Extremely Broad Electroluminescence from a Two-Dimensional Hybrid Perovskite Light-Emitting Diode Extremely Broad Electroluminescence from a Two-Dimensional Hybrid Perovskite Light-Emitting Diode AITranslate

Universidad Nacional Autónoma de México; Universidad Nacional Autónoma de México; Benemérita Universidad Autónoma de Puebla; Benemérita Universidad Autónoma de Puebla; Universidad Nacional Autónoma de México
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A single-source white-light-emitting diode from a white-light-emitting, two-dimensional hybrid perovskite is reported. The device shows an extremely broad white electroluminescence emission (fwhm = 475 nm, centered about 700 nm), almost three times as broad as its photoluminescence (176 nm) with an excellent color rendering index (CRI) of 99.

KeyWords AITranslate

singlesource white LED halide perovskite broadband emission perovskite electroluminescence whitelightemitting perovskite
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00884

Chinese Library Classification Number:

Citation Information:

A single-source white-light-emitting diode from a white-light-emitting, two-dimensional hybrid perovskite is reported. The device shows an extremely broad white electroluminescence emission (fwhm = 475 nm, centered about 700 nm), almost three times as broad as its photoluminescence (176 nm) with an excellent color rendering index (CRI) of 99.

quote

GB/T 7714-2015 [1] Paulina CarmonaMonroy, Wilson Bernal, Enrique PérezGutiérrez, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00884.
MLA [1] Paulina CarmonaMonroy, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00884.
APA [1] Paulina CarmonaMonroy, Wilson Bernal, Enrique PérezGutiérrez, M. Judith Percino, & Diego SolisIbarra. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00884
IEEE [1] Paulina CarmonaMonroy, Wilson Bernal, Enrique PérezGutiérrez, M. Judith Percino, and Diego SolisIbarra, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00884. keywords: {singlesource white LED halide perovskite broadband emission perovskite electroluminescence whitelightemitting perovskite}