Combining the compounding and the mixed methods, a new dry-wet methodhas been developed and used to prepare RE three primary colours phosphor. Related technological conditions have been investigated. Tested results and practice show that the newproduct has moderate and even particle size with stable properties, and meet the requirements of the key material for energy-saving lamp.
KeyWords AITranslate
1刘宇晖.三基色荧光粉蓝粉制取工艺的改进[J].江西有色金属,2002,16(2):18-21. 被引量:1
2李璠,李样生.钡镁多铝酸盐蓝色荧光粉的研究进展[J].江苏化工,2002,30(6):25-29. 被引量:5
3刘培培.软件可靠性费用估算方法研究[J].河北大学学报:自然科学版,2003,23(4):434-439. 被引量:3
4李同锴,徐景智,杨景发,杨宝柱,刘虎,张玉芳.植物生长灯荧光粉的研制[J].河北大学学报:自然科学版,2003,23(4):375-376.
1丁建红,李许波,倪海勇.铝源对稀土三基色蓝粉的影响[J].材料研究与应用,2007,1(1):34-36. 被引量:1
2祝理君,曾智江,史利军,冯宏伟.溶胶—凝胶法制备BAM前驱体BaMgAl_(10)O_(17)研究[J].兵器材料科学与工程,2007,30(1):35-38. 被引量:3
3祝理君,余展,曾智江,史利军.PDP用BAM蓝色荧光粉制备技术研究现状[J].兵器材料科学与工程,2007,30(6):70-74. 被引量:5
4陈鹏,朱月华,黄如喜.稀土氯磷酸盐体系蓝色荧光粉的研究[J].南京师大学报:自然科学版,2008,31(4):84-88.
5黄宁,陈未如,石帅.面向评估的软件可靠性与费用模型的研究[J].佳木斯大学学报:自然科学版,2009,27(1):70-72. 被引量:1
6卜贺,金永生,李静.基于层次分析法的电信运营商销售费用效益评估[J].北京邮电大学学报:社会科学版,2010,12(2):39-44. 被引量:3
7顾爱华,张春阳,胡庆新.软件可靠性增长G-O模型的改进[J].内蒙古大学学报:自然科学版,2014,45(2):192-195. 被引量:3
8吴勇.软化学合成方法在稀土材料中的应用[J].太原城市职业技术学院学报,2011(12):170-171.
1洪广言,刘书珍.国内外灯用稀土三基色荧光粉的剖析:(六)形貌分析[J].发光快报,1995(4):18-21.
2关中素,唐明道.国内外灯用稀土三基色荧光粉的剖析:(二)发光性能的测试和分析[J].发光快报,1995(4):4-6.
3关中素,唐明道.国内外灯用稀土三基色荧光粉的剖析:(三)热稳定性的测试和分析[J].发光快报,1995(4):7-9.
4洪广言,关中素.国内外灯用稀土三基色荧光粉的剖析:(一)稀土三基色荧光粉的进展[J].发光快报,1995(4):1-3. 被引量:1
5洪广言,李有谟.国内外灯用稀土三基色荧光粉的剖析:(五)粒度分析[J].发光快报,1995(4):15-17. 被引量:1
6刘书珍,洪广言.国内外灯用稀土三基色荧光粉的剖析:(四)稀土三基色荧光粉的结构分析[J].发光快报,1995(4):10-14.
7徐鹏霄,乔辉,王仍,刘诗嘉,曾巧玉,张可锋,李向阳.干湿结合法在CdZnTe衬底上制备折射型红外微透镜的研究[J].半导体光电,2014,35(6):1022-1025. 被引量:3
8马进锋,周惠英.基于铁塔公司建设需求的室分设计技术分析[J].移动通信,2016,40(18):51-57. 被引量:1
9“高亮度低光衰灯用稀土三基色荧光粉”项目通过鉴定[J].稀土信息,2005,11(12):34-34.
10任国旭.GSM无线网络容量规划方法新探[J].邮电设计技术,2003(1):14-21.
Basic Information:
DOI:
Chinese Library Classification Number:TN104.3[电子电信—物理电子学]
Citation Information:
Combining the compounding and the mixed methods, a new dry-wet methodhas been developed and used to prepare RE three primary colours phosphor. Related technological conditions have been investigated. Tested results and practice show that the newproduct has moderate and even particle size with stable properties, and meet the requirements of the key material for energy-saving lamp.
quote
| GB/T 7714-2015 | [1] LI Xiao-liang, WAN Yuan-kao, HU Jun, et al. Research and Preparation of RE Three Primary Colours Phosphor for Energy-Saving Lamp[J]. Rare Metals and Cemented Carbides, 1997(1): 9-13. |
| MLA | [1] LI Xiao-liang, et al., "Research and Preparation of RE Three Primary Colours Phosphor for Energy-Saving Lamp." Rare Metals and Cemented Carbides, no. 1, 1997, pp. 9-13. |
| APA | [1] LI Xiao-liang, WAN Yuan-kao, HU Jun, WEI Jing-hua, & JIANG Rong-ying. (1997). Research and Preparation of RE Three Primary Colours Phosphor for Energy-Saving Lamp. Rare Metals and Cemented Carbides(1), 9-13. |
| IEEE | [1] LI Xiao-liang, WAN Yuan-kao, HU Jun, WEI Jing-hua, and JIANG Rong-ying, "Research and Preparation of RE Three Primary Colours Phosphor for Energy-Saving Lamp," Rare Metals and Cemented Carbides, no. 1, pp. 9-13, 1997. keywords: {RE three primary colours phosphor, dry-wet method, technology} |