daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study of Nb Reduction for Preparation of Niobium Suboxide as Electrolytic Capacitor Anode Material AITranslate

School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University;School of Materials Science and Engineering, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the preparation of niobium suboxide by Nb reduction. Niobium Suboxide powder is prepared by agate grinding and mixing-reduction roasting-screening. The process were further optimized through orthogonal experiments and variance analysis. Physical and microscopic examination of the product is made through XRD and SEM. Niobium suboxide anode is prepared with method similar to that for tantalum electrolytic capacitor and its electric property is investigated by electrolytic capacitor anode testing. The results show that niobium suboxide prepared by Nb reduction of Nb2O5 has good electric property with specific capacity 69 500 μF · V/g,loss 11.25 %, leakage current (value of K) ≤ 1.8 × 10.4μA/(μF · V), which are better than those of the Chinese national standard (GB/T 3136-- 1995) for FTal 6-- 300 tantalum powder for capacitor.

KeyWords AITranslate

niobium suboxide Nb reduction preparation electrolytic capacitor anode electrical property

1何季麟.钽铌电子材料新进展[J].中国有色金属学报,2004,14(F01):291-300. 被引量:23

2李春光,钟景明,高勇,董宁利.铌电容器及其电介质的稳定性[J].中国有色金属学报,2003,13(6):1401-1406. 被引量:5

3钟晖,李荐,戴艳阳,钟海云.铌电解电容器最新研究发展动态[J].稀有金属,2002,26(2):139-142. 被引量:10

4Fedorenko A I,et al. Layer systems on the base of nitrogen-doped tantalum with enhanced stability[J]. Crystal Research and Technology, 1997,32 (6) : 843.

5Qiu Yongjian,et al. The stabilization of niobium solid electrolyte capacitors [J]. Active and Passive Electronic Components, 2002,25 (2):201.

6Pozdeev Y. Reliability comparison of tantalum and niobium solid electrolytic capacitors[J]. Quality and Reliability Engineering International, 1998,14 (2) :79.

7李荐,李庆奎,温俊杰,钟海云.低价铌氧化物电解电容器阳极的研制[J].稀有金属材料与工程,2005,34(7):1144-1146. 被引量:3

8Fife James A. Partial reduction of niobium pentoxide for its use as a capacitor anode[P]. US Pat: 6416730 B1,2002-07-09.

9Schnitter Christoph, et al. Niobium based electrolytic capacitor anode[P]. WO Pat:2002017338 A1,2002-02-28.

10Kimmel Jonathan L, et al. Refractory metal suboxide powders suitable for sintered capacitor anodes[P]. WO Pat:2002037513 A2,2002-05-10.

1李荐,易丹青,温俊杰,钟海云.新型电解电容器阳极材料低价铌氧化物的制备[J].中国有色金属学报,2005,15(6):893-899. 被引量:4

2李荐,温俊杰,钟海云.镁还原法制备新型电解电容器阳极材料低价铌氧化物的工艺研究[J].稀有金属与硬质合金,2005,33(2):19-22. 被引量:4

3李荐,温俊杰,钟海云,易丹青.高能球磨法制备新型电解电容器阳极材料低价铌氧化物工艺研究[J].稀有金属与硬质合金,2005,33(3):4-8. 被引量:2

4李荐,易丹青,温俊杰,钟晖.NbH还原制备新型电容器阳极材料低价铌氧化物[J].中南大学学报:自然科学版,2006,37(3):461-466.

5顾健,武高辉,赵骁.高阻尼空心微珠/环氧复合材料的制备及性能研究[J].功能材料,2007,38(5):764-766. 被引量:10

6喜琍.电解电容器的可靠性试验及失效分析[J].电子质量,2007(3):31-33. 被引量:2

7左宏,李新芳,刘春明.微量Ga对电容器阳极用铝箔组织及比电容的影响[J].东北大学学报:自然科学版,2013,34(10):1400-1403. 被引量:2

8铌电解电容器将成替代品[J].国际电子变压器,2005(5).

9Jingbo SONG,Weimin MAO,Hong YANG,Huiping FENG.Effect of Trace Sn on Pitting Behaviors of High Voltage Anode Aluminum Foil[J].材料科学技术:英文版,2008,24(5):718-722. 被引量:2

10刘仲娥,王耀东,宋金荣,陶珊,潘平华.电容器在能量转换技术应用中的新进展[J].材料导报,2005,19(2):34-35. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]

Citation Information:

Study is made of the preparation of niobium suboxide by Nb reduction. Niobium Suboxide powder is prepared by agate grinding and mixing-reduction roasting-screening. The process were further optimized through orthogonal experiments and variance analysis. Physical and microscopic examination of the product is made through XRD and SEM. Niobium suboxide anode is prepared with method similar to that for tantalum electrolytic capacitor and its electric property is investigated by electrolytic capacitor anode testing. The results show that niobium suboxide prepared by Nb reduction of Nb2O5 has good electric property with specific capacity 69 500 μF · V/g,loss 11.25 %, leakage current (value of K) ≤ 1.8 × 10.4μA/(μF · V), which are better than those of the Chinese national standard (GB/T 3136-- 1995) for FTal 6-- 300 tantalum powder for capacitor.

quote

GB/T 7714-2015 [1] LI Jian, WEN Jun-jie, ZHONG Hai-yun. Study of Nb Reduction for Preparation of Niobium Suboxide as Electrolytic Capacitor Anode Material[J]. Rare Metals and Cemented Carbides, 2006(2): 21-26.
MLA [1] LI Jian, et al., "Study of Nb Reduction for Preparation of Niobium Suboxide as Electrolytic Capacitor Anode Material." Rare Metals and Cemented Carbides, no. 2, 2006, pp. 21-26.
APA [1] LI Jian, WEN Jun-jie, & ZHONG Hai-yun. (2006). Study of Nb Reduction for Preparation of Niobium Suboxide as Electrolytic Capacitor Anode Material. Rare Metals and Cemented Carbides(2), 21-26.
IEEE [1] LI Jian, WEN Jun-jie, and ZHONG Hai-yun, "Study of Nb Reduction for Preparation of Niobium Suboxide as Electrolytic Capacitor Anode Material," Rare Metals and Cemented Carbides, no. 2, pp. 21-26, 2006. keywords: {niobium suboxide;Nb reduction;preparation;electrolytic capacitor anode;electrical property}