Effect of Low-speed Wire Cut Electrical Discharge Machining on the Bending Strength of Ti(C,N)-based Cermet AITranslate

Powder Metallurgy Research Institute,Central South University;Powder Metallurgy Research Institute,Central South University;Powder Metallurgy Research Institute,Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effect of low-speed wire cut electrical discharge machining (WEDM-LS) on the bending strength of Ti(C,N)-based cermet of Ti(C,N)-7%WC -20%Ni-7%Mo was studied by hydraulic universal testing machine. The morphology and chemical composition of the machining surface, and the microstruc- ture of the deterioration layer were observed and analyzed by SEM and EDS. The results show that WEDM -LS causes obvious electrical erosion deterioration layer, significantly reducing the bending strength and increasing the intensity dispersion of the sample. There are a large number of microscopic defects such as micro-cracks,holes and grain shedding in microstructure of the deterioration layer.

KeyWords AITranslate

low-speed wire cut electrical discharge machining Ti(C N)-based cermet bending strength de- terioration layer grinding

1郭涛,王笃诚.关于电火花线切割变质层的研究[J].电子工艺技术,1991(2):40-47. 被引量:2

2刘寿荣.电火花切割加工对WC—Co硬质合金显微结构的影响[J].粉末冶金技术,1991,9(2):83-89. 被引量:1

3绪方,张颖.电火花加工表面的残余应力与变质层[J].国外金属加工,1993(1):19-25. 被引量:1

4贾昌乐,王晓冬,马德通.电加工表面变质层与模具使用寿命[J].电加工,1996(1):18-22. 被引量:8

5郑富强,邹丹,臧海天.硬质合金线切割加工变质层的形成及对材料性能的影响[J].电加工与模具,2009(5):18-20. 被引量:4

6张方圆,段春争,王敏杰.已加工表面变质层的发展研究[J].机械设计与制造,2014(10):265-268. 被引量:4

7郑富强,陈康华,李詠侠,邹丹.基于正交试验的硬质合金电火花加工实验分析[J].模具制造,2016,16(2):68-70. 被引量:3

8孙瑶,巩亚东,刘寅.慢走丝电火花线切割TC4试验研究和参数优化[J].东北大学学报:自然科学版,2016,37(7):979-983. 被引量:9

9郭崇文,李文斌.YG6硬质合金电火花线切割加工工艺参数研究[J].稀有金属与硬质合金,2015,43(3):67-70. 被引量:18

10边留进,林子超,孙方宏,郭松寿.基于正交试验的慢走丝电火花线切割加工的参数优化[J].现代制造工程,2013(10):1-5. 被引量:21

1赵丽丽.机械加工对金属零件加工精度的影响[J].世界有色金属,2019,0(5):227-228. 被引量:2

1杨鲧.机械加工中加工精度的影响因素与控制[J].机电工程技术,2019,48(12):84-85. 被引量:4

2孙波.机械齿轮轴加工工艺与优化研究与发展趋势[J].中国金属通报,2020(13):268-269. 被引量:1

1郭霜,许甲岿,程中甫,付猛.摆线轮慢走丝线切割加工关键技术研究[J].现代制造技术与装备,2018,54(2):85-86. 被引量:2

2激发创想 展望未来[J].现代制造,2017,0(40):62-62.

3樊长昕.不同矿料级配对抗车辙剂沥青混合料高温性能的影响[J].山西交通科技,2017(5):27-30. 被引量:2

4Junichi SUZUMURA,周贤全(译).用导电润滑脂预防滚动轴承电蚀[J].国外铁道车辆,2018,55(2):33-37. 被引量:2

5P.WU,S.C.LIU,X.R.JIANG.Effect of multi-walled carbon nanotube addition on the microstructures and mechanical properties of Ti(C,N)-based cermets[J].先进陶瓷(英文),2018,7(1):58-63. 被引量:1

6张仁奇.步进电机位置采集在显微缺陷检测系统中的应用[J].通讯世界,2017,23(21):145-146.

7张敏敏,陈森,于泽州,刘赞,陈庸,彭强,李达.沉积行为对电火花沉积Ti(C,N)涂层微结构的调控机制[J].热加工工艺,2018,47(4):159-163. 被引量:2

8杨琦,杨天钧.35CrMo钢汽车螺栓的断裂失效分析[J].铸造技术,2017,38(12):2900-2902. 被引量:3

9肖光春,张衍路,许崇海,孟祥龙.石墨烯增韧Al_2O_3/Ti(C,N)纳米复合陶瓷刀具材料的制备及其微观结构分析[J].齐鲁工业大学学报,2018,32(2):41-44. 被引量:1

10高磊,林鹏.厂拌热再生沥青混合料的最佳RAP掺量研究[J].华东交通大学学报,2018,35(1):103-108. 被引量:18

Basic Information:

DOI:

Chinese Library Classification Number:TF125.31[冶金工程—粉末冶金]

Citation Information:

The effect of low-speed wire cut electrical discharge machining (WEDM-LS) on the bending strength of Ti(C,N)-based cermet of Ti(C,N)-7%WC -20%Ni-7%Mo was studied by hydraulic universal testing machine. The morphology and chemical composition of the machining surface, and the microstruc- ture of the deterioration layer were observed and analyzed by SEM and EDS. The results show that WEDM -LS causes obvious electrical erosion deterioration layer, significantly reducing the bending strength and increasing the intensity dispersion of the sample. There are a large number of microscopic defects such as micro-cracks,holes and grain shedding in microstructure of the deterioration layer.

quote

GB/T 7714-2015 [1] ZENG Shou-fu, WANG Xiao-ling, YI Jian-hong. Effect of Low-speed Wire Cut Electrical Discharge Machining on the Bending Strength of Ti(C,N)-based Cermet[J]. Rare Metals and Cemented Carbides, 2018(2): 42-48.
MLA [1] ZENG Shou-fu, et al., "Effect of Low-speed Wire Cut Electrical Discharge Machining on the Bending Strength of Ti(C,N)-based Cermet." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 42-48.
APA [1] ZENG Shou-fu, WANG Xiao-ling, & YI Jian-hong. (2018). Effect of Low-speed Wire Cut Electrical Discharge Machining on the Bending Strength of Ti(C,N)-based Cermet. Rare Metals and Cemented Carbides(2), 42-48.
IEEE [1] ZENG Shou-fu, WANG Xiao-ling, and YI Jian-hong, "Effect of Low-speed Wire Cut Electrical Discharge Machining on the Bending Strength of Ti(C,N)-based Cermet," Rare Metals and Cemented Carbides, no. 2, pp. 42-48, 2018. keywords: {low-speed wire cut electrical discharge machining;Ti(C, N)-based cermet;bending strength;de- terioration layer;grinding}