麟,何力军.国内外铍及含铍材料的研究进展[J].中国有色金属学报,2014,24(5):1212-1223. 被引量:34
3吕滨江,彭建,童小山,潘复生.挤压温度对Mg-2.0Zn-0.3Zr-0.9Y新型镁合金组织和性能的影响[J].稀有金属材料与工程,2013,42(4):841-844. 被引量:15
4李玉斌,蒙大桥,刘柯钊,谢志强.铍晶粒长大规律研究[J].稀有金属材料与工程,2008,37(5):812-815. 被引量:3
5丁文江,靳丽,吴文祥,董杰.变形镁合金中的织构及其优化设计[J].中国有色金属学报,2011,21(10):2371-2381. 被引量:64
1吕一格,代彦明,刘兆刚,李志年,赵志灵,张健康,魏冬冬.热挤压对铍铝合金显微组织和性能的影响研究[J].稀有金属与硬质合金,2019,47(5):60-63. 被引量:3
1吕一格,张健康,代彦明,李美岁,赵志灵,李志年,李军义,魏冬冬.62Be-38Al合金高、低温力学性能及断裂机制[J].稀有金属与硬质合金,2020,48(3):73-76. 被引量:2
2鲍文科,高世阳,刘均波,魏文庆,张丽娜.热挤压及固溶对Al-7Zn-2.5Mg-2.5Cu高强铝合金组织与性能的影响[J].热加工工艺,2020,49(19):105-107. 被引量:1
3夏一骁,匡泽洋,鞠渤宇,杨文澍,武高辉.铍/铝复合材料制备技术与性能设计研究进展[J].铸造技术,2023,44(6):514-524.
1余虹云,李瑞,陈庆吟,潘伟健,胡豪竞,吴细毛,侯嘉鹏,王强.纯铝线强度和导电率反常制约现象及机制分析[J].轻合金加工技术,2018,46(2):37-43. 被引量:1
2蔡小勇,唐群华,戴品强.准静态拉伸过程中CoCrFeMnNi高熵合金显微组织的演变[J].中国有色金属学报,2018,28(1):135-141. 被引量:4
3赵子博,王国强,杨晓龙,刘建荣,李玉兰,杨锐.Ti-6246中α相转变织构的形成机制[J].材料研究学报,2017,31(10):796-800. 被引量:4
4潘瑜,张殿涛,谭雨宁,李珍,郑玉峰,李莉.等通道挤压制备医用超细晶Mg-3Sn-0.5Mn合金及其力学性能[J].金属学报,2017,53(10):1357-1363. 被引量:9
5邵梅月,吴文祥,靳丽.挤压温度对Mg-1Gd合金织构演变的影响[J].热加工工艺,2017,0(19):51-54.
6强华,张芝民,张文慧,周璐.挤压比对5154铝合金微结构、织构和力学性能的影响[J].锻压技术,2018,43(3):154-159. 被引量:4
7周丽丹,张增耀,王红霞.ECAP过程中不同形态的Mg_2Si相演变规律及合金性能研究[J].热加工工艺,2017,46(15):53-56. 被引量:2
8李浩,宋言红,唐馨.变温等通道角挤压对Mg-Zn-Mn合金组织与性能的影响[J].热加工工艺,2017,46(23):69-72. 被引量:2
9杨娇娥,丁雪佳,朱姝弱.有机蒙脱土对PP/POE体系微观结构及性能的影响[J].塑料,2018,47(2):37-40.
10孙世仁,刘虹,陈文琳.复杂截面空心铝型材挤压过程数值模拟及模具结构改进[J].模具工业,2018,44(4):19-23. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG146.24[金属学及工艺—金属材料]
Citation Information:
The study was carried out on the effect of extrusion temperature on microstructure and properties of beryllium material and its texture evolution during extrusion. The results show that the crystal grains of beryllium ingot are refined after extrusion, and its tensile strength, yield strength and fracture elongation are improved in different degrees. With extrusion temperature increasing, beryllium grain size increases and (1010) fiber texture is enhanced, both affecting the mechanical properties of beryllium rods. In order to ana- lyze the relationship between mechanical properties, crystal structure and texture of extruded beryllium rods, mechanical testing was carried out with the samples obtained according to a certain slope angle along the extrusion direction. It is found that the tensile strength and yield strength significantly decrease, while the fracture elongation greatly increases. Therefore, the plasticity of beryllium material can be improved by controlling texture direction via equal channel extrusion.
quote
| GB/T 7714-2015 | [1] LV Yi-ge, WANG Dong-xin, DAI Yan-ming, et al. Study on Microstructure and Properties of the Extruded Beryllium at Different Temperatures and Proposals for Extrusion Process[J]. Rare Metals and Cemented Carbides, 2018(2): 49-53. |
| MLA | [1] LV Yi-ge, et al., "Study on Microstructure and Properties of the Extruded Beryllium at Different Temperatures and Proposals for Extrusion Process." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 49-53. |
| APA | [1] LV Yi-ge, WANG Dong-xin, DAI Yan-ming, XIN Meng-ming, LI Mei-sui, ZHANG Jian-kang, LIU Zhao-gang, & WANG Zhan-hong. (2018). Study on Microstructure and Properties of the Extruded Beryllium at Different Temperatures and Proposals for Extrusion Process. Rare Metals and Cemented Carbides(2), 49-53. |
| IEEE | [1] LV Yi-ge, WANG Dong-xin, DAI Yan-ming, XIN Meng-ming, LI Mei-sui, ZHANG Jian-kang, LIU Zhao-gang, and WANG Zhan-hong, "Study on Microstructure and Properties of the Extruded Beryllium at Different Temperatures and Proposals for Extrusion Process," Rare Metals and Cemented Carbides, no. 2, pp. 49-53, 2018. keywords: {beryllium material;extrusion;temperature;mechanical property;fiber texture;fracture elongation} |