Study on Preparation of High-purity Platinum AITranslate
Abstract AITranslate
High-purity platinum was prepared by the combination process of dissolution of crude platinum with aqua regia-oxidation and carrier hydrolysis-ion exchange-NH4 Cl precipitation,and the effects of impu- rity elements removal in each process step were studied. The experimental results show that platinum can be effectively separated from other precious metals and base metals by dissolution of crude platinum with aqua regia, and then oxidation and carrier hydrolysis,ion exchange and precipitation of Pt-containing solution. The obtained purified (NH4)2 PtCl6 precursor was calcined and washed,and Pt powder was prepared. Based on GDMS analysis,the impurity content in Pt powder is less than 3 ×10^-6 ,and the purity of platinum is more than 99. 999%.
KeyWords AITranslate
1赵飞,吴喜龙,高芳,杨褚伟,郭保金,赵云,曾世勇,明潇.从炉灰、酸泥中回收并提取高纯铂、钯的工艺实验[J].贵金属,2009,30(4):44-47. 被引量:6
2罗瑶,贺昕,熊晓东,陈斐,吴聪,陈峤,李轶轁.离子交换法除去高纯铂中杂质离子的研究[J].贵金属,2013,34(S01):1-3. 被引量:5
3宋元宁.水解法分离Pt-Rh及氯铂酸的制取[J].湿法冶金,1998(2):39-41. 被引量:2
1赵家春,吴跃东,童伟锋,杨海琼,保思敏,裴洪营,董海刚.高纯铂制备技术研究进展[J].贵金属,2020,41(1):92-97. 被引量:5
2杨泉,董海刚,张纯熹,范云鹏,吴跃东,童伟锋,赵家春.从某钌蒸馏渣中回收提纯铂的研究[J].贵金属,2022,43(3):31-34.
1郝海英,张巧霞,熊晓东,罗俊锋,付丰年,于文军,户赫龙,董亭义.新型贵金属材料在5G时代的研究现状及应用展望[J].贵金属,2020,41(S01):68-72. 被引量:4
2李进,刘丰,闫硕,杨瑶,宋妍妍,陆凤鞠.贵金属在电催化析氢中的应用[J].广州化工,2022,50(1):19-21. 被引量:1
3王欢,吴喜龙,熊庆丰,谭文进,杨泉,李勇.加压碱溶综合回收失效重整催化剂中的铂和铝[J].贵金属,2021,42(3):47-50. 被引量:1
4赵雨,吴喜龙,王彪,王欢,李勇,刘文,杨深宏.载体溶解法回收失效Pt/TiO_(2)催化剂中的铂[J].贵金属,2021,42(4):37-40.
5杨泉,董海刚,张纯熹,范云鹏,吴跃东,童伟锋,赵家春.从某钌蒸馏渣中回收提纯铂的研究[J].贵金属,2022,43(3):31-34.
1魏连会,刘宇峰,姬妍茹,董艳,杨庆丽,宋淑敏,石杰,孙兴荣.发酵黑荸荠中挥发性物质的GC-MS分析[J].中国调味品,2018,43(3):140-142. 被引量:7
2朱刚直,易勤,范志宏,马岳慧,王丹丹,王磊,程泽能.LC-MS/MS法测定大鼠血浆中PAC-1的新型抗癌衍生物的浓度及其药物动力学研究(英文)[J].中国药学:英文版,2017,26(11):811-818.
3张园,陈波,张美玲,赵海芹,林琳,林丹,王贤亲.超高效液相色谱-质谱联用法测定生物检材中乌头碱[J].中国法医学杂志,2018,33(1):68-70. 被引量:13
4于辉辉,袁旭音,韩磊,周睿,章琪,唐豆豆.太湖西部流域滨岸带土壤磷形态空间分布与影响因素比较[J].环境科学研究,2018,31(3):537-546. 被引量:1
5吴博文,陈红亮.电解锰陈旧废渣的理化特性分析研究[J].神州,2018,0(11):185-187.
6王一平.用预曝气和预沉淀控制活性污泥沉降性能[J].环境科学与管理,1993,0(4):68-70.
7张盼,刘平,刘新宽,陈晓红,何代华,马凤仓,李伟,张柯.不同成分铜铁合金组织与性能变化研究[J].铸造技术,2018,39(3):506-511. 被引量:6
8陆婷婷,胡国胜,马晓红,姚雷,李玉红.佩兰精油镇静催眠作用的研究[J].上海交通大学学报:农业科学版,2018,36(1):30-35. 被引量:3
9张坤鹏,刘宏,徐进勇.电感耦合等离子体质谱(ICP-MS)法测定高铁基体样品中微量元素[J].中国无机分析化学,2018,8(1):37-40. 被引量:6
10田露,窦金孝,余江龙.氧化镁湿法烟气脱硫反应特性的分析[J].冶金能源,2018,37(2):59-64. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF114[冶金工程—冶金物理化学]
Citation Information:
High-purity platinum was prepared by the combination process of dissolution of crude platinum with aqua regia-oxidation and carrier hydrolysis-ion exchange-NH4 Cl precipitation,and the effects of impu- rity elements removal in each process step were studied. The experimental results show that platinum can be effectively separated from other precious metals and base metals by dissolution of crude platinum with aqua regia, and then oxidation and carrier hydrolysis,ion exchange and precipitation of Pt-containing solution. The obtained purified (NH4)2 PtCl6 precursor was calcined and washed,and Pt powder was prepared. Based on GDMS analysis,the impurity content in Pt powder is less than 3 ×10^-6 ,and the purity of platinum is more than 99. 999%.
quote
| GB/T 7714-2015 | [1] YANG Hai-qiong, ZHAO Jia-chun, CHEN Jia-lin, et al. Study on Preparation of High-purity Platinum[J]. Rare Metals and Cemented Carbides, 2018(2): 64-67. |
| MLA | [1] YANG Hai-qiong, et al., "Study on Preparation of High-purity Platinum." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 64-67. |
| APA | [1] YANG Hai-qiong, ZHAO Jia-chun, CHEN Jia-lin, LI Bo-jie, WANG Ying-wu, & DONG Hai-gang. (2018). Study on Preparation of High-purity Platinum. Rare Metals and Cemented Carbides(2), 64-67. |
| IEEE | [1] YANG Hai-qiong, ZHAO Jia-chun, CHEN Jia-lin, LI Bo-jie, WANG Ying-wu, and DONG Hai-gang, "Study on Preparation of High-purity Platinum," Rare Metals and Cemented Carbides, no. 2, pp. 64-67, 2018. keywords: {high-purity platinum;dissolution with aqua regia;carrier hydrolysis;ion exchange;NHL Cl precipitation} |