daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress of Refractory High-entropy Alloys AITranslate

Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College;Department of Mechanical and Electronic Engineering,Guizhou Communication Vocational College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The research progress of refractory high-entropy alloy is reviewed. The phase composition and crystal structure of refractory high-entropy alloy are analyzed. The performance advantages of refractory high-entropy alloy are introduced,including high temperature stability, strength and hardness and so on. The problems of high-entropy alloy are discussed in the three aspects of mass density, room temperature brittleness and high temperature oxidation resistance. Finally, the future development direction of the refractory high-entropy alloy is pointed out.

KeyWords AITranslate

refractory high-entropy alloy alloy composition crystal structure high temperature oxidation re- sistance research progress development direction

1张素芳,杨潇,张勇.Al_(0.3)CrCuFeNi_2高熵合金单晶材料的制备及性能[J].金属学报,2013,49(11):1473-1480. 被引量:13

2Can Huang,Yi-Zhou Tang,Yong-Zhong Zhang,An-Ping Dong,Jian Tu,Lin-Jiang Chai,Zhi-Ming Zhou.Microstructure and dry sliding wear behavior of laser clad AlCrNiSiTi multi-principal element alloy coatings[J].稀有金属:英文版,2017,36(7):562-568. 被引量:5

3梁红玉,罗娟,颜雨飞.高熵合金在高速切削刀具上的应用及发展趋势[J].材料导报,2013,27(5):115-120. 被引量:10

4张保森,程江波,徐滨士.等离子熔覆(CuCoCrFeNi)95B5高熵合金涂层研究[J].稀有金属材料与工程,2014,43(5):1128-1132. 被引量:14

5梁秀兵,陈永雄,张志彬,郭伟,商俊超.热处理对FeCrNiCoCu高熵合金涂层的影响[J].装甲兵工程学院学报,2013,27(4):96-99. 被引量:13

6任波,马建辉,赵瑞锋,关绍康,张红松.粉末冶金制备AlCrMoNiTi高熵合金的时效硬化特性(英文)[J].稀有金属材料与工程,2014,43(6):1286-1290. 被引量:1

7安旭龙,刘其斌,郑波.激光熔覆制备高熵合金MoFeCrTiWAl_xSi_y涂层的组织与性能[J].红外与激光工程,2014,43(4):1140-1144. 被引量:22

1赵海朝,乔玉林,梁秀兵,胡振峰,陈永雄.轻质高熵合金的研究进展与展望[J].稀有金属材料与工程,2020,49(4):1457-1468. 被引量:10

2要玉宏,梁霄羽,金耀华,王正品,刘江南,南條弘.新型NbMoCrTiAl-1Si-xB(x=0、1)难熔高熵合金的微观组织及高温氧化行为研究[J].表面技术,2020,49(6):224-235. 被引量:6

3李工,戴凤祥,张翼飞,刘庆琦,范笑锋.Al系高熵合金高温氧化性能研究进展[J].燕山大学学报,2021,45(3):189-201. 被引量:6

4夏铭,孙博,王鑫,梁秀兵,沈宝龙.高熵合金增材制造研究现状与展望[J].材料导报,2021,35(13):13119-13127. 被引量:3

5程彩霞,李炎粉,刘师多.冶金烧结温度对发动机用TiZr基非晶合金组织和力学性能的影响[J].粉末冶金工业,2021,31(6):72-76.

6侯庆玲,葛亚琼,畅泽欣,马明锋,李济鹏.选区激光熔化CoCrFeNi-X高熵合金的研究进展[J].粉末冶金工业,2023,33(1):115-119. 被引量:2

1卢煜,李春燕,田霖,翟建树,寇生中.高熵合金的性能研究进展[J].稀有金属,2022,46(10):1352-1364. 被引量:1

2姬留杰,闫胜男,秦勉.固溶温度对VAR制备传感器用Ti-6Ni-3Mo-1Sn合金组织和力学性能的影响[J].真空科学与技术学报,2021,41(3):296-300.

3房晓彤,上官晓峰,邵文婷,徐大鹏,杨巍.反应磁控溅射高熵合金薄膜的工艺与表征[J].西安工业大学学报,2021,41(3):323-331.

4梅金娜,薛飞,吴天栋,卫娜,蔡振.FeCrNiMn高熵合金本构方程的建立[J].材料导报,2021,35(S01):336-341. 被引量:3

5李荣斌,龙文宇,张志玺,张如林,张茂龙.多组元Al_xFeCrVTi_(0.25)高熵合金微观组织与力学性能研究[J].热加工工艺,2021,50(14):27-30. 被引量:1

6邹芹,张萌蕾,李艳国,罗永安.WC硬质合金强韧化的研究进展与展望[J].机械工程学报,2021,57(14):195-204. 被引量:6

7于克东,赵伟,张辉.离焦量对激光熔覆TiCoNiCrFe高熵合金涂层组织与性能的影响研究[J].齐鲁工业大学学报,2021,35(5):55-59. 被引量:2

8宋若康,张琳.CrMn0.3FeVCu0.06高熵合金的微观组织及抗辐照性能[J].稀有金属材料与工程,2021,50(11):4141-4148. 被引量:3

9张舒研,张志彬,王鑫,高洋洋,梁秀兵,王立忠.Cu含量对新型AlNiZrCoYSi高熵非晶合金玻璃形成能力与耐腐蚀性能的影响[J].稀有金属材料与工程,2021,50(12):4587-4591. 被引量:1

10邹芹,张呈祥,李艳国,黎克楠.超薄切割片的加工变形研究现状[J].金刚石与磨料磨具工程,2022,42(1):119-128. 被引量:1

1谢珊珊,李慧,霍东兴,李亚敏.6.5%Si及梯度硅钢的制备工艺[J].热加工工艺,2017,46(18):39-42.

2杨旭升.破解初中物理浮力问题之难[J].中学物理:初中版,2018,36(1):14-14. 被引量:3

3高守雷,张童心,范金辉.浅议中国古代青铜剑的铸造技术[J].铸造技术,2018,39(4):808-811. 被引量:3

4张宇,王晓鹏,孔凡涛,陈玉勇.合金成分对TiAl合金热变形加工影响的研究进展[J].稀有金属材料与工程,2017,46(11):3570-3576. 被引量:7

5何肖飞,曹燕光,王毛球,闫永明,孙挺,尉文超.轧制工艺对22CrMo钢带状组织的影响[J].金属热处理,2018,43(4):134-139. 被引量:6

6尹跃洪,张璐.电场中(MgO)_2吸附H_2的理论研究[J].原子与分子物理学报,2017,34(6):1063-1068.

7于孟生,郝天之,陈齐风,谢军.基于频率法的质量块影响索力敏感性分析[J].建筑结构,2017,47(S1):829-832. 被引量:2

8吴渊,宋温丽,周捷,曹迪,王辉,刘雄军,吕昭平.块体非晶合金的韧塑化[J].物理学报,2017,66(17):126-143. 被引量:7

9屠鹏,边红霞.基于电学参数的鲜切苹果品质检测[J].食品工业科技,2018,39(3):265-269. 被引量:4

10彭超群.《物理冶金学》——跨越半个世纪的材料科学经典著作[J].中国机械工程,2018,29(7):879-881. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TG132.32[一般工业技术—材料科学与工程]

Citation Information:

The research progress of refractory high-entropy alloy is reviewed. The phase composition and crystal structure of refractory high-entropy alloy are analyzed. The performance advantages of refractory high-entropy alloy are introduced,including high temperature stability, strength and hardness and so on. The problems of high-entropy alloy are discussed in the three aspects of mass density, room temperature brittleness and high temperature oxidation resistance. Finally, the future development direction of the refractory high-entropy alloy is pointed out.

quote

GB/T 7714-2015 [1] WANG Yin, GUO Ya-xiong, WANG Zhen, et al. Research Progress of Refractory High-entropy Alloys[J]. Rare Metals and Cemented Carbides, 2018(2): 68-74.
MLA [1] WANG Yin, et al., "Research Progress of Refractory High-entropy Alloys." Rare Metals and Cemented Carbides, no. 2, 2018, pp. 68-74.
APA [1] WANG Yin, GUO Ya-xiong, WANG Zhen, TIAN Xing-qiang, SHANG Xiao-juan, & CHEN Jia. (2018). Research Progress of Refractory High-entropy Alloys. Rare Metals and Cemented Carbides(2), 68-74.
IEEE [1] WANG Yin, GUO Ya-xiong, WANG Zhen, TIAN Xing-qiang, SHANG Xiao-juan, and CHEN Jia, "Research Progress of Refractory High-entropy Alloys," Rare Metals and Cemented Carbides, no. 2, pp. 68-74, 2018. keywords: {refractory high-entropy alloy;alloy composition;crystal structure;high temperature oxidation re- sistance;research progress;development direction}