daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

A New Technological Process for Smelting Ferro-Tungsten-Molybdenum AITranslate

Institute of Mechanics, Chinese Academy of Sciences;Institute of Mechanics, Chinese Academy of Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper introduces the use of W and Mo in alloy steel, describes the mechanism of ferro-tungsten-molybdenum smelting in three-phase AC working frequency plasmafurnace directly with mixed charge of W and Mo concentrates and gives the pilot experimentresults. The ferro-tungsten-molybdenum, obtained with Mo/W of 0. 05~0. 5 at recovery ofMo and W>90% respectively, is applicable to smelting ahoy steel. This new technologicalroute is open to utilization of the W-Mo intergrowth mineral resource.

KeyWords AITranslate

W concentrate Mo concentrate. plasma smelting ferro-tungstenmolybdenum new technology

1孙善长,杨德鑫,蒋汉祥.硅铝热法冶炼钨钼复合铁合金试验[J].铁合金,1993(4):30-32. 被引量:3

2赵先存,郑鲁.我国钨钼合金钢的发展及成就[J].中国钨业,1989(11):7-10. 被引量:2

1罗林根,王磊,郭培民,赵志民,林银河,李正邦.用低品质钨钼矿研制钨钼复合合金热力学分析[J].钢铁,2015,50(9):28-33. 被引量:1

1付宇明,赵华洋,郑丽娟,齐童.多元陶瓷相在激光熔覆层中的溶解机制研究[J].中国机械工程,2019,30(23):2884-2889.

1孙善长,杨德鑫,蒋汉祥.硅铝热法冶炼钨钼复合铁合金试验[J].铁合金,1993(4):30-32. 被引量:3

2Good.,JE,王爱萍.世界等离子冶炼技术的发展[J].钢铁工艺,1992(3):26-28.

3兰尧中.等离子技术在钒,钛冶金若干领域的应用[J].钒钛,1992(5):9-11.

4白宝玲,冯敏莉.等离子技术在高炉渣口喷涂的应用[J].冶金设备管理与维修,1990(2):41-45.

5朱兆鹏.等离子技术与钼冶金[J].中国钼业,2000,24(1):26-29.

6代红庆,宋春燕.等离子技术在炼钢过程中的应用[J].唐钢科技,1998(1):21-26.

7邓森彪,陈雪梅,梁南山.涟钢高炉高块矿比炉料结构冶金性能研究[J].世界有色金属,2016,0(7):64-65. 被引量:1

8郭和才.混合炉料对高炉冶炼气体运动的影响[J].湖南冶金,1996,24(1):53-57.

9风林.大喷煤量技术的开发——高富氯及等离子技术[J].钢铁,1993(2):84-84.

10张勇,魏丽艳.超大型高炉原料冶金性能优化研究[J].中国钢铁业,2013(4):12-14.

Basic Information:

DOI:

Chinese Library Classification Number:TF6[冶金工程—钢铁冶金]

Citation Information:

The paper introduces the use of W and Mo in alloy steel, describes the mechanism of ferro-tungsten-molybdenum smelting in three-phase AC working frequency plasmafurnace directly with mixed charge of W and Mo concentrates and gives the pilot experimentresults. The ferro-tungsten-molybdenum, obtained with Mo/W of 0. 05~0. 5 at recovery ofMo and W>90% respectively, is applicable to smelting ahoy steel. This new technologicalroute is open to utilization of the W-Mo intergrowth mineral resource.

quote

GB/T 7714-2015 [1] CAO Yong-xian, XU Yong-xiang. A New Technological Process for Smelting Ferro-Tungsten-Molybdenum[J]. Rare Metals and Cemented Carbides, 1997(1): 5-8.
MLA [1] CAO Yong-xian, and XU Yong-xiang. "A New Technological Process for Smelting Ferro-Tungsten-Molybdenum." Rare Metals and Cemented Carbides, no. 1, 1997, pp. 5-8.
APA [1] CAO Yong-xian, & XU Yong-xiang. (1997). A New Technological Process for Smelting Ferro-Tungsten-Molybdenum. Rare Metals and Cemented Carbides(1), 5-8.
IEEE [1] CAO Yong-xian and XU Yong-xiang, "A New Technological Process for Smelting Ferro-Tungsten-Molybdenum," Rare Metals and Cemented Carbides, no. 1, pp. 5-8, 1997. keywords: {W concentrate, Mo concentrate. plasma smelting, ferro-tungstenmolybdenum, new technology}