Influence of Additives on the Morphology of Al(OH)_3 Ultra-fine Powder Prepared by Homogeneous Precipitation AITranslate

School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University;School of Metallurgical Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ultra-fine Al(OH)3 powder is prepared by homogenous precipitation. Study is made on the influence of different addictives on the powder morphology. The morphology of powder is analyzed through scan electron microscope. The results show that additives strongly influence the morphology of powders obtained by homogenous precipitation. The morphology of powders is changed with the type of additives. The addition of PVP and NaH2PO4 fail to form regular morphology; while the addition of PVA results in sheet structure; the particle is dispersive yet irregular with the addition of SDS. Regular spherical particles are obtained with the addition of X.

KeyWords AITranslate

homogeneous precipitation additives Al (OH) 3 ultra-fine powder morphology

1卫芝贤,胡双启,金宠,丁骋南.室温固相法制备高纯超细氢氧化铝[J].应用基础与工程科学学报,2003,11(2):122-125. 被引量:12

2宁桂玲,常玉芬,刘延来,滕飞,林源.含羧/酯基有机分子对氧化铝微粒形态调控作用研究[J].高等学校化学学报,2002,23(3):345-348. 被引量:11

3范伟东,彭志宏,李小斌.添加剂对超细氢氧化铝粉体形貌影响[J].中国锰业,2005,23(2):40-42. 被引量:4

4李东英,安黛宗,刘珩.均匀沉淀法制备纳米氧化锌和片状氧化锌粉体[J].云南化工,2003,30(3):37-39. 被引量:19

5施剑林,高建华,阮美玲.均相沉淀法制备球形氢氧化铝颗粒及其热分解行为[J].无机材料学报,1992,7(2):161-167. 被引量:11

6Sarikaya Y,et al. The effect of Al^3+ concentration on the properties of alumina powders obtained by reaction between aluminum sulphate and urea in boiling aqueous solution[J]. J Eur Ceram Soc,2002,22(12) :1905.

7唐浩林,潘牧,赵修建.溶胶凝胶法制备α-Al_2O_3纳米材料团聚控制研究新进展[J].材料导报,2002,16(9):44-45. 被引量:20

8田明原,施尔畏,元如林,王步国,李汶军,仲维卓,庄击勇.铝氢氧化物和氧化物晶粒的热液法制备及其形成机理[J].中国科学:E辑,1998,28(2):113-118. 被引量:26

9赖复兴,李启厚,黄凯,郭学益,艾侃.CdS/AlOOH纳米粉末组装行为的研究(I):载体γ-AIOOH纳米颗粒的制备[J].湿法冶金,2003,22(4):195-199. 被引量:3

10王宇菲,卓海宇.沉淀法制备纳米粉体及其形貌控制[J].湖南有色金属,2002,18(5):23-25. 被引量:8

1张宝生,李树勋.热风阀温度场的有限元分析[J].冶金设备,2015(2):51-53.

2史文峰,周杰,王治玲.超细镍粉提取方法的试验探讨[J].新疆有色金属,2003,26(S1):50-51.

3林齐,李群,叶骞.制备低钠α-Al_2O_3微粉烧结时添加剂的作用[J].轻金属,2003(7):13-15. 被引量:1

4王延芳,常崇伟.氧化铝微粉降钠途径初探[J].轻金属,1994(2):9-11.

5陈滨,吴晓华,李小斌,彭志宏,刘桂华.在AlCl_3和Al(NO_3)_3-尿素体系中制备Al(OH)_3微球颗粒[J].广东有色金属学报,2006,16(2):116-119. 被引量:1

6常照荣,王泽云,丁运长,周云庭,张军英.球形氧化锌粉末的制备研究[J].化学世界,1996,37(9):461-462. 被引量:4

7陈敏,郝俊杰,覃慧敏.均匀沉淀法制备超细钼粉[J].粉末冶金工业,2009,19(2):1-4. 被引量:10

8段学臣,高桂兰,吴湘伟,杨向萍.纳米二氧化钛粉末的研制[J].稀有金属与硬质合金,2002,30(4):17-30. 被引量:26

9韩晓斌,黄丽,回峥.微波水解法制备针形α-Fe_2O_3纳米粒子[J].无机材料学报,1999,14(4):669-673. 被引量:31

10尤其伸,黄伟光,张水菊.乙酸-苯甲酸铵沉淀分离连续测定钙和镁[J].冶金分析,1997,17(6):43-45. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:TF123.72[冶金工程—粉末冶金]

Citation Information:

Ultra-fine Al(OH)3 powder is prepared by homogenous precipitation. Study is made on the influence of different addictives on the powder morphology. The morphology of powder is analyzed through scan electron microscope. The results show that additives strongly influence the morphology of powders obtained by homogenous precipitation. The morphology of powders is changed with the type of additives. The addition of PVP and NaH2PO4 fail to form regular morphology; while the addition of PVA results in sheet structure; the particle is dispersive yet irregular with the addition of SDS. Regular spherical particles are obtained with the addition of X.

quote

GB/T 7714-2015 [1] CHEN Bin, TAN Pei-long, WU Xiao-hua, et al. Influence of Additives on the Morphology of Al(OH)_3 Ultra-fine Powder Prepared by Homogeneous Precipitation[J]. Rare Metals and Cemented Carbides, 2006(2): 12-15.
MLA [1] CHEN Bin, et al., "Influence of Additives on the Morphology of Al(OH)_3 Ultra-fine Powder Prepared by Homogeneous Precipitation." Rare Metals and Cemented Carbides, no. 2, 2006, pp. 12-15.
APA [1] CHEN Bin, TAN Pei-long, WU Xiao-hua, & LIU Yun-feng. (2006). Influence of Additives on the Morphology of Al(OH)_3 Ultra-fine Powder Prepared by Homogeneous Precipitation. Rare Metals and Cemented Carbides(2), 12-15.
IEEE [1] CHEN Bin, TAN Pei-long, WU Xiao-hua, and LIU Yun-feng, "Influence of Additives on the Morphology of Al(OH)_3 Ultra-fine Powder Prepared by Homogeneous Precipitation," Rare Metals and Cemented Carbides, no. 2, pp. 12-15, 2006. keywords: {homogeneous precipitation;additives;Al (OH) 3 ultra-fine powder;morphology}