Abstract AITranslate

Specific volume --particle diameter relation has been studied for capacitor Tapowder. According to the relationship,derived from the approximate mathematical model,aspecific volume-particle diameter curve is obtained with a max of specific volume for eachtype of Ta powder. After introducing a correction factor into the curve,a real specific volumeof Ta powder can be estimated.

KeyWords AITranslate

capacitor Ta powder specific volume and partcle diameter mathematical model specific volume estimation

1廖国清.电机和电器特性曲线的数学处理[J].电机电器技术,1998(1):16-18.

2张卫平,吴兆麟,赵徐森,龚绍文.功率因数校正器的三频分析法[J].电子学报,1997,25(11):46-48. 被引量:1

3李荐,易丹青,温俊杰,钟海云.新型电解电容器阳极材料低价铌氧化物的制备[J].中国有色金属学报,2005,15(6):893-899. 被引量:4

4潘佐郑.对跳线长度计算中引进样条曲线方法的数学处理[J].电力建设,1993,14(6):67-69.

5刘君,吴广宁,周凯,周利军,曹开江.基于电声脉冲法的空间电荷测量装置[J].高电压技术,2009,35(3):607-612. 被引量:13

6陈培育,李树青,王瑶.用于微机保护的1/4周波傅氏算法研究[J].电工技术,2013(12):24-25. 被引量:1

7李泽,许宝才,王建江,蔡旭东.片状羰基铁低频吸波性能的多因素参数调控[J].磁性材料及器件,2017,48(2):45-48. 被引量:2

8沈尔忠,邓京川,王魁香.磁场建像中的理论模型和数学处理[J].吉林大学自然科学学报,1995(4):92-96.

9郝思鹏,范瑛.电路理论的数学和工程背景[J].南京工程学院学报:自然科学版,2003,1(3):24-27.

10程付安,常汉宝,刘伯运,邵利民.扭振分析在轴功测量技术中的应用[J].内燃机,2006,22(5):35-37.

Basic Information:

DOI:

Chinese Library Classification Number:TM535.1[电气工程—电器]

Citation Information:

Specific volume --particle diameter relation has been studied for capacitor Tapowder. According to the relationship,derived from the approximate mathematical model,aspecific volume-particle diameter curve is obtained with a max of specific volume for eachtype of Ta powder. After introducing a correction factor into the curve,a real specific volumeof Ta powder can be estimated.

quote

GB/T 7714-2015 [1] WANG Shi-guang. Specific Volume-Particle Diameter Model Establishment and Its Mathematical Treatment for Ta Powder[J]. Rare Metals and Cemented Carbides, 1997(1): 14-20.
MLA [1] WANG Shi-guang. "Specific Volume-Particle Diameter Model Establishment and Its Mathematical Treatment for Ta Powder." Rare Metals and Cemented Carbides, no. 1, 1997, pp. 14-20.
APA [1] WANG Shi-guang. (1997). Specific Volume-Particle Diameter Model Establishment and Its Mathematical Treatment for Ta Powder. Rare Metals and Cemented Carbides(1), 14-20.
IEEE [1] WANG Shi-guang, "Specific Volume-Particle Diameter Model Establishment and Its Mathematical Treatment for Ta Powder," Rare Metals and Cemented Carbides, no. 1, pp. 14-20, 1997. keywords: {capacitor Ta powder,specific volume and partcle diameter, mathematical model,specific volume estimation}