Self-Assembled anti-Napthalene-3,4:9,10-bis(benzimidazole)s: Stabilizing Room Temperature Columnar Phase with Ambipolar Conductivity AITranslate

Indian Institute of Technology Guwahati;Organic and Flexible Electronics Laboratory;Centre for Nano and Soft Matter Sciences, Arkavathi Campus;Organic and Flexible Electronics Laboratory; Indian Institute of Technology Guwahati
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The isolation of syn- and anti-perinone derivatives and the room temperature columnar self-assembly of an anti-perinone compound with ambipolar conductivity are reported. These compounds displayed a wide absorption range encompassing the entire visible spectrum with a low band gap.

KeyWords AITranslate

liquid crystal syn/antiperinones naphthalene bis(benzimidazole) wide absorption range ambipolar conductivity
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01101

Chinese Library Classification Number:

Citation Information:

The isolation of syn- and anti-perinone derivatives and the room temperature columnar self-assembly of an anti-perinone compound with ambipolar conductivity are reported. These compounds displayed a wide absorption range encompassing the entire visible spectrum with a low band gap.

quote

GB/T 7714-2015 [1] Paresh Kumar Behera, Kajal Yadav, Doddamane Sreenivasamurthy Shankar Rao, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01101.
MLA [1] Paresh Kumar Behera, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01101.
APA [1] Paresh Kumar Behera, Kajal Yadav, Doddamane Sreenivasamurthy Shankar Rao, Upendra Kumar Pandey, & Achalkumar Ammathnadu Sudhakar. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01101
IEEE [1] Paresh Kumar Behera, Kajal Yadav, Doddamane Sreenivasamurthy Shankar Rao, Upendra Kumar Pandey, and Achalkumar Ammathnadu Sudhakar, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01101. keywords: {liquid crystal syn/antiperinones naphthalene bis(benzimidazole) wide absorption range ambipolar conductivity}