daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Elucidating the Piezoelectric, Ferroelectric, and Dielectric Performance of Lead-Free KNN/PVDF and Its Copolymer-Based Flexible Composite Films Elucidating the Piezoelectric, Ferroelectric, and Dielectric Performance of Lead-Free KNN/PVDF and Its Copolymer-Based Flexible Composite Films AITranslate

Utkal University; University of St Andrews; Jeju National University; Central Institute of Petrochemicals Engineering & Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ecofriendly, reliable, and high-performance piezoelectric materials are drawing huge interest in resolving the environmental problems arising due to consumption of fossil fuel energy. Among the lead-free ferroelectrics, potassium sodium niobate (KNN, (K,Na)NbO3) is one of the most promising piezoelectric ceramics that can replace Pb(Zr,Ti)O3. In the present work, the piezoelectric performance of KNN incorporated in poly(vinylidene fluoride) (PVDF) and its copolymers, polyvinylidene fluoride-trifluoroethylene (PVDF-TrFE) and poly(vinylidene fluoride-hexafluoropropylene) (PVDF-HFP), has been compared. The films were fabricated by a solution casting method and were further polarized by a corona poling technique. The results confirmed that the nanocomposite film with 8 wt % KNN filler in PVDF-TrFE (PTK8) exhibited the highest F(β) value, maximum remnant polarization, and dielectric constant value than other nanocomposites. The relative β-phase contents in PTK8, PHK8, and PK8 composite films reached 85, 76, and 75.8%, respectively, indicating that KNN acts as the most suitable nucleating agent in PVDF-TrFE. Also, the piezoelectric voltage output of the PTK8-based nanogenerator was found to be remarkably higher (∼20 V) as compared to other nanocomposite-based piezoelectric nanogenerators. It also exhibited a maximum power density of 0.54 μW/cm2 that was significantly improved in comparison to other composites. This nanogenerator was found to be a promising power generation device promoting miniaturization of self-powered systems.

KeyWords AITranslate

piezoelectric nanocomposite leadfree PVDF/KNN PVDFTrFE/KNN PVDFHFP/KNN
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00306

Chinese Library Classification Number:

Citation Information:

Ecofriendly, reliable, and high-performance piezoelectric materials are drawing huge interest in resolving the environmental problems arising due to consumption of fossil fuel energy. Among the lead-free ferroelectrics, potassium sodium niobate (KNN, (K,Na)NbO3) is one of the most promising piezoelectric ceramics that can replace Pb(Zr,Ti)O3. In the present work, the piezoelectric performance of KNN incorporated in poly(vinylidene fluoride) (PVDF) and its copolymers, polyvinylidene fluoride-trifluoroethylene (PVDF-TrFE) and poly(vinylidene fluoride-hexafluoropropylene) (PVDF-HFP), has been compared. The films were fabricated by a solution casting method and were further polarized by a corona poling technique. The results confirmed that the nanocomposite film with 8 wt % KNN filler in PVDF-TrFE (PTK8) exhibited the highest F(β) value, maximum remnant polarization, and dielectric constant value than other nanocomposites. The relative β-phase contents in PTK8, PHK8, and PK8 composite films reached 85, 76, and 75.8%, respectively, indicating that KNN acts as the most suitable nucleating agent in PVDF-TrFE. Also, the piezoelectric voltage output of the PTK8-based nanogenerator was found to be remarkably higher (∼20 V) as compared to other nanocomposite-based piezoelectric nanogenerators. It also exhibited a maximum power density of 0.54 μW/cm2 that was significantly improved in comparison to other composites. This nanogenerator was found to be a promising power generation device promoting miniaturization of self-powered systems.

quote

GB/T 7714-2015 [1] Alekhika Tripathy, Nirmal Prashanth Maria Joseph Raj, Sang Jae Kim, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00306.
MLA [1] Alekhika Tripathy, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00306.
APA [1] Alekhika Tripathy, Nirmal Prashanth Maria Joseph Raj, Sang Jae Kim, & Ananthakumar Ramadoss. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00306
IEEE [1] Alekhika Tripathy, Nirmal Prashanth Maria Joseph Raj, Sang Jae Kim, and Ananthakumar Ramadoss, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00306. keywords: {piezoelectric nanocomposite leadfree PVDF/KNN PVDFTrFE/KNN PVDFHFP/KNN}