Influence of Nb Element on Continuous Cooling Transformation and Microstructure Change of Weathering Steel AITranslate
Abstract AITranslate
Investigation was made of the continuous cooling transformation (CCT) curves of the weathering steels with Nb and without Nb by Gleeble-1500D thermal simulator,and the influences were analyzed of the Nb element and cooling rate on CCT curve and microstructure changing law. The results show that the addition of Nb inhibits phase transformation of the weathering steel and decreases its phase transformation temperature,causing CCT curve to move to the lower right. Under the condition of cooling rate 15 ℃/s,the microstructure of the weathering steel with Nb significantly changes. With the increase of cooling rate, the hardness of the weathering steel with Nb increases gradually. Lots of bainite forms at the cooling rate of above 5 ℃/s,and some martensite forms at the cooling rate of over 20 ℃/s,which is good for strength and performance improvement of the weathering steel.
KeyWords AITranslate
1Mao X P,Cheng X W, Li L J,et al. Research on steel- making process of Ti microalloyed steel during EAF-LF- CSP process [J]. Iron and Steel Supplement, 2006, 41 (1) :218-223.
2赵培林,孙新军,杜显彬,王建军,雍岐龙.终冷温度对不同成分700MPa级耐候钢组织和性能的影响[J].金属热处理,2011,36(6):87-91. 被引量:15
3侯豁然,付俊岩.我国铁道车辆用高强度耐大气腐蚀钢的进展[J].钢铁,2004,39(6):71-74. 被引量:22
4刘丽宏,齐慧滨,卢燕平,李晓刚.耐大气腐蚀钢的研究概况[J].腐蚀科学与防护技术,2003,15(2):86-89. 被引量:108
5于千.耐候钢发展现状及展望[J].钢铁研究学报,2007,19(11):1-4. 被引量:76
6董杰,王华川,张婕,霍喜伟,袁鹏举,董俊华,刘春明.经济耐候钢的研究[J].莱钢科技,2007(5):117-121. 被引量:2
7宗云,赵莉萍,麻永林,王宝峰,宋海彬.低碳含铌微合金钢的连续冷却相变行为及显微组织[J].机械工程材料,2011,35(7):31-34. 被引量:5
8刘秉余,于景媛,李宝绵,崔建忠.微量Nb对低合金钢组织转变的影响[J].材料科学与工程学报,2009,27(3):393-396. 被引量:3
1张贺佳,张俊粉,李吉伟,王宝华,李国民,魏亮亮.Cu合金化对Cr9Mo1钢耐腐蚀及力学性能的影响[J].材料科学与工艺,2018,26(4):73-79. 被引量:6
2张贺佳,张春雷,王琪,张俊粉.含Cu超耐腐蚀钢筋Cr9Mo1的实验研究[J].北方钒钛,2019,0(1):51-56.
1焦海东,刘丽霞,彭军,郑丽丽,吴世杰.国内钢的显微组织耐蚀性研究概述[J].中国铸造装备与技术,2020,55(1):5-12. 被引量:1
2闫志波,陈红卫,贺会敏,王向明.Ni-Cu-Nb复合60Si2Cr弹簧钢的奥氏体连续冷却转变[J].石家庄职业技术学院学报,2020,32(2):5-9.
3于驰,王宏岩,高秀华,王宏伟.冷却工艺对货油舱用耐蚀钢组织性能的影响[J].材料科学与工艺,2020,28(4):31-40. 被引量:1
4于晗.热处理工艺对高强高导铜合金组织级性能的影响[J].材料科学与工艺,2020,28(5):31-37. 被引量:3
5闫志波,赵海涛,陈红卫.301不锈钢螺栓断裂原因分析[J].锻压技术,2020,45(10):7-12. 被引量:2
6侯元盛,左景辉,刘忱,刘常升.货油舱上甲板用耐蚀钢的腐蚀行为[J].腐蚀与防护,2022,43(2):43-47.
1王昭东,曲锦波,王国栋,刘相华,曹刚,马玉璞.10MnMoNiNb钢形变奥氏体连续冷却相变规律和显微组织[J].钢铁研究学报,1999,11(1):37-40. 被引量:8
2张永涛,李荣斌,孙会,黄丽琴,李建新.2.25Cr-1Mo-0.25V低合金耐热钢的相变行为[J].上海电机学院学报,2012,15(2):119-122. 被引量:1
3杨景红,刘清友,孙冬柏,李向阳.冷速及变形对X70级管线钢相变及组织的影响[J].材料热处理学报,2008,29(5):59-63. 被引量:16
4杜辰伟,陆珏钰,兰鹏,张家泉,尚成嘉.奥氏体晶粒度对钢坯铸态热塑性及相变的影响[J].材料热处理学报,2016,37(10):146-153. 被引量:7
5张立红,于浩,杨宪礼,康永林.X70针状铁素体管线钢连续冷却转变及微观组织研究[J].锻压技术,2005(z1):132-136. 被引量:1
6吴茂林,余驰斌,赵刚,张灵杰.XER70S-6钢形变奥氏体连续冷却相变规律和显微组织研究[J].热处理,2006,21(1):21-24. 被引量:1
7黄绪传,殷胜,周丽萍.奥氏体变形对一种Cr-Mo双相钢连续冷却相变的影响[J].物理测试,2017,35(1):21-24. 被引量:2
8郑丽璇,赵翔.Ni-Ti-Nb合金不同变形条件下的相变曲线[J].热加工工艺,2007,36(20):13-14.
9赵明纯,单以银,曲锦波,肖福仁,钟勇,杨柯.控制热加工下管线钢中针状铁素体的形成[J].金属学报,2001,37(8):810-824. 被引量:11
10赵明纯,单以银,肖福仁,李玉海,杨柯.管线钢中针状铁素体的形成及其强韧性的分析[J].材料科学与工艺,2001,9(4):356-358. 被引量:51
Basic Information:
DOI:
Chinese Library Classification Number:TG146.416[金属学及工艺—金属材料]
Citation Information:
Investigation was made of the continuous cooling transformation (CCT) curves of the weathering steels with Nb and without Nb by Gleeble-1500D thermal simulator,and the influences were analyzed of the Nb element and cooling rate on CCT curve and microstructure changing law. The results show that the addition of Nb inhibits phase transformation of the weathering steel and decreases its phase transformation temperature,causing CCT curve to move to the lower right. Under the condition of cooling rate 15 ℃/s,the microstructure of the weathering steel with Nb significantly changes. With the increase of cooling rate, the hardness of the weathering steel with Nb increases gradually. Lots of bainite forms at the cooling rate of above 5 ℃/s,and some martensite forms at the cooling rate of over 20 ℃/s,which is good for strength and performance improvement of the weathering steel.
quote
| GB/T 7714-2015 | [1] XIE Tian-shu, ZHAO Zeng-wu, LI Yan, et al. Influence of Nb Element on Continuous Cooling Transformation and Microstructure Change of Weathering Steel[J]. Rare Metals and Cemented Carbides, 2014(1): 38-41. |
| MLA | [1] XIE Tian-shu, et al., "Influence of Nb Element on Continuous Cooling Transformation and Microstructure Change of Weathering Steel." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 38-41. |
| APA | [1] XIE Tian-shu, ZHAO Zeng-wu, LI Yan, & LI Bao-wei. (2014). Influence of Nb Element on Continuous Cooling Transformation and Microstructure Change of Weathering Steel. Rare Metals and Cemented Carbides(1), 38-41. |
| IEEE | [1] XIE Tian-shu, ZHAO Zeng-wu, LI Yan, and LI Bao-wei, "Influence of Nb Element on Continuous Cooling Transformation and Microstructure Change of Weathering Steel," Rare Metals and Cemented Carbides, no. 1, pp. 38-41, 2014. keywords: {Nb;weathering steel;continuous cooling transformation;microstructure change;cooling rate} |