Study of Modified Si-Cr-Fe High-temperature Anti-oxidation Coating by Fused Slurry Method AITranslate
Abstract AITranslate
The high-temperature anti-oxidation Ge-added Si-Cr-Fe coating on the niobium alloy substrate is prepared by fused slurry method. The surface, section morphology, structure, component and phase distribution of the coating before and after oxidization is analyzed,and comparison is made between the morphology,structure and anti-oxidization property of 2-step coating and 1-step coating, The results indicate that the coating consists of tow layers. The out layer, the main body of the coating, is the complex phase of (Cr,Fe,Ge,Nb)Si2. The inner layer which is a diffusion transition layer consists of the dense phases of (Cr,Fe,Ge,Nb)Si2 and microdosis(Cr,Fe,Ge,Nb)5Si3. The interfaces among the body of coating,the diffusion transition layer and the substrate are smooth, dense with wider transition layer which can effectively stop the extension of cracks to improve high-temperature anti-oxidization property.
KeyWords AITranslate
1上海科学技术情报研究所.难熔金属及其合金的防护涂层[M].上海:上海商务印书馆,1974.
2美国国家材料咨询委员会所属涂层委员会.高温抗氧化涂层[M].北京:科学出版社,1980.
3Vilasi M,et al. Phase equilibria in the Nb-Fe-Cr-Si systern[J]. Journal of Alloy and Compounds, 1998, (269) :187.
4翟金坤,马祥,白新德,侯卫红.C-103铌合金上Si-Cr-Ti料浆熔烧涂层的改性研究[J].航空学报,1994,15(4):499-506. 被引量:20
5贾中华.料浆法制备铌合金和钼合金高温抗氧化涂层[J].粉末冶金技术,2001,19(2):74-76. 被引量:41
6Vilasi M,et al. New silicides for new niobium protective coatings[J]. Journal of Alloys and Compounds, 1998,(264) : 244.
7Brian V Cockeram. Growth and oxidation resistance of boron-modified and germanium-doped silicide diffusion coatings formed by the halide-activated pack cementation method[J]. Surface and Coatings Technology. 1995, (76-77) :20.
8Leyens C,et al. Transformation and oxitation of a sputtered low- expansion Ni- Cr- Al- Ti- Si bond coating for thermal barrier systems[J]. Surface and Coatings Technology, 1997, (94-95) : 155.
1赵猛,李争显,黄春良,张欣,华云峰,慕伟意.铌合金表面辉光等离子渗Mo的扩散研究[J].稀有金属,2010,34(6):839-843. 被引量:2
2刘超锋,林茹,孟庆乐.金属基体陶瓷涂料的研究与应用[J].涂料工业,2007,37(9):61-64. 被引量:7
3于斌,何俊,刘志栋,靳庆臣,陈威,王祥龙.电子束重熔处理对硅化物涂层表面形貌和性能的影响[J].真空与低温,2009,15(3):149-152. 被引量:7
4于斌,靳庆臣,刘志栋,何俊.硅化物涂层电子束重熔表面改性技术[J].中国空间科学技术,2010,30(5):54-58. 被引量:2
5杨凌霄,郭喜平,乔彦强,潘若冰.Nb-Ti-Si基超高温合金表面Ge-Y改性硅化物渗层的组织形成[J].金属学报,2013,49(11):1433-1438.
6贵永亮,张良,王振磊,宋春燕,陈振飞.Fe-Cr-Si系合金的研究现状与展望[J].材料导报:纳米与新材料专辑,2013,27(2):343-345. 被引量:6
7薛飞,王进卿,池作和.锅炉受热面复合陶瓷涂层的抗高温腐蚀性能[J].材料保护,2017,50(8):80-83. 被引量:5
8杨涛,杜继红,汪欣,严鹏,李晴宇,唐勇.难熔金属表面硅化物涂层的研究进展[J].材料保护,2019,0(7):121-127. 被引量:4
1于斌,刘志栋,靳庆臣,何俊,程彬.电子束表面改性技术质量控制与性能影响分析[J].真空与低温,2010,16(2):63-71. 被引量:5
2于斌,刘志栋,靳庆臣,程彬,陈威,石晓强,李兴利.国内外空间复合材料压力容器研究进展及发展趋势分析(二)[J].压力容器,2012,29(4):30-41. 被引量:10
3于斌,杨学虎,刘志栋,靳庆臣.高能束高频等效热源表面改性技术[J].焊接,2012(7):55-57.
4崔学军,李国军,任瑞铭.甲基三甲氧基硅烷改性工业硅溶胶的工艺及其机理[J].材料科学与工程学报,2012,30(4):528-532. 被引量:6
5陈海君,刘序英,叶祥,欧阳芬芬,程广亮,刘康生,周雅.铌及铌合金的表面防护技术[J].江西化工,2013,29(3):1-5. 被引量:1
6牙亚萌,张胜利,李唯,张镓远,陈彬源,李浩.高温、含H_2S环境的设备内壁陶瓷金属涂层防腐技术[J].天然气与石油,2016,34(2):72-77. 被引量:7
7陈松,董天顺,李国禄,周秀锴,王朝建,张晓敏,田庚凡.热喷涂层的重熔技术及其发展现状[J].焊接技术,2016,45(5):76-79. 被引量:7
8高恒蛟,熊玉卿,赵栋才,王金晓,王兰喜.耐高温抗氧化铱涂层的研究现状[J].真空与低温,2016,22(4):187-191. 被引量:1
9王勇,吴圣,杜禾,张升霞,吴斌,谢会.一种Fe-Cr-Si-B系合金喷焊层组织及性能[J].电焊机,2017,47(10):119-122.
10陈子辉,刘仲阳,林家祥.柔性有机硅陶瓷面漆的理论及应用探索[J].涂料技术与文摘,2017,38(10):1-5. 被引量:7
1何俊,于斌,张涛,张永和.铌合金硅化物涂层的制备工艺及改进途径[J].航空制造技术,2010,0(1):74-77. 被引量:8
2任鑫,王福会,汪信.Al-Si涂层在900℃硫酸盐中的热腐蚀行为[J].腐蚀科学与防护技术,2004,16(4):187-191. 被引量:7
3相珺,刘尊智,张爱民,马胜男,王东宇.不锈钢表面SiO_2系陶瓷涂层的耐蚀性研究[J].腐蚀科学与防护技术,2016,28(4):341-345. 被引量:3
4贾中华.料浆法制备铌合金和钼合金高温抗氧化涂层[J].粉末冶金技术,2001,19(2):74-76. 被引量:41
5王泽书.铁素体可锻铸铁的脆性与碳硅比[J].铸造,1990(9):29-31.
6赵斌,李智超,李和万.复合涂层技术研究进展[J].热加工工艺,2010,39(22):127-130. 被引量:4
7李耀东,赵越超,高红.料浆法SiO_2基陶瓷涂层制备及性能研究[J].表面技术,2007,36(3):23-24. 被引量:2
8赵越超,高红,马状,孙方红.料浆法SiO_2基陶瓷涂层耐蚀性能研究[J].热加工工艺,2007,36(2):37-38. 被引量:4
9宋福田,董卫萍,孙思铭,翟宗宝.乙炔气改性类石墨涂层结构和性能研究[J].铸造技术,2016,37(2):245-248.
10唐勇,杜继红,李争显,黄春良,胡湘银.铌及铌合金高温抗氧化防护涂层研究[J].表面技术,2009,38(5):42-43. 被引量:11
Basic Information:
DOI:
Chinese Library Classification Number:TG174.44[金属学及工艺—金属表面处理]
Citation Information:
The high-temperature anti-oxidation Ge-added Si-Cr-Fe coating on the niobium alloy substrate is prepared by fused slurry method. The surface, section morphology, structure, component and phase distribution of the coating before and after oxidization is analyzed,and comparison is made between the morphology,structure and anti-oxidization property of 2-step coating and 1-step coating, The results indicate that the coating consists of tow layers. The out layer, the main body of the coating, is the complex phase of (Cr,Fe,Ge,Nb)Si2. The inner layer which is a diffusion transition layer consists of the dense phases of (Cr,Fe,Ge,Nb)Si2 and microdosis(Cr,Fe,Ge,Nb)5Si3. The interfaces among the body of coating,the diffusion transition layer and the substrate are smooth, dense with wider transition layer which can effectively stop the extension of cracks to improve high-temperature anti-oxidization property.
quote
| GB/T 7714-2015 | [1] XIAO Lai-rong, CAI Zhi-gang, YIN Lei, et al. Study of Modified Si-Cr-Fe High-temperature Anti-oxidation Coating by Fused Slurry Method[J]. Rare Metals and Cemented Carbides, 2006(2): 16-20. |
| MLA | [1] XIAO Lai-rong, et al., "Study of Modified Si-Cr-Fe High-temperature Anti-oxidation Coating by Fused Slurry Method." Rare Metals and Cemented Carbides, no. 2, 2006, pp. 16-20. |
| APA | [1] XIAO Lai-rong, CAI Zhi-gang, YIN Lei, ZHANG Li-ping, & XIANG Cai-wen. (2006). Study of Modified Si-Cr-Fe High-temperature Anti-oxidation Coating by Fused Slurry Method. Rare Metals and Cemented Carbides(2), 16-20. |
| IEEE | [1] XIAO Lai-rong, CAI Zhi-gang, YIN Lei, ZHANG Li-ping, and XIANG Cai-wen, "Study of Modified Si-Cr-Fe High-temperature Anti-oxidation Coating by Fused Slurry Method," Rare Metals and Cemented Carbides, no. 2, pp. 16-20, 2006. keywords: {fused slurry;niobium alloy;silicide;high-temperature anti-oxidation coating} |