Influence of Y_2O_3 on the Properties of WC-8Ni Cemented Carbide and the Sintering Temperature AITranslate
Abstract AITranslate
The influence of Y2O3(1. 1 % of ni mass) on the physical and chemical. properties of WC-8Ni cemented carbide and the sintering tenlperaturc xu,as investigated. It wasfound that addition of Y2O3 not only improved the properties, but decreased the sinteringtemperature. Using SEM the microstructure of cement f}d carbides of three temperatures wasanalysed and compared. The relation of the properties of the alloy to the sintering temperature. and the reasons for decreasing the sintering temperature were explained.
KeyWords AITranslate
1林信平,曹顺华,李炯义.一种新型晶粒长大抑制剂对纳米硬质合金烧结行为的影响[J].稀有金属与硬质合金,2004,32(4):4-9. 被引量:3
2曹顺华,林信平,李炯义,蔡志勇,谢湛.一种新型晶粒长大抑制剂对YG10硬质合金烧结行为的影响[J].中南大学学报:自然科学版,2005,36(4):533-538. 被引量:8
3杨眉,刘清才,黄志强,刘清友.Al_2O_3/WC-8Co纳米/微米复合材料显微结构与力学性能[J].煤炭学报,2010,35(3):494-497. 被引量:1
4李先容,高宇,徐俊,李强.添加微量Y_2O_3对WC-8%Ni合金微观组织与性能的影响[J].硬质合金,2010,27(3):135-138. 被引量:2
5胡海波.添加剂对WC-Ni硬质合金组织结构与力学性能的影响[J].稀有金属与硬质合金,2013,41(1):55-59. 被引量:4
6李炯义,曹顺华,林信平.硬质合金中的晶粒长大抑制剂[J].硬质合金,2004,21(1):56-60. 被引量:23
1赵正,刘福田,李文虎.铁硼合金和钼对钢结硬质合金烧结的影响[J].机械工程材料,2008,32(2):1-3. 被引量:1
2张宇,钟敏霖,刘文今.送粉激光熔覆合成制备WC/Ni硬质合金涂层及其耐磨性[J].金属热处理,2005,30(11):1-5. 被引量:26
3吴其山.超细WC-Co硬质合金研究综述[J].中国钨业,2005,20(6):35-40. 被引量:19
4张利平,张国珍,张久兴,周美玲.叠层加压SPS烧结制备梯度硬质合金[J].稀有金属材料与工程,2006,35(1):70-73. 被引量:3
5邱友绪,李宁,张伟,文玉华,张勇,周永贵.WC-Co超细晶硬质合金晶粒长大抑制剂及其机理的研究[J].硬质合金,2006,23(4):254-257. 被引量:21
6张武装,刘咏,黄伯云.纳米晶WC-Co硬质合金的研究现状[J].材料导报,2007,21(2):79-82. 被引量:22
7刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21
8孙东平.晶粒长大抑制剂对WC-8%Co超细硬质合金性能的影响[J].稀有金属与硬质合金,2009,37(2):7-11. 被引量:7
9姜爱民,蒋显全,陈巧旺,陈异.晶粒长大抑制剂在硬质合金中的应用概况[J].硬质合金,2010,27(4):252-257. 被引量:13
10肖代红,贺跃辉,宋旼,申婷婷,欧小琴.超细晶WC-10Co-VC-NbC硬质合金的组织与性能[J].材料热处理学报,2010,31(10):26-29. 被引量:2
1周芳,高甲生,侯清宇.等离子弧喷焊Co/Y_2O_3复合结构涂层研究[J].焊接技术,2005,34(2):19-20.
2朱涛,朱维东,周芳,黄碧芳.稀土Y_2O_3对激光熔覆Al/Fe基合金涂层的影响[J].现代机械,2012(5):77-80. 被引量:2
3杨海林,周雪安,赵万军,阮建明.Y_2O_3对锌熔再生硬质合金组织及性能的影响[J].硬质合金,2010,27(2):65-70. 被引量:11
4孙万昌,张佩,李攀,佘晓林,魏汉军,赵坤,张峰.烧结工艺和Y_2O_3添加量对Ti(C,N)基金属陶瓷显微组织和力学性能的影响[J].中国有色金属学报,2015,25(5):1277-1284. 被引量:6
5王成磊,高原,张光耀.Y_2O_3对铝合金表面激光增材制造组织及耐蚀性影响[J].稀有金属材料与工程,2017,46(3):812-817. 被引量:7
6封延松,程西云.Y_2O_3对镍基碳化钛金属陶瓷熔覆层组织的影响[J].润滑与密封,2008,33(9):13-15. 被引量:9
7张政,代绪恩,江佩泽,王斌俨.混合稀土对生物陶瓷涂层组织结构与性能的影响[J].中国科技博览,2015,0(3):334-336.
8盛定高.精铸镍基合金涡轮叶片缺陷激光熔覆修复工艺[J].铸造技术,2009,30(10):1341-1343. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The influence of Y2O3(1. 1 % of ni mass) on the physical and chemical. properties of WC-8Ni cemented carbide and the sintering tenlperaturc xu,as investigated. It wasfound that addition of Y2O3 not only improved the properties, but decreased the sinteringtemperature. Using SEM the microstructure of cement f}d carbides of three temperatures wasanalysed and compared. The relation of the properties of the alloy to the sintering temperature. and the reasons for decreasing the sintering temperature were explained.
quote
| GB/T 7714-2015 | [1] YONG Zhi-hua, WANG Shi-yuan, WANG Zhen-ning, et al. Influence of Y_2O_3 on the Properties of WC-8Ni Cemented Carbide and the Sintering Temperature[J]. Rare Metals and Cemented Carbides, 1997(1): 21-24. |
| MLA | [1] YONG Zhi-hua, et al., "Influence of Y_2O_3 on the Properties of WC-8Ni Cemented Carbide and the Sintering Temperature." Rare Metals and Cemented Carbides, no. 1, 1997, pp. 21-24. |
| APA | [1] YONG Zhi-hua, WANG Shi-yuan, WANG Zhen-ning, & DENG Ming. (1997). Influence of Y_2O_3 on the Properties of WC-8Ni Cemented Carbide and the Sintering Temperature. Rare Metals and Cemented Carbides(1), 21-24. |
| IEEE | [1] YONG Zhi-hua, WANG Shi-yuan, WANG Zhen-ning, and DENG Ming, "Influence of Y_2O_3 on the Properties of WC-8Ni Cemented Carbide and the Sintering Temperature," Rare Metals and Cemented Carbides, no. 1, pp. 21-24, 1997. keywords: {cemented carbide, Y_2O_3, property. sintering tempature} |