Investigation on Corrosion Resistance of Ni-based Cladding Layer Reinforced by In-situ Grown VC-WC-W_2C AITranslate

Department of Physics, Henan Institute of Education;Department of Physics, Henan Institute of Education;Department of Physics, Henan Institute of Education
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ni-based cladding layer reinforeed by in-situ grown VC-WC-W2C particles was prepared on the surfarce of 45# steel substrate by laser cladding technology,and its corrosion resistance was studied in 10% H2SO4 solution with static immersion method. The results show that all the Ni-based cladding layers with different contents of V2O5 +WO3 +C exhibit good corrosion resistance in 10% H2SO4 solution, of which the corrosion resistance of Ni-based cladding layer with 25 % (V2O5 + WO3 + C) is the best, almost three times as much as that of pure Ni-60 cladding layer.

KeyWords AITranslate

VC-WC-W2 C Ni60 self-fluxing alloy laser cladding particle reinforcement in-situ growth cor-rosion resistance

1LUO Fang,YAO Jian hua,HU Xia xia,CHAI Guo-zhong.Effect of Laser Power on the Cladding Temperature Field and the Heat Affected Zone[J].钢铁研究学报:英文版,2011(1):73-78. 被引量:25

2李荐,李淳伟,夏亨,刘凡,李艳芬,杨亮,杨俊.添加ZrO_2对Si_3N_4复合陶瓷材料力学性能的影响[J].稀有金属与硬质合金,2012,40(1):38-40. 被引量:7

3周笑薇,晁明举,杨文超.原位生成WB-CrB增强镍基激光熔覆层的耐蚀性研究[J].激光杂志,2011,32(1):43-44. 被引量:5

4葛亚琼,王文先.不同激光功率下镁合金表面激光熔覆Ni60合金涂层的显微组织和磨损性能[J].中国表面工程,2012,25(1):45-50. 被引量:16

5胡泽祥,刘杰瑞,郭纯,周健松,张世堂.激光熔覆NiCoCrAlY/HfB_2复合涂层结构及高温摩擦学性能[J].中国表面工程,2012,25(2):69-74. 被引量:5

6梁会琴,晁明举,王东升,梁二军.Ta_2O_5/Ni60激光熔覆层的耐蚀性研究[J].激光杂志,2007,28(6):78-79. 被引量:4

7邱星武,李刚,邱玲.激光熔覆技术发展现状及展望[J].稀有金属与硬质合金,2008,36(3):54-57. 被引量:54

1高东强,王蕊,陈威,王哲.激光熔覆改善材料性能的研究进展[J].热加工工艺,2017,46(12):14-18. 被引量:19

2王晓峰,赵瑞山,谌志伟.氩弧熔覆NiCrWCAl合金涂层组织结构与性能研究[J].稀有金属与硬质合金,2018,46(3):13-18. 被引量:1

1董虎林,彭建洪,李海琴,毛多鹭,包海萍,杨永潇,李海宾.原位法制备颗粒增强铁基复合材料的研究进展[J].热加工工艺,2017,0(22):23-28. 被引量:4

2王立超,李振,谢小军.汽车发动机ZL109活塞表面激光熔覆及耐蚀性能研究[J].铸造技术,2018,39(4):910-913. 被引量:2

3付祖冈,张自强,孟贺超,程相榜.激光熔覆技术在高腐蚀环境下液压支架的试验研究[J].煤炭科学技术,2018,46(5):155-159. 被引量:12

4练国富,张浩,黄旭,陈昌荣,江吉彬.热传导环境因素对激光熔覆成形质量的影响[J].应用激光,2018,38(5):705-712.

5陈晶,颜飞雪.基于激光熔覆技术的热防护材料选择[J].材料导报,2018,32(A02):322-325. 被引量:1

6何昱煜,刘益剑,陈明,黄无云,戴鑫,毛建良,徐泽玮.激光扫描速率与熔覆层组织性能的规律研究[J].激光技术,2019,43(2):201-204. 被引量:8

7顾彩香,顾昊文,李文戈,朱冠军,冯杰才.激光熔覆技术在船舶工程中的研究状况[J].船舶工程,2019,41(1):74-78. 被引量:4

8丁阳喜,张远昊,邵晓峰.高速轮轨钢超声振动辅助激光熔覆涂层的滚动摩擦磨损性能[J].材料保护,2019,52(3):6-12.

9江国业,徐平,李敏,庞铭,王岩.扫描速度对激光熔覆Ni35微观组织与力学特性的影响[J].热加工工艺,2019,48(16):96-101. 被引量:4

10徐平,江国业,胡艳娇,庞铭.匙孔效应对激光熔覆层横截面几何形貌的影响研究[J].表面技术,2019,48(10):125-130. 被引量:5

1王长生,杨蕴林.WC加入量对Ni60自熔合金喷焊层磨粒磨损性能影响[J].热加工工艺,1997,26(1):28-30. 被引量:16

2卢金斌.真空熔结镍基合金的界面组织研究[J].真空,2006,43(6):30-31. 被引量:7

3雷宇,罗军明,万润根.Y_2O_3对45钢表面激光熔覆镍基合金的影响[J].新技术新工艺,2007(8):64-65. 被引量:3

4周笑薇,晁明举,王文丽.碳纳米管对Ni60激光熔覆层的耐蚀性影响[J].激光杂志,2007,28(2):75-76. 被引量:2

5姚秀军,边秀房,宋金子.厚镍基激光熔覆层的研究[J].特种铸造及有色合金,2009(8):776-778. 被引量:2

6周思华,晁明举,刘奎立,郭艳花.原位生成WC-B_4C增强镍基激光熔覆层及其性能研究[J].表面技术,2014,43(3):25-30. 被引量:15

7卢金斌,穆云超,毋新房.激光熔覆添加稀土Ni基合金涂层的组织[J].热加工工艺,2007,36(16):53-55. 被引量:1

8罗军明,张剑平,温桢洪.Y_2O_3对40Cr钢激光熔覆层组织性能影响[J].应用激光,2009,29(5):402-404. 被引量:2

9卢金斌.真空熔结镍基合金涂层性能的研究[J].表面技术,2006,35(6):25-26. 被引量:12

10相珺,李刚,邱玲,况军,邱星武.ZrO_2增强镍基激光熔覆层的组织与性能[J].机械工程材料,2009,33(2):59-62. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG174.4[金属学及工艺—金属表面处理]

Citation Information:

Ni-based cladding layer reinforeed by in-situ grown VC-WC-W2C particles was prepared on the surfarce of 45# steel substrate by laser cladding technology,and its corrosion resistance was studied in 10% H2SO4 solution with static immersion method. The results show that all the Ni-based cladding layers with different contents of V2O5 +WO3 +C exhibit good corrosion resistance in 10% H2SO4 solution, of which the corrosion resistance of Ni-based cladding layer with 25 % (V2O5 + WO3 + C) is the best, almost three times as much as that of pure Ni-60 cladding layer.

quote

GB/T 7714-2015 [1] YANG Ning, LI Li-kai, ZHAO Xian-lin. Investigation on Corrosion Resistance of Ni-based Cladding Layer Reinforced by In-situ Grown VC-WC-W_2C[J]. Rare Metals and Cemented Carbides, 2014(1): 42-45.
MLA [1] YANG Ning, et al., "Investigation on Corrosion Resistance of Ni-based Cladding Layer Reinforced by In-situ Grown VC-WC-W_2C." Rare Metals and Cemented Carbides, no. 1, 2014, pp. 42-45.
APA [1] YANG Ning, LI Li-kai, & ZHAO Xian-lin. (2014). Investigation on Corrosion Resistance of Ni-based Cladding Layer Reinforced by In-situ Grown VC-WC-W_2C. Rare Metals and Cemented Carbides(1), 42-45.
IEEE [1] YANG Ning, LI Li-kai, and ZHAO Xian-lin, "Investigation on Corrosion Resistance of Ni-based Cladding Layer Reinforced by In-situ Grown VC-WC-W_2C," Rare Metals and Cemented Carbides, no. 1, pp. 42-45, 2014. keywords: {VC-WC-W2 C;Ni60 self-fluxing alloy;laser cladding;particle reinforcement;in-situ growth;cor-rosion resistance}