Preparation and Performance of a New(Ti,V)C Steel Bonded Carbide AITranslate
Abstract AITranslate
A (Ti,V)C steel bonded carbide was prepared by in-situ sintering with the powders of titanium, ferrovanadium, carbon, ferrochromium, ferromolybdenum and iron as its raw materials. The phase composition,microstructure and micro-area composition of the carbide were studied by XRD, SEM and EDS. And the bending strength of the carbide sample was also measured. The results show that the morphology of (Ti,V)C reinforcing phase in the carbide is more regular and rounding than TiC particles. The bending strength is high. Furthermore, cleavage of reinforcing phase, quasi-cleavage of matrix and dimple are presented in the fractographic appearance of the carbide sample.
KeyWords AITranslate
1张焱,尤显卿,田四光,钟成山,丁峰.钢结硬质合金的发展现状[J].热处理,2008,23(1):12-15. 被引量:14
2Roger Nabb. Advantages of ferro-titanit for the metal working industry[J]. Metal Powder Report, 1988, 43 (3) :198-200.
3严有为,魏伯康,傅正义,林汉同,袁润章.原位TiC颗粒增强铁基复合材料及其组织形成机理[J].金属学报,1999,35(10):1117-1120. 被引量:41
4Brown I W M,Owers W R. Fabrication, microstructure and properties of Fe-TiC ceramic-metal composites [J]. Current Applied Physics,2004(4):171-174.
5刘均波,王立梅,刘均海,黄继华.粘结相对原位合成TiC钢结硬质合金组织结构和性能的影响[J].粉末冶金技术,2007,25(4):266-270. 被引量:4
6刘长松,黄继华,殷声.Fe-Ti-C系燃烧合成反应的热力学分析[J].无机材料学报,2002,17(2):288-292. 被引量:7
7Fredricksson H, Hillert M,Nica M. The decomposition of the M2C carbide in high speed steel [J]. Scand J Metall, 1979,12 (8):115-122.
8Utter,Bodenschatz E. Dynamics of low anisotropy morphologies indirectional solidification[J]. Physical Review E,2002,66:5 604-5 611.
9Arenas F, Rondon C, Sepulveda R. Friction and tribological behavior of (Ti,V) C-Co cermets[J]. J Mater Process Technol, 2003,143-144 :822-826.
1郑铮辉,吕健,张伟彬,张建波,李亚军,冯可桃,阚高辉.TiC/ZrC添加量对TiC基钢结硬质合金组织与性能的影响[J].稀有金属与硬质合金,2021,49(2):76-81. 被引量:1
1陈劲松,黄本生,张雷,罗红,李豪,肖晓华,王水波.焊接温度对TM52/304瞬间液相扩散焊接头性能的影响[J].材料科学与工程学报,2023,41(1):107-113.
1龚伟,李华,要小鹏.(Ti,V)C钢结硬质合金的烧结行为及物相分析[J].粉末冶金工业,2009,19(3):30-35. 被引量:2
2龚伟,李华,要小鹏.(Ti,V)C钢结硬质合金的烧结行为、物相及组织结构[J].钢铁钒钛,2009,30(2):80-85. 被引量:2
3龚伟,李华,朱勇.V含量对(Ti,V)C35CrMo钢结硬质合金组织与力学性能的影响[J].粉末冶金技术,2009,27(5):336-340.
4骆世雄.连铸板坯轧材“刨不动”的原因分析[J].连铸,1996,0(1):37-40.
5龚伟,李自胜.(Ti,V)C35CrMo原位烧结钢结硬质合金的热处理及性能的研究[J].粉末冶金工业,2010,20(1):41-46. 被引量:2
6于春兰,曹刚,秦潞潞,李文竹.钢包回转台连杆板坯缺陷分析[J].理化检验:物理分册,2009,45(1):45-47. 被引量:2
7秦桂红,严彪,毛彭龄.含3at.%Ce的Ni-Ti基形状记忆合金的初步研究[J].上海钢研,2004(3):28-31. 被引量:2
8李静.酒钢不锈钢AOD冶炼使用铬铁粉的工艺研究[J].中国设备工程,2016,0(10):65-66.
9孟飞,果世驹,杨霞,张恒,郭林.粉末冶金制备添加20%铜的316L不锈钢/铜复合材料工艺研究[J].粉末冶金工业,2006,16(4):1-4. 被引量:1
10郭西缅,王岚.Fe刻蚀金刚石的研究[J].复合材料学报,1997,14(2):132-136. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF125.32[冶金工程—粉末冶金]
Citation Information:
A (Ti,V)C steel bonded carbide was prepared by in-situ sintering with the powders of titanium, ferrovanadium, carbon, ferrochromium, ferromolybdenum and iron as its raw materials. The phase composition,microstructure and micro-area composition of the carbide were studied by XRD, SEM and EDS. And the bending strength of the carbide sample was also measured. The results show that the morphology of (Ti,V)C reinforcing phase in the carbide is more regular and rounding than TiC particles. The bending strength is high. Furthermore, cleavage of reinforcing phase, quasi-cleavage of matrix and dimple are presented in the fractographic appearance of the carbide sample.
quote
| GB/T 7714-2015 | [1] WANG Hao-hui. Preparation and Performance of a New(Ti,V)C Steel Bonded Carbide[J]. Rare Metals and Cemented Carbides, 2009(4): 22-25. |
| MLA | [1] WANG Hao-hui. "Preparation and Performance of a New(Ti,V)C Steel Bonded Carbide." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 22-25. |
| APA | [1] WANG Hao-hui. (2009). Preparation and Performance of a New(Ti,V)C Steel Bonded Carbide. Rare Metals and Cemented Carbides(4), 22-25. |
| IEEE | [1] WANG Hao-hui, "Preparation and Performance of a New(Ti,V)C Steel Bonded Carbide," Rare Metals and Cemented Carbides, no. 4, pp. 22-25, 2009. keywords: {(Ti, V) C;in-situ sintering;steel bonded carbide;microstructure;micro-area composition} |